IP Library Granted Patent US 10,651,506
Granted Patent B2
US 10,651,506 · App. 15/738,358 · Granted May 12, 2020

All-solid-state secondary battery and method of producing the same

Inventors: Hideyuki Fukui (Osaka, JP); Shiken Ryou (Osaka, JP); Yasushi Takano (Osaka, JP)
Assignee: Hitachi Zosen Corporation
H01M10/0585H01M4/64H01M10/02H01M10/0436H01M10/0486H01M10/0562H01M10/0565H01M2004/027H01M2004/028H01M2300/0065
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,651,506
App. No.
15/738,358
Granted
May 12, 2020
Kind
B2
Abstract

The present invention provides an all-solid-state secondary battery and a method for producing the same that can prevent the collapse of a laminate due to a shearing force occurring in the peripheral portion of the laminate when the laminate is pressed, and the occurrence of an internal short circuit can be prevented. The all-solid-state secondary battery includes a laminate and a plate-shaped insulating member both arranged between the positive electrode collector and the negative electrode collector. The laminate includes a positive electrode layer, a solid electrolyte layer, and a negative electrode layer. The plate-shaped insulating member is arranged around the laminate and contacted at least with the solid electrolyte layer to electrically insulate the positive electrode layer from the negative electrode layer. In the insulating member, a contact inner edge portion contacted with the laminate is thicker than a plate-shaped portion on the outer side.

Claims (6)

1. An all-solid-state secondary battery comprising:

a pair of collectors;

a laminate; and

a plate-shaped insulating member, the laminate and the insulating member being arranged between the pair of collectors, the laminate including a positive electrode layer, a solid electrolyte layer, and a negative electrode layer stacked together, the insulating member being arranged around the laminate and contacted at least with the solid electrolyte layer to electrically insulate the positive electrode layer and the negative electrode layer from each other,

wherein in the insulating member, a contact inner edge portion contacted with the laminate has a larger thickness than a plate-shaped portion positioned on an outer side, and

wherein the insulating member is arranged between the pair of collectors via a positive electrode-side adhesive layer and a negative electrode-side adhesive layer, and the adhesive layers are arranged distant from an inner end of the insulating member to provide a distortion absorbing region to each of the collectors.

Assignments (2)
CHANGE OF NAME Recorded May 20, 2026
From: HITACHI ZOSEN CORPORATION
To: KANADEVIA CORPORATION
Reel/Frame 075587/0740 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 20, 2017
From: FUKUI, HIDEYUKI; TAKANO, YASUSHI
To: HITACHI ZOSEN CORPORATION
Reel/Frame 044921/0695 →
Priority Claims (1)
JP 2015-125202 · Jun 23, 2015 · national
Continuity (1)
Related Publication 20180198169A1 · Jul 12, 2018