Systems and methods to control lithium plating

Inventors: Hiroshi Imoto (Kakogawa, JP); Ken Ogata (Kakogawa, JP); Juichi Arai (Kakogawa, JP); Yang Yang (Kakogawa, JP)
Assignee: TeraWatt Technology Inc.
H01M50/449H01M4/133H01M4/1393H01M10/0525H01M50/403H01M50/411
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,462,804
App. No.
16/243,032
Granted
Oct 4, 2022
Kind
B2
Abstract

Various battery cell arrangements are presented herein. The battery cell can include an anode current collector. The battery cell can include a carbon-based anode coating layer that coats the anode current collector. A first bond between the anode current collector and the anode coating layer may have a first adhesion strength. The battery cell also includes a cathode, a separator layer that contacts the cathode, and a separator coating layer. The separator coating layer can be positioned between the anode coating layer and the separator layer. A second bond between the separator coating material and the anode coating material has a second adhesion strength. The second adhesion strength of the second bond may be greater than the first adhesion strength of the first bond.

Claims (38)

1. A battery cell, comprising:

an anode current collector comprising copper foil;

an anode coating layer that coats the anode current collector, wherein:

the anode coating layer comprises a lithium-ion conductive electrolyte;

a first bond between the anode current collector and the anode coating layer has a first adhesion strength; and

lithium metal plating occurs directly on a side of the copper foil of the anode current collector facing the anode coating layer during charging;

a cathode;

a separator layer that contacts the cathode;

a separator coating layer, distinct from the separator layer, wherein the separator coating layer is positioned between the anode coating layer and the separator layer, wherein:

a second bond between the separator coating layer and the anode coating layer has a second adhesion strength; and

the second adhesion strength of the second bond is greater than the first adhesion strength of the first bond.

2. The battery cell of claim 1 , wherein the separator coating layer comprises polyvinylidene fluoride (PVDF).

3. The battery cell of claim 1 , further comprising an electrolyte solution that permeates the cathode, the separator layer, and the separator coating layer.

4. The battery cell of claim 1 , wherein no lithium plating is present between the anode coating layer and the separator coating layer.

5. The battery cell of claim 1 , further comprising: a liquid electrolyte that is soaked into the cathode, anode coating layer, separator layer, and separator coating layer of the battery cell.

6. The battery cell of claim 1 , wherein the lithium-ion conductive electrolyte comprises one or more of a lithium ion conductive solid state electrolyte or a gel electrolyte.

7. The battery cell of claim 6 , wherein the lithium-ion conductive electrolyte comprises the gel electrolyte and the gel electrolyte comprises one or more of polyvinylidene flouride (PVdF), polyacrylonitrile (PAN), or polymethyl methacrylate (PMMA).

8. The battery cell of claim 6 , wherein the lithium-ion conductive electrolyte comprises the lithium ion conductive solid state electrolyte and the lithium ion conductive solid state electrolyte comprises an inorganic solid state electrolyte.

9. A method of creating a battery cell, the method comprising:

coating an anode current collector with an anode coating layer, wherein the anode current collector comprises copper foil, and wherein the anode coating layer comprises a lithium-ion conductive electrolyte;

coating a separator with a separator coating layer;

pressing the anode current collector toward the separator such that the anode coating layer is pressed against the separator coating layer; and

applying heat while the anode current collector is being pressed against the separator such that the anode coating layer is pressed against the separator coating layer, wherein

a first bond between the anode current collector and the anode coating layer has a first adhesion strength;

a second bond between the separator coating layer and the anode coating layer having a second adhesion strength is present;

the second adhesion strength of the second bond is greater than the first adhesion strength of the first bond; and

during charging, lithium metal plating occurs directly on the copper foil of the anode current collector.

10. The method of creating the battery cell of claim 9 , wherein the separator comprises polyvinylidene fluoride (PVDF).

11. The method of creating the battery cell of claim 9 , the method further comprising: adding an electrolyte solution that permeates a cathode of the battery cell, the separator, and the separator coating layer.

12. The method of creating the battery cell of claim 9 , wherein no lithium plating is present between the anode coating layer and the separator coating layer.

13. The method of creating the battery cell of claim 9 , wherein the lithium-ion conductive electrolyte comprises one or more of a solid state electrolyte layer or a gel electrolyte.

14. The method of creating the battery cell of claim 13 , wherein the lithium-ion conductive electrolyte comprises the gel electrolyte and the gel electrolyte comprises one or more of polyvinylidene flouride (PVdF), polyacrylonitrile (PAN), or polymethyl methacrylate (PMMA).

15. The method of creating the battery cell of claim 14 , further comprising gelling the gel electrolyte by adding an organic solvent.

16. The method of creating the battery cell of claim 13 , wherein the lithium-ion conductive electrolyte comprises a lithium ion conductive solid state electrolyte and the lithium ion conductive solid state electrolyte comprises an inorganic solid state electrolyte.

17. The method of creating the battery cell of claim 9 , wherein coating the separator with the separator coating layer comprises coating the separator with a PVdF slurry that comprises NMP (N-methylpyrrolidone).

18. The method of creating the battery cell of claim 9 , wherein pressing the anode current collector toward the separator comprises applying a pressure between 50 and 200 N/cm 2 .

19. The method of creating the battery cell of claim 9 , wherein the step of applying heat comprises applying heat at a temperature between 75 and 100 Celsius.

20. The method of creating the battery cell of claim 9 , further comprising rolling the battery cell to form a “jelly-roll” style battery cell.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 3, 2020
From: CHONGQING JINKANG NEW ENERGY AUTOMOBILE CO., LTD.
To: SF MOTORS, INC.
Reel/Frame 052823/0463 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 3, 2020
From: SF MOTORS, INC.
To: TERAWATT TECHNOLOGY INC.
Reel/Frame 052827/0684 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 8, 2019
From: IMOTO, HIROSHI; OGATA, KEN; ARAI, JUICHI; YANG, YANG
To: CHONGQING JINKANG NEW ENERGY AUTOMOBILE CO., LTD.; SF MOTORS INC.
Reel/Frame 047936/0443 →
Continuity (1)
Related Publication 20200220141A1 · Jul 9, 2020