Use of polymeric additives for paraffin-containing fluids
The present invention is concerned with the use of polymeric additives for paraffin-containing fluids as pour point depressants and low temperature flow improvers, wherein the polymers comprise styrene and maleic acid dialkyl ester building blocks.
1. A method for reducing the pour point of a paraffin-containing fluid, comprising adding to a paraffin-containing fluid a polymer comprising the following building blocks:
wherein
and —R 2 are, independent from each other, a C12- to C36- alkyl group;
the alkyl groups being a mixture of branched and linear, the ratio of the linear alkyl groups to the branched alkyl groups is in the range from 95:5 to 5:95 (weight % : weight %),
at least 90% of the number of the building blocks are a) and b), relative to the total number of all building blocks incorporated in the polymer; and
the building blocks a) and b) are, relative to each other, present in the polymer in a ratio of from 80:20 to 20:80 (number:number);
wherein the paraffin-containing fluid is a crude oil, a petroleum oil, a shale oil, a tar sands oil, or mixtures thereof; and
wherein 20 to 2000 ppm (weight:weight) of the polymers are used in the paraffin-containing fluid.
2. The method according to claim 1 , wherein the polymer consists of more than 98% of the building blocks a) and b).
3. The method according to claim 1 , wherein the branched alkyl groups are 2-alkyl- 1 -alkyl groups.
4. The method according to claim 1 , wherein the branched to linear ratio of the alkyl chains is from 10:90 to 90:10 (weight % : weight %).
5. The method according to claim 1 , wherein the ratio of the number of building blocks a) and b) is from 75:25 to 50:50.
6. The method according to claim 1 , wherein the polymers have an acid value of less than 2 mg KOH/g, measured according to DIN EN 14104.
7. The method according to claim 1 , wherein the polymers comprise in total 50 to 150 building blocks a) and b) per polymer chain.
8. The method according to claim 1 , wherein 100 ppm to 2000 ppm (weight:weight) of the polymers are used in the paraffin-containing fluid.
9. The method according to claim 1 , wherein the polymer is used as being part of a liquid composition, comprising
(A) 1 to 50 wt. % of the polymers, dissolved in
(B) 99 to 50 wt. % of an aromatic solvent,
each relative to the total weight of (A) and (B).