Method of manufacturing microchannel chip
Disclosed is method of manufacturing a microchannel chip by joining together a resin channel substrate having microchannels formed on at least one side thereof and a resin lid substrate, the method including: a step (A) wherein surface modification treatment is applied on joining surfaces of the channel substrate and the lid substrate; and a step (B) wherein, after the step (A), the joining surfaces of the channel substrate and the lid substrate are mated and the channel substrate and the lid substrate are pressurized under heating via a fluid or an elastic body having a durometer hardness of E20 or less.
1. A method of manufacturing a microchannel chip by joining together a resin channel substrate having microchannels formed on at least one side thereof and a resin lid substrate, the method comprising:
a step (A) wherein surface modification treatment is applied on joining surfaces of the channel substrate and the lid substrate; and
a step (B) wherein, after the step (A), the joining surfaces of the channel substrate and the lid substrate are mated and the channel substrate and the lid substrate are pressurized under heating via a fluid or an elastic body having a durometer hardness of E20 or less, wherein
in the step (A), the surface modification treatment is applied using 3-aminopropyltrimethoxysilane for the joining surface of one of the channel substrate and the lid substrate and using 3-glycidoxypropyltrimethoxysilane for the joining surface of the other of the channel substrate and the lid substrate, and
the durometer hardness is measured using a type E durometer in accordance with JIS K6253.
2. The method of manufacturing a microchannel chip according to claim 1 , wherein the channel substrate and the lid substrate are made of cyclic olefin resin.
3. The method of manufacturing a microchannel chip according to claim 1 , wherein, in the step (B), an autoclave is used to pressurize the channel substrate and the lid substrate via the fluid.
4. The method of manufacturing a microchannel chip according to claim 3 , wherein, in the step (B), the channel substrate and the lid substrate, placed on top of each other, are accommodated in a bag, the interior of the bag is depressurized and hermetically sealed, the channel substrate and the lid substrate hermetically sealed within the bag are placed in the autoclave, and the channel substrate and the lid substrate are pressurized via the fluid.