IP Library › Granted Patent US 10,908,321
Granted Patent B2
US 10,908,321 · App. 16/582,152 · Granted Feb 2, 2021

Glass laminate, front plate for display, and display device

Inventors: Kensuke Fujii (Tokyo, JP); Michinori Suehara (Tokyo, JP); Kazunari Tohyama (Tokyo, JP)
Assignee: AGC Inc.
G02B1/115B32B17/10036C03C17/36G02B5/282
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,908,321
App. No.
16/582,152
Granted
Feb 2, 2021
Kind
B2
Abstract

A glass laminate includes a glass substrate including a first main surface and a second main surface, and a functional layer at least on the first main surface. The functional layer includes at least two layers having a refractive index different from each other and the at least two layers are alternately laminated. The functional layer includes an outermost layer farthest from the glass substrate and a second layer that is adjacent to the outermost layer and lies closer to the glass substrate than the outermost layer. The outermost layer includes SiO 2 as a main component. The second layer has a carbon concentration of 3×10 18 atoms/cm 3 or more and 5×10 19 atoms/cm 3 or less, and the carbon concentration of the second layer is lower than that of the outermost layer.

Claims (21)

1. A glass laminate, comprising:

a glass substrate including a first main surface and a second main surface; and

a functional layer at least on the first main surface, the functional layer including at least two layers having a refractive index different from each other, the at least two layers being alternately laminated,

wherein the functional layer includes an outermost layer farthest from the glass substrate, the outermost layer including SiO 2 as a main component, and

the functional layer includes a second layer that is adjacent to the outermost layer and lies closer to the glass substrate than the outermost layer, the second layer having a carbon concentration of 3×10 18 atoms/cm 3 or more and 5×10 19 atoms/cm 3 or less, and the carbon concentration of the second layer is lower than a carbon concentration of the outermost layer.

2. The glass laminate according to claim 1 , wherein the functional layer includes at least one low refractive index layer and at least one high refractive index layer having a refractive index higher than the low refractive index layer, and the layer number of the low refractive index layer is 1 or more and 6 or less and the layer number of the high refractive index layer is same as the layer number of the low refractive index layer.

3. The glass laminate according to claim 2 , wherein the layer number of each of the low refractive index layer and the high refractive index layer is 1,

the outermost layer is the low refractive index layer, and

the high refractive index layer includes, as a main component, any one of SiN, TiO 2 , Nb 2 O 5 , Ta 2 O 5 , and ZrO 2 .

4. The glass laminate according to claim 2 , wherein the layer number of each of the low refractive index layer and the high refractive index layer is 2 or more and 6 or less, the outermost layer is one layer of the low refractive index layers,

each of the high refractive index layers includes, as a main component, any one of SiN, TiO 2 , Nb 2 O 5 , Ta 2 O 5 , and ZrO 2 , and

the main component of all of the high refractive index layers is the same, or the main component of at least one layer of the high refractive index layers is different from the main component of the other high refractive index layer(s).

5. The glass laminate according to claim 1 , further comprising an antifouling layer on the outermost layer.

6. The glass laminate according to claim 5 , wherein the antifouling layer is formed of a fluorine-based silane coupling material.

7. The glass laminate according to claim 5 , wherein the carbon concentration of the outermost layer is 5×10 18 atoms/cm 3 or more and 6×10 19 atoms/cm 3 or less.

8. The glass laminate according to claim 1 , wherein the first main surface of the glass substrate has an antiglare layer.

9. The glass laminate according to claim 1 , wherein the functional layer includes a main surface that does not face the glass substrate, the main surface having a concave-convex shape, and

the concave-convex shape has a root mean square roughness (RMS) of 10 nm or more and 1,000 nm or less.

10. The glass laminate according to claim 1 , wherein the outermost layer includes Al—SiO 2 .

11. A front plate for display, comprising the glass laminate according to claim 1 .

12. A display device, comprising the front plate for display according to claim 11 .

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 25, 2019
From: FUJII, KENSUKE; SUEHARA, MICHINORI; TOHYAMA, KAZUNARI
To: AGC INC.
Reel/Frame 050485/0598 →
Priority Claims (1)
JP 2018-186454 · Oct 1, 2018 · national
Continuity (1)
Related Publication 20200103559A1 · Apr 2, 2020
Cited By (1)
US 12,307,998