IP Library Granted Patent US 11,014,823
Granted Patent B2
US 11,014,823 · App. 16/704,088 · Granted May 25, 2021

Recovering a caustic solution via calcium carbonate crystal aggregates

Inventors: Kenton Robert Heidel (Calgary, CA); David William Keith (Canmore, CA); Jane Anne Ritchie (Calgary, CA); Nicholas Vollendorf (New Berlin, WI); Eric Fessler (Brookfield, WI)
Assignee: Carbon Engineering Ltd.
C01F11/182B01D9/0036C01F11/181C01F11/183D21C11/0078B01D2009/0086C01P2004/61C01P2004/62Y02P40/40
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,014,823
App. No.
16/704,088
Granted
May 25, 2021
Kind
B2
Abstract

Techniques for growing crystalline calcium carbonate solids such that the crystalline calcium carbonate solids include a volume of 0.0005 mm 3 to 5 mm 3 , include a slaker to react quicklime (CaO) and a low carbonate content fluid to yield a slurry of primarily slaked lime (Ca(OH) 2 ); a fluidized-bed reactive crystallizer that encloses a solid bed mass and includes an input for a slurry of primarily slaked lime, an input for an alkaline solution and carbonate, and an output for crystalline calcium carbonate solids that include particles and an alkaline carbonate solution; a dewatering apparatus that includes an input coupled to the crystallizer and an output to discharge a plurality of separate streams that each include a portion of the crystalline calcium carbonate solids and alkaline carbonate solution; and a seed transfer apparatus to deliver seed material into the crystallizer to maintain a consistent mass of seed material.

Claims (33)

1. A method for growing crystalline calcium carbonate solids in the presence of an alkaline carbonate solution in a fluidized-bed reactive crystallizer the method comprising:

reacting, in a slaking process, quicklime (CaO) and a low carbonate content fluid to yield a slurry of primarily slaked lime (Ca(OH) 2 );

introducing the slurry of primarily slaked lime and the alkaline carbonate solution comprising between 0.1 M to 4.0 M hydroxide and between 0.1 M to 4.1 M carbonate into a fluidized-bed reactive crystallizer comprising a bed of solid particles flowing the slurry of primarily slaked lime and the alkaline carbonate solution through the fluidized-bed reactive crystallizer to fluidize the bed of solid particles, the slurry of primarily slaked lime and the alkaline carbonate solution having a fluidization flow velocity within a range of 2 m/h to 70 m/h;

reacting the Ca(OH) 2 slurry and the alkaline carbonate solution to deposit a portion of precipitated calcium carbonate (CaCO 3 ) onto the bed of solid particles; and

discharging a portion of the bed of solid particles and the alkaline carbonate solution.

2. The method of claim 1 , wherein discharging a portion of the bed of solid particles and the alkaline carbonate solution includes discharging one or more solid particles with a diameter from 0.1 mm to 0.4 mm.

3. The method of claim 2 , wherein:

discharging a portion of the bed of solid particles and the alkaline carbonate solution includes discharging one or more solid particles comprising a volume from 0.0005 mm 3 to 0.035 mm 3 .

4. The method of claim 1 , wherein introducing the slurry of primarily slaked lime comprises injecting the slurry into a recirculation stream influent upstream of the fluidized-bed reactive crystallizer.

5. The method of claim 4 , wherein introducing the alkaline carbonate solution comprises injecting the alkaline carbonate solution into the recirculation stream influent upstream of the fluidized-bed reactive crystallizer.

6. The method of claim 1 , further comprising introducing an additive.

7. The method of claim 6 , wherein introducing an additive includes introducing an additive comprising at least one of: nitrilotriacetic acid, phenol, sucrose, NH 4 Cl, and H-EDTA.

8. The method of claim 1 , further comprising extending a height of the bed of solid particles to between 15 feet and 50 feet.

9. The method of claim 1 , further comprising controlling a level of total suspended solids within the fluidized-bed reactive crystallizer to between 100 ppm and 1500 ppm.

10. The method of claim 1 , wherein discharging a fraction of the bed of solid particles and the alkaline carbonate solution includes discharging a set of solid particles comprising a diameter within a range of 0.1 mm to 0.2 mm.

11. The method of claim 1 , further comprising increasing a volume of the solid particles by reacting the Ca(OH) 2 slurry and the alkaline carbonate solution to deposit a portion of the precipitated calcium carbonate (CaCO 3 ) onto the bed of solid particles.

12. The method of claim 1 , further comprising decreasing a concentration of dissolved carbonate by reacting the Ca(OH) 2 slurry and the alkaline carbonate solution to deposit a portion of the precipitated calcium carbonate (CaCO 3 ) onto the bed of solid particles.

13. The method of claim 1 , increasing a concentration of dissolved hydroxide by reacting the Ca(OH) 2 slurry and the alkaline carbonate solution to deposit a portion of the precipitated calcium carbonate (CaCO 3 ) onto the bed of solid particles.

14. A method for growing crystalline calcium carbonate solids in the presence of an alkaline carbonate solution in a fluidized-bed reactive crystallizer, the method comprising:

introducing a slurry of primarily slaked lime and an alkaline carbonate solution comprising between 0.1 M to 4.0 M hydroxide and between 0.1 M to 4.1 M carbonate into a fluidized-bed reactive crystallizer comprising a bed of solid particles;

adding the slurry of primarily slaked lime to the fluidized-bed reactive crystallizer at a loading rate between 5 kg-Ca/m 2 /h to 35 kg-Ca/m 2 /h;

flowing the slurry of primarily slaked lime and the alkaline carbonate solution through the fluidized-bed reactive crystallizer to fluidize the bed of solid particles;

reacting the slurry of primarily slaked lime and the alkaline carbonate solution to deposit a portion of precipitated calcium carbonate (CaCO 3 ) onto the bed of solid particles; and

discharging a portion of the bed of solid particles and the alkaline carbonate solution.

15. The method of claim 14 , wherein introducing the slurry of primarily slaked lime and the alkaline carbonate solution into a fluidized-bed reactive crystallizer includes introducing the slurry of primarily slaked lime at one or more entry points.

16. The method of claim 14 , wherein introducing the slurry of primarily slaked lime comprises injecting the slurry into a recirculation stream influent upstream of the fluidized-bed reactive crystallizer.

17. The method of claim 16 , wherein introducing the slurry of primarily slaked lime and the alkaline carbonate solution comprises injecting the alkaline carbonate solution into the recirculation stream influent upstream of the fluidized-bed reactive crystallizer.

18. The method of claim 14 , further comprising introducing an additive.

19. The method of claim 18 , wherein introducing the additive includes introducing an additive comprising at least one of: nitrilotriacetic acid, phenol, sucrose, NH 4 Cl, and H-EDTA.

20. The method of claim 14 , further comprising extending a height of the bed of solid particles to between 15 feet and 50 feet.

21. The method of claim 14 , further comprising controlling a level of total suspended solids within the fluidized-bed reactive crystallizer to between 100 ppm and 1500 ppm.

22. The method of claim 14 , further comprising reacting, in a slaking process, quicklime (CaO) and a low carbonate content fluid to yield the slurry of primarily slaked lime, wherein reacting quicklime and a low carbonate content fluid includes supplying 10 moles of quicklime (CaO) per 1 mole of dissolved carbonate.

23. The method of claim 22 , wherein supplying 10 moles of CaO per 1 mole of dissolved carbonate to a slaker reduces a portion of solid particles in the fluidized-bed reactive crystallizer having a volume less than a volume of a 100 μm diameter sphere.

Assignments (5)
CHANGE OF NAME Recorded Feb 28, 2024
From: CARBON ENGINEERING LTD.
To: CARBON ENGINEERING ULC
Reel/Frame 066593/0551 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 5, 2019
From: VOLLENDORF, NICHOLAS; FESSLER, ERIC
To: PROCORP ENTERPRISES LLC
Reel/Frame 051189/0265 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 5, 2019
From: HEIDEL, KENTON ROBERT; KEITH, DAVID WILLIAM; RITCHIE, JANE ANNE
To: CARBON ENGINEERING LIMITED PARTNERSHIP
Reel/Frame 051189/0350 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 5, 2019
From: PROCORP ENTERPRISES LLC
To: CARBON ENGINEERING LIMITED PARTNERSHIP
Reel/Frame 051189/0419 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 5, 2019
From: CARBON ENGINEERING LIMITED PARTNERSHIP
To: CARBON ENGINEERING LTD.
Reel/Frame 051189/0474 →
Continuity (3)
Continuation 15370620 · Dec 6, 2016
Division 14281430 · May 19, 2014
Related Publication 20200109059A1 · Apr 9, 2020
Cited By (3)
US 12,583,756 US 12,654,132 US 12,714,966