US 10,524,491 · App. 15/808,110 · Granted Jan 7, 2020

Coated packaging products, systems and methods

Inventors: A. Gus Eskamani (Hudson, OH); Melanie Dorenkott (Westlake, OH); Tiffani A. Sutton-Gilbert (Cleveland, OH); Michael Kaminski (Elyria, OH); Michael A. Pintz (Fairview Park, OH); Ed Nolan (Medina, OH)
Assignee: Flavorseal LLC
A23L3/10B05D1/02A23V2002/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,524,491
App. No.
15/808,110
Granted
Jan 7, 2020
Kind
B2
Abstract

In a method of forming a coated bag for pre-treating an item stored in the bag, a bag is provided, having a sidewall extending from a closed bottom end to an open top end and defining an interior surface of a cavity. The bag is expanded from a flattened condition to an expanded condition. At least one adhesive dispenser is inserted through the open top end of the bag into the cavity. An adhesive is applied from the at least one inserted adhesive dispenser to form an adhesive coating on the interior surface of the cavity. A particulate dispenser is inserted through the open top end of the bag into the cavity. A particulate is discharged from the inserted particulate dispenser to embed the particulate in the adhesive coating. The adhesive coating is dried to retain the embedded particulate on the interior surface of the sidewall.

Claims (29)

1. A method of forming a coated bag for pre-treating an item stored in the bag, the method comprising:

providing a bag having a sidewall extending from a closed bottom end to an open top end and defining an interior surface of a cavity;

expanding the bag from a flattened condition to an expanded condition;

inserting at least one adhesive dispenser through the open top end of the bag into the cavity;

applying an adhesive from the at least one inserted adhesive dispenser to form an adhesive coating on the interior surface of the cavity;

inserting a particulate dispenser through the open top end of the bag into the cavity;

discharging a particulate from the inserted particulate dispenser to embed the particulate in the adhesive coating; and

drying the adhesive coating to retain the embedded particulate on the interior surface of the sidewall;

wherein the adhesive is a first adhesive and the adhesive coating is a first adhesive coating, the method further comprising applying a second adhesive from the at least one inserted adhesive dispenser to form a second adhesive coating on the embedded particulate, such that the embedded particulate is captured between the first and second adhesive coatings.

2. The method of claim 1 , wherein applying the adhesive comprises spraying a liquid adhesive having a viscosity between approximately 6 dPa and approximately 10 dPa.

3. The method of claim 1 , wherein applying the adhesive comprises spraying a liquid adhesive at a temperature between approximately 87° F. and approximately 175° F.

4. The method of claim 1 , wherein applying the adhesive comprises spraying a liquid adhesive at a pressure between approximately 200 psi and approximately 1300 psi.

5. The method of claim 1 , wherein applying the adhesive comprises spraying a liquid adhesive at a flow rate between about 1 g per second and about 2 g per second.

6. The method of claim 1 , wherein expanding the bag from the flattened condition to the expanded condition comprises applying suction to an outer surface of the sidewall.

7. The method of claim 1 , wherein drying the adhesive coating comprises maintaining the coated bag at a maximum temperature of up to approximately 160° F.

8. The method of claim 1 , wherein drying the adhesive coating comprises applying infrared radiation to an exterior surface of the bag.

9. The method of claim 1 , wherein discharging the particulate from the inserted particulate dispenser comprises discharging at least one of a seasoning particulate, a coloring particulate, and a preservative particulate.

10. The method of claim 1 , wherein the first and second adhesives are substantially the same material.

11. The method of claim 1 , wherein the first and second adhesives are applied at substantially the same temperature.

12. The method of claim 1 , wherein the first and second adhesives have substantially the same viscosity when applied.

13. The method of claim 1 , wherein discharging the particulate comprises discharging a first particulate, the method further comprising discharging a second particulate after applying the second adhesive, such that the second particulate is embedded in the second adhesive coating.

14. The method of claim 13 , further comprising applying a third adhesive from the at least one inserted adhesive dispenser after discharging the second particulate to form a third adhesive coating on the second embedded particulate, such that the second embedded particulate is captured between the second and third adhesive coatings.

15. The method of claim 1 , wherein the adhesive coating has an area density between approximately 20 mg/in 2 and approximately 60 mg/in 2 .

16. The method of claim 1 , wherein discharging the particulate comprises discharging a first particulate, the method further comprising discharging a second particulate after discharging the first particulate to embed the second particulate in the adhesive coating, the second particulate being different from the first particulate.

17. The method of claim 16 , wherein the first particulate has an average particle size that is at least 100 times an average particle size of the second particulate, the second particulate being embedded in the adhesive coating in spaces between the embedded first particulate.

18. The method of claim 1 , wherein the adhesive comprises an edible adhesive and the particulate comprises an edible particulate.

19. The method of claim 1 , wherein applying the adhesive to form the adhesive coating comprises spraying an aerated liquid adhesive to form an adhesive coating having gas bubbles trapped throughout the adhesive coating.

20. The method of claim 1 , wherein applying the adhesive to form the adhesive coating comprises spraying an aerated liquid adhesive to form a foamed adhesive coating on the interior surface of the cavity.

21. The method of claim 1 , wherein the interior surface has a surface tension between about 30 dynes/cm and about 38 dynes/cm.

Assignments (7)
RELEASE OF SECURITY INTEREST Recorded Aug 1, 2025
From: KEYBANK NATIONAL ASSOCIATION
To: OUTLOOK GROUP, LLC; FLAVORSEAL, LLC
Reel/Frame 071912/0103 →
RELEASE OF SECURITY INTEREST Recorded Aug 1, 2025
From: KEYBANK NATIONAL ASSOCIATION
To: FLAVORSEAL, LLC
Reel/Frame 071912/0047 →
SECURITY INTEREST Recorded Jul 3, 2025
From: FLAVORSEAL LLC; M&Q IP LEASING, LLC
To: BMO BANK N.A., AS AGENT
Reel/Frame 071602/0685 →
CORRECTIVE ASSIGNMENT TO CORRECT THE CORRECTIVE ASSIGNMENT TO CORRECT PATENT NUMBER 9984591 THAT SHOULD HAVE BEEN ENTERED AS 9984597 PREVIOUSLY RECORDED AT REEL: 062505 FRAME: 0770. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT. Recorded Dec 27, 2023
From: OUTLOOK GROUP, LLC; FLAVORSEAL, LLC
To: KEYBANK NATIONAL ASSOCIATION
Reel/Frame 066489/0054 →
SECURITY INTEREST Recorded Jan 27, 2023
From: OUTLOOK GROUP, LLC; FLAVORSEAL, LLC
To: KEYBANK NATIONAL ASSOCIATION
Reel/Frame 062505/0770 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 25, 2018
From: ESKAMANI, A. GUS, DR.; DORENKOTT, MELANIE; SUTTON-GILBERT, TIFFANI; KAMINSKI, MICHAEL; PINTZ, MICHAEL A.; NOLAN, ED
To: FLAVORSEAL LLC
Reel/Frame 045632/0140 →
SECURITY INTEREST Recorded Feb 12, 2018
From: FLAVORSEAL, LLC
To: KEYBANK NATIONAL ASSOCIATION
Reel/Frame 044893/0944 →
Continuity (3)
Division 15270463 · Sep 20, 2016
Provisional Application 62221172 · Sep 21, 2015
Related Publication 20180064145A1 · Mar 8, 2018
Cited By (1)
US 12,319,473