Ink composition for inkjet printing organic light-emitting diodes and method of manufacturing the same

Inventors: Xianglong Li (Guangdong, CN); Hong Meng (Guangdong, CN)
Assignee: SHENZHEN CHINA STAR OPTOELECTRONICS SEMICONDUCTOR DISPLAY TECHNOLOGY CO., LTD.
C09D11/38C09D11/36H01L51/0059H01L51/0061H01L51/0062H01L51/0072H01L51/0005
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,441,045
App. No.
16/649,999
Granted
Sep 13, 2022
Kind
B2
Abstract

An ink composition for inkjet printing organic light-emitting diodes and a method of manufacturing the same are disclosed. The ink composition includes 0.01-40% of bipolar light emission component, 10-99.9% of solvent, 0.01-5% of surface tension modifier, and 0.01-5% of viscosity modifier by weight. The method of manufacturing the ink composition includes steps of: dispersing the bipolar light emission component in the solvent firstly, and then adding the viscosity modifier and the surface tension modifier under stirring, so as to obtain the ink composition. By using the ink composition, specific hole and electron transport layers provided in the organic light-emitting diode manufactured by inkjet printing may be omitted, thereby simplifying the structure of the organic light-emitting diode. Moreover, the ink composition has suitable viscosity, surface tension, and volatility.

Claims (21)

1. An ink composition for inkjet printing organic light-emitting diodes, comprising: 20% of bipolar light emission component, 70% of solvent, 2% of surface tension modifier, and 2% of viscosity modifier by weight,

wherein the bipolar light emission component is single-component light emission material selected from a group consisting of fluorescence material, phosphorescence material, thermally activated delayed fluorescence material, room temperature phosphorescence material, aggregation-induced delayed fluorescence material, free radical material, quantum dot material, excimer material, and exciplex material; or

the bipolar light emission component is multi-component light emission material and comprises light emission material and host material, wherein the light emission material is selected from a group consisting of fluorescent material, phosphorescence material, thermally activated delayed fluorescence material, room temperature phosphorescence material, aggregation-induced delayed fluorescence material, free radical material, quantum dot material, excimer material, and exciplex material, and the host material is selected from single-component bipolar host material or multi-component bipolar host material.

2. The ink composition of claim 1 , wherein the single-component bipolar host material is selected from a group consisting of CBP, 26DczPPy, and 35DczPPy, and the multi-component bipolar host material is selected from a group consisting of TCTA/26DczPPy, mCP/B3PyMPM, PVK/OXD-7, TCTA/B3PyMPM, m-MTDATA/OXD-7, and NPB/PO-T2T.

3. The ink composition of claim 1 , wherein the solvent includes one of alkane hydrocarbon compound, aromatic hydrocarbon compound, alcohol compound, and high boiling point solvent.

4. The ink composition of claim 3 , wherein the high boiling point solvent is selected from a group consisting of ether compound, ester compound, and aromatic compound.

5. The ink composition of claim 1 , wherein the surface tension modifier is selected from one or more of a group consisting of cosolvent and surfactant.

6. The ink composition of claim 1 , wherein the surface tension modifier is selected from one or more of a group consisting of imidazole and a derivative thereof, phenol, and hydroquinone.

7. The ink composition of claim 1 , wherein the viscosity modifier is selected from one or more of a group consisting of alcohol, ether, ester, phenol, and amine.

8. An ink composition for inkjet printing organic light-emitting diodes, comprising: 0.01-40% of bipolar light emission component, 10-99.9% of solvent, 0.01-5% of surface tension modifier, and 0.01-5% of viscosity modifier by weight,

wherein the bipolar light emission component is single-component light emission material selected from a group consisting of fluorescence material, phosphorescence material, thermally activated delayed fluorescence material, room temperature phosphorescence material, aggregation-induced delayed fluorescence material, free radical material, quantum dot material, excimer material, and exciplex material; or

the bipolar light emission component is multi-component light emission material and comprises light emission material and host material, wherein the light emission material is selected from a group consisting of fluorescent material, phosphorescence material, thermally activated delayed fluorescence material, room temperature phosphorescence material, aggregation-induced delayed fluorescence material, free radical material, quantum dot material, excimer material, and exciplex material, and the host material is selected from single-component bipolar host material or multi-component bipolar host material.

9. The ink composition of claim 8 , wherein the single-component bipolar host material is selected from a group consisting of CBP, 26DczPPy, and 35DczPPy, and the multi-component bipolar host material is selected from a group consisting of TCTA/26DczPPy, mCP/B3PyMPM, PVK/OXD-7, TCTA/B3PyMPM, m-MTDATA/OXD-7, and NPB/PO-T2T.

10. The ink composition of claim 8 , wherein the solvent includes one of alkane hydrocarbon compound, aromatic hydrocarbon compound, alcohol compound, and high boiling point solvent.

11. The ink composition of claim 10 , wherein the high boiling point solvent is selected from a group consisting of ether compound, ester compound, and aromatic compound.

12. The ink composition of claim 8 , wherein the surface tension modifier is selected from one or more of a group consisting of cosolvent and surfactant.

13. The ink composition of claim 8 , wherein the surface tension modifier is selected from one or more of a group consisting of imidazole and a derivative thereof, phenol, and hydroquinone.

14. The ink composition of claim 8 , wherein the viscosity modifier is selected from one or more of a group consisting of alcohol, ether, ester, phenol, and amine.

15. A method of manufacturing the ink composition for inkjet printing organic light-emitting diode according to any one of claim 8 , comprising steps of:

dispersing the bipolar light emission component in the solvent to obtain a pre-formed composition; and

adding the viscosity modifier and the surface tension modifier into the pre-formed composition under stirring to obtain the ink composition.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 24, 2020
From: LI, XIANGLONG; MENG, HONG
To: SHENZHEN CHINA STAR OPTOELECTRONICS SEMICONDUCTOR DISPLAY TECHNOLOGY CO., LTD.
Reel/Frame 052203/0117 →
Priority Claims (1)
CN 201911296708.5 · Dec 16, 2019 · national
Continuity (1)
Related Publication 20210179876A1 · Jun 17, 2021