IP Library Granted Patent US 10,731,010
Granted Patent B2
US 10,731,010 · App. 16/002,044 · Granted Aug 4, 2020

Multi-ionic salts and uses thereof

Inventors: Stephanie Wunder (Chadds Ford, PA); Parameswara Rao Chinnam (Ambler, PA)
Assignee: TEMPLE UNIVERSITY—OF THE COMMONWEALTH SYSTEM OF HIGHER EDUCATION
C08G77/58C08G77/398C08K5/56H01M4/13H01M10/0568H01M10/0569C08G77/70H01M10/0525H01M2300/0028
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,731,010
App. No.
16/002,044
Granted
Aug 4, 2020
Kind
B2
Abstract

The invention provides a novel composition comprising a multi-ionic polyoligomeric silsesquioxane and a polyether solvent, optionally with an additional lithium salt. The composition of the invention allows for improved lithium ion transference over lithium salts alone by avoiding the problem of ion aggregation that reduces conductivity in single ion conductors. Also provided is a method for forming such a composition and a liquid electrolyte comprising a multi-ionic polyoligomeric silsesquioxane and a polyether solvent, optionally with an additional lithium salt.

Claims (40)

1. A composition comprising:

a polyether solvent; and

a polyoligomeric silsesquioxane of Formula (I):

[(O 1.5 )Si-L-X] n Y n ,  Formula (I);

wherein n is an even integer;

L is a divalent linking group;

Y is a cationic group selected from the group consisting of Li + , Na + , K + , and Mg 2+ ; and

X is an anionic group.

2. The composition of claim 1 , wherein the polyether solvent is tetraglyme.

3. The composition of claim 1 , wherein n is 8.

4. The composition of claim 1 , wherein L is selected from the group consisting of alkyl, siloxane, heteroatom, and combinations thereof.

5. The composition of claim 1 , wherein L is —OSi(Me) 2 (CH 2 ) 3 —; and wherein the O is bound to the silicon atom of Formula (I).

6. The composition of claim 1 , wherein X is —[NSO 2 CF 3 ] − .

7. The composition of claim 1 , wherein the polyoligomeric silsesquioxane of Formula (I) is a polyoligomeric silsesquioxane of Formula (II):

[(O 1.5 )Si—OSi(Me) 2 (CH 2 ) 3 —NSO 2 CF 3 ] n Li n ,  Formula (II);

wherein n is an even integer selected from the group consisting of 6, 8, 10, and 12.

8. The composition of claim 1 , further comprising an additional lithium salt.

9. The composition of claim 8 , wherein the additional lithium salt is selected from the group consisting of lithium bis(trifluoromethanesulfonyl)imide, lithium trifluoromethanesulfonate, and lithium tetrafluoroborate.

10. The composition of claim 8 , wherein the weight ratio of the additional lithium salt to the polyoligomeric silsesquioxane of Formula (I) is about 80/20.

11. The composition of claim 8 , wherein the ratio of the number ether oxygens in the polyether solvent to the number of Li + ions in the composition is between about 20/1 and about 9/1.

12. A liquid electrolyte comprising arrays of disordered particles of a polyoligomeric silsesquioxane of Formula (I) in a polyether solvent:

[(O 1.5 )Si-L-X] n Li n ,  Formula (I);

wherein in Formula (I), n is an even integer;

L is a divalent linking group; and

X is an anionic group.

13. The liquid electrolyte of claim 12 , further comprising lithium bis(trifluoromethanesulfonyl)imide.

14. The liquid electrolyte of claim 13 , wherein the ratio of the number ether oxygens in the polyether solvent to the number of Li + ions in the polyoligomeric silsesquioxane of Formula (I) and the lithium bis(trifluoromethanesulfonyl)imide is about 17.1/1.

15. The liquid electrolyte of claim 12 , wherein the polyether solvent is tetraglyme.

16. The liquid electrolyte of claim 12 , wherein L is —OSi(Me) 2 (CH 2 ) 3 —;

wherein the O is bound to the silicon atom of Formula (I); and

X is —[NSO 2 CF 3 ] − .

17. A battery comprising the liquid electrolyte of claim 12 .

18. A method for forming a composition, the method comprising:

adding a polyoligomeric silsesquioxane of Formula (I) to a polyether solvent under an inert atmosphere:

[(O 1.5 )Si-L-X] n Li n ,  Formula (I);

wherein in Formula (I), n is an even integer;

L is a divalent linking group; and

X is an anionic group.

19. The method of claim 18 , further comprising the step of adding an additional lithium salt to the polyether solvent.

20. The method of claim 19 , wherein the additional lithium salt is lithium bis(trifluoromethanesulfonyl)imide.

Assignments (2)
CONFIRMATORY LICENSE Recorded Feb 19, 2025
From: TEMPLE UNIVERSITY - OF THE COMMONWEALTH SYSTEMOF HIGHER EDUCATION
To: NATIONAL SCIENCE FOUNDATION
Reel/Frame 070253/0740 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 18, 2020
From: WUNDER, STEPHANIE L.; CHINNAM, PARAMESWARA RAO
To: TEMPLE UNIVERSITY-OF THE COMMONWEALTH SYSTEM OF HIGHER EDUCATION
Reel/Frame 052978/0187 →
Continuity (2)
Provisional Application 62516499 · Jun 7, 2017
Related Publication 20180355116A1 · Dec 13, 2018