Methods and apparatus for compensating for material distortion during additive manufacturing

Inventors: Kenneth J. Susnjara (Birdseye, IN); Scott G. Vaal (Jasper, IN)
Assignee: Thermwood Corporation
B29C64/106B29C64/194B29C64/393B33Y10/00B33Y30/00B33Y40/00B33Y50/02
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,800,093
App. No.
16/677,194
Granted
Oct 13, 2020
Kind
B2
Abstract

Embodiments of the present disclosure are drawn to additive manufacturing methods. An exemplary method may include generating a tool path for forming a component via additive manufacturing, and assessing the tool path to identify a change in direction. The method may also include determining if the change in direction exceeds a predetermined angle, and adding a tangent arc to the tool path before the change in direction if the change in direction exceeds the predetermined angle.

Claims (28)

1. An additive manufacturing method, comprising:

generating a tool path including a first portion and a second portion, the tool path including an outward diversion with respect to the first portion;

moving a nozzle and a roller according to the first portion of the tool path while depositing heated material with the nozzle;

moving the nozzle and the roller according to the outward diversion while depositing the heated material prior to the second portion of the tool path; and

engaging the deposited heated material with the roller to move at least a portion of the heated material deposited along the outward diversion toward the second portion, wherein the second portion and the first portion extend in different directions.

2. The method of claim 1 , wherein the outward diversion is added to the tool path after the generation of the tool path including the first portion and the second portion.

3. The method of claim 1 , wherein the outward diversion has a shape of an outward bulge with respect to the first portion.

4. The method of claim 3 , wherein the outward bulge is positioned between the first portion and the second portion.

5. The method of claim 1 , further including positioning the roller in alignment with the outward diversion and out of alignment with the first portion prior to moving the roller according to the second portion.

6. The method of claim 1 , further including positioning the roller in alignment with the outward diversion such that a central portion of the roller overlaps a portion of the outward diversion having a largest deviation with respect to the first portion.

7. The method of claim 1 , wherein a location of the outward diversion is based on an angle formed by the first portion and the second portion.

8. The method of claim 1 , wherein a shape of the outward diversion is determined based on an angle of a change in direction formed by the first portion and the second portion.

9. The method of claim 1 , wherein the outward diversion connects the first portion of the tool path and the second portion of the tool path.

10. The method of claim 9 , wherein the outward diversion includes a portion that diverts away from the first portion and away from the second portion.

11. The method of claim 10 , wherein the deposited heated material that was deposited when moving the nozzle according to the outward diversion is engaged by the roller and moved toward the first portion and toward the second portion.

12. An additive manufacturing method, comprising:

generating a tool path including a first portion and a second portion;

adding an outward bulge to the tool path at the end of the first portion;

moving a nozzle according to the first portion of the tool path while depositing material,

diverting the nozzle along the outward bulge while depositing the material, prior to moving the nozzle according to the second portion; and

engaging the deposited material with the roller to move at least a portion of the material deposited along the outward bulge toward the second portion, wherein the second portion and the first portion extend in different directions.

13. The method of claim 12 , wherein the outward bulge is added to the tool path after generation of the first portion and the second portion of the tool path.

14. The method of claim 12 , wherein the outward bulge is formed in a direction opposite to the second portion of the tool path.

15. The method of claim 12 , further including moving the roller away from the first portion and the outward bulge prior to moving the roller according to the second portion.

16. The method of claim 15 , further comprising rotating the roller to a location opposite to the second portion before moving the nozzle along the second portion.

17. The method of claim 12 , wherein a location of the outward bulge is based on an angle formed by the first portion and the second portion.

18. The method of claim 12 , wherein the outward bulge connects the first portion of the tool path and the second portion of the tool path.

19. The method of claim 12 , wherein the material that was deposited when moving the nozzle according to the outward diversion is engaged by the roller to move the deposited material toward the first portion and toward the second portion.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 11, 2019
From: SUSNJARA, KENNETH J.; VAAL, SCOTT G.
To: THERMWOOD CORPORATION
Reel/Frame 050972/0396 →
Continuity (2)
Continuation 15435431 · Feb 17, 2017
Related Publication 20200139615A1 · May 7, 2020
Cited By (1)
US 12,605,883