IP Library › Granted Patent US 10,836,144
Granted Patent B2
US 10,836,144 · App. 15/874,975 · Granted Nov 17, 2020

Self-healing glass panel

Inventors: Yali Li (Saline, MI); Mohammad Omar Faruque (Ann Arbor, MI)
Assignee: FORD GLOBAL TECHNOLOGIES, LLC
B32B17/10963B29C65/02B29C70/683B29C70/70B29C70/745B32B17/10036B32B17/10064B32B2305/72B32B2307/762B32B2605/006
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,836,144
App. No.
15/874,975
Granted
Nov 17, 2020
Kind
B2
Abstract

A self-healing glass panel includes first and second glass layers, a reservoir between the first and second glass layers, and a liquid healing agent for healing the first or second glass layers if a crack occurs. The liquid healing agent is entrapped in the reservoir by at least one of the first or second glass layers.

Claims (25)

1. A self-healing glass panel comprising:

first and second glass layers;

a reservoir between the first and second glass layers; and

a liquid healing agent for healing the first or second glass layers if a crack occurs, wherein the reservoir opens to both the first and second glass layers and the liquid healing agent is entrapped in the reservoir by the first and second glass layers.

2. The self-healing glass panel as recited in claim 1 , wherein the liquid healing agent is liquid over a temperature range of −40° F. to 200° F.

3. The self-healing glass panel as recited in claim 1 , wherein the liquid self-healing agent is silicone-based or epoxy-based.

4. The self-healing glass panel as recited in claim 1 , wherein the reservoir is a micro-reservoir.

5. The self-healing glass panel as recited in claim 1 , wherein the first and second glass layers and the liquid healing agent have substantially equivalent indices of refraction.

6. The self-healing glass panel as recited in claim 1 , wherein the liquid healing agent is curable upon exposure to moisture.

7. A self-healing glass panel comprising:

first and second glass layers;

a polymer interlayer sandwiched between the first and second glass layers, the polymer interlayer defining reservoirs therein, wherein the reservoir includes at least one of through-holes in the polymer interlayer or dimples in the polymer interlayer; and

a liquid healing agent for healing at least one of the first or second glass layers if a crack occurs, the liquid healing agent being disposed in the reservoirs and contained in the reservoirs by at least one of the first or second glass layers.

8. The self-healing glass panel as recited in claim 7 , wherein the reservoir includes the dimples, and the polymer interlayer and the first glass layer exclusively contain the liquid healing agent in the dimples.

9. The self-healing glass panel as recited in claim 7 , wherein the reservoir includes the through-holes, and the polymer interlayer and the first and second glass layers exclusively contain the liquid healing agent in the through-holes.

10. The self-healing glass panel as recited in claim 7 , wherein the reservoir include the dimple, the polymer interlayer has top and bottom sides, and the dimples are on both the top and bottom sides.

11. The self-healing glass panel as recited in claim 7 , wherein the reservoirs are arranged in a pattern.

12. The self-healing glass panel as recited in claim 7 , wherein the reservoirs are micro-reservoirs.

13. The self-healing glass panel as recited in claim 7 , wherein the liquid self-healing agent is silicone-based or epoxy-based.

14. A method of fabricating a self-healing glass panel, the method comprising:

depositing a liquid healing agent into reservoirs defined in a polymer interlayer, wherein the reservoirs include at least one of through-holes in the polymer interlayer or dimples in the polymer interlayer;

causing the liquid healing agent to immobilize in the reservoirs;

sandwiching polymer interlayer with the immobilized healing agent between first and second glass layers; and

after the sandwiching, causing the immobilized healing agent to mobilize, wherein the liquid healing agent is then contained in the reservoirs by at least one of the first or second glass layers.

15. The method as recited in claim 14 , wherein a reduction in temperature is used to cause the liquid healing agent to immobilize in the reservoirs, and an increase in temperature is used to cause the solidified healing agent to mobilize.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 19, 2018
From: LI, YALI; FARUQUE, MOHAMMAD OMAR
To: FORD GLOBAL TECHNOLOGIES, LLC
Reel/Frame 044662/0508 →
Continuity (1)
Related Publication 20190224949A1 · Jul 25, 2019