Nanofibril cellulose additive
A variety of systems, methods and compositions are disclosed, including, in one method, a method for well treatment may comprise providing a treatment fluid comprising an aqueous base fluid; and a nanofribril cellulose additive, wherein the nanofribril cellulose additive comprises nanofribril cellulose and a surfactant adsorbed onto a surface of the nanofribril cellulose; and introducing the treatment fluid into a well bore penetrating a subterranean formation. Additional systems, methods and compositions are also disclosed.
1. A method for well treatment comprising:
preparing a treatment fluid comprising:
an aqueous base fluid; and
a nanofibril cellulose additive, wherein the nanofibril cellulose additive comprises nanofibril cellulose and a surfactant adsorbed onto a surface of the nanofibril cellulose, wherein the nanofibril cellulose additive is a particulate with a size ranging from about 5 microns to about 1,500 microns; and
introducing the treatment fluid into a well bore penetrating a subterranean formation.
2. The method of claim 1 , wherein the treatment fluid is a cement composition, a spacer fluid, a drilling fluid, or a fracturing fluid.
3. The method of claim 1 , wherein the treatment fluid is a cement composition further comprising a hydraulic cement.
4. The method of claim 1 , wherein the nanofibril cellulose comprises nanofibril cellulose derived from at least one cellulosic source selected from the group consisting of bacteria, wood, bleached kraft pulp, bleached sulfite pulp, sugar beet pulp, wheat straw, soy hulls, sisal, bagasse, palm trees, ramie, carrots, luffa cylindrical, and any combination thereof.
5. The method of claim 1 , wherein the nanofibril cellulose is an unmodified nanofibril cellulose that was treated with the surfactant.
6. The method of claim 1 , wherein the nanofibril cellulose additive is present in the treatment fluid in an amount of about 0.1% to about 10% by weight of the treatment fluid.
7. The method of claim 1 , wherein the nanofibril cellulose comprises individual nanofibrils with a diameter of about 100 nanometers or less and a length of about 3000 nanometers or greater.
8. The method of claim 1 , wherein the surfactant is a foaming surfactant selected from the group consisting of betaines, hydrolyzed keratin, amine oxides, cocoamidopropyl dimethylamine oxide, methyl ester sulfonates; alkyl or alkene amidobetaines, alpha-olefin sulfonates, quaternary surfactants, C8 to C22 alkylethoxylate sulfates, and combinations thereof.
9. The method of claim 1 , wherein the surfactant is a foaming surfactant comprising a mixture of an ethoxylated alcohol ether sulfate surfactant, an alkyl or alkene amidopropyl betaine surfactant, and an alkyl or alkene dimethylamine oxide surfactant.
10. The method of claim 1 , further comprising foaming the treatment fluid with a gas, wherein the surfactant is a foaming surfactant.
11. The method of claim 1 , wherein the nanofibril cellulose additive has a surface area of about 50 m 2 /g to about 70 m 2 /g.
12. The method of claim 1 , wherein the treatment fluid further comprises a cement, wherein the treatment fluid is foamed, and wherein the treatment fluid has a foam quality of about 18% to about 38%.
13. The method of claim 12 , wherein the foam quality is calculated by the following:
Foam
quality
=
Total
Foam
Volume
-
Liquid
Volume
Total
Foam
Volume
.
14. The method of claim 1 , wherein the nanofibril cellulose additive and the aqueous base fluid are present in a weight ratio ranging of about 1:2 to about 1:100.
15. A method for well treatment comprising:
preparing a treatment fluid comprising:
an aqueous base fluid; and
a nanofibril cellulose additive, wherein the nanofibril cellulose additive comprises nanofibril cellulose and a surfactant adsorbed onto a surface of the nanofibril cellulose, wherein the nanofibril cellulose and the surfactant are present in a weight ratio ranging from about 1:5 to about 1:12, wherein the nanofibril cellulose additive is a particulate with a size ranging from about 5 microns to about 1,500 microns;
introducing the treatment fluid into a well bore penetrating a subterranean formation.
16. The method of claim 15 , wherein the nanofibril cellulose additive has a surface area of about 50 m 2 /g to about 70 m 2 /g.
17. The method of claim 15 , wherein the treatment fluid further comprises a cement, wherein the treatment fluid is foamed, and wherein the treatment fluid has a foam quality of about 18% to about 38%.