IP Library Granted Patent US 12,372,116
Granted Patent B1
US 12,372,116 · App. 16/805,966 · Granted Jul 29, 2025

System and method for lubricating surfaces of parts

Inventors: Michael Richard Herzberg (Kansas City, MO); Brandon Kyle Leslie (Lee's Summit, MO); Joshua Michael Schnitzler (Lee's Summit, MO); Krishawn Michele Goodwin (Lee's Summit, MO)
Assignee: Honeywell Federal Manufacturing & Technologies, LLC
F16C33/1095C10M103/00C10M103/02C10M103/06C23C8/80F16C33/043B23K26/0093B23K26/352C23C4/11
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,372,116
App. No.
16/805,966
Granted
Jul 29, 2025
Kind
B1
Abstract

A method for lubricating a surface of an object comprises generating and directing a laser beam to strike the surface of the object to create an oxide area on the surface struck by the laser beam; and applying a dry film lubricant to the oxide area.

Claims (27)

1. A method for lubricating a surface of an object, the method comprising:

generating and directing a laser beam to strike the surface of the object to create an oxide area on the surface struck by the laser beam; and

applying a dry film lubricant in a powder form to the oxide area.

2. The method of claim 1 , wherein directing the laser beam includes directing the laser beam to strike selective areas on the surface of the object.

3. The method of claim 1 , wherein directing the laser beam includes directing the laser beam to strike a pattern on the surface of the object.

4. The method of claim 1 , wherein the laser beam is generated to have a wavelength ranging from approximately 700 nanometers to approximately 1400 nanometers.

5. The method of claim 1 , wherein the laser beam is generated to have an average power ranging from approximately 5 Watts to approximately 30 watts.

6. The method of claim 1 , wherein the dry film lubricant includes molybdenum disulfide.

7. The method of claim 1 , wherein the dry film lubricant includes tungsten disulfide.

8. The method of claim 1 , wherein the dry film lubricant includes graphite.

9. A method for lubricating a surface of an object, the method comprising:

generating and directing a laser beam to strike the surface of the object to create an oxide area on the surface struck by the laser beam, wherein the laser beam is generated to have a wavelength ranging from approximately 700 nanometers to approximately 1400 nanometers and to have an average power ranging from approximately 5 Watts to approximately 30 watts; and

applying a dry film lubricant including molybdenum disulfide in a powder form to the oxide area.

10. The method of claim 9 , wherein directing the laser beam includes directing the laser beam to strike selective areas on the surface of the object.

11. The method of claim 9 , wherein directing the laser beam includes directing the laser beam to strike a pattern on the surface of the object.

12. A system for lubricating a surface of an object, the system comprising:

a laser system configured to generate and direct a laser beam to strike the surface of the object to create an oxide area on the surface struck by the laser beam; and

a dry film lubricant in a powder form configured to be applied to the oxide area.

13. The system of claim 12 , wherein the laser system directs the laser beam to strike selective areas on the surface of the object.

14. The system of claim 12 , wherein the laser system directs the laser beam to strike a pattern on the surface of the object.

15. The system of claim 12 , wherein the laser system generates the laser beam to have a wavelength ranging from approximately 700 nanometers to approximately 1400 nanometers.

16. The system of claim 12 , wherein the laser system generates the laser beam to have an average power ranging from approximately 5 Watts to approximately 30 watts.

17. The system of claim 12 , wherein the dry film lubricant includes molybdenum disulfide.

18. The system of claim 12 , wherein the dry film lubricant includes tungsten disulfide.

19. The system of claim 12 , wherein the dry film lubricant includes graphite.

20. The system of claim 12 , wherein the laser system generates the laser beam to have a wavelength ranging from approximately 700 nanometers to approximately 1400 nanometers and to have an average power ranging from approximately 5 Watts to approximately 30 watts.

21. The method of claim 1 , wherein the dry film lubricant is applied to the oxide area through a supply line propelled by a compressed gas.

Assignments (3)
CONFIRMATORY LICENSE Recorded Aug 27, 2025
From: HONEYWELL FEDERAL MANUFACTURING & TECHNOLOGIES, LLC
To: NNSA
Reel/Frame 072613/0544 →
CONFIRMATORY LICENSE Recorded Jan 9, 2023
From: HONEYWELL FEDERAL MANUFACTURING & TECHNOLOGIES, LLC (FM&T)
To: U.S. DEPARTMENT OF ENERGY
Reel/Frame 062313/0076 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 16, 2020
From: HERZBERG, MICHAEL RICHARD; LESLIE, BRANDON KYLE; SCHNITZLER, JOSHUA MICHAEL; GOODWIN, KRISHAWN MICHELE
To: HONEYWELL FEDERAL MANUFACTURING & TECHNOLOGIES, LLC
Reel/Frame 052123/0212 →
References Cited (7)
US 3157529A · Sliney · 1964 [cited by applicant]
US 4227756A · Bhushan · 1980 [cited by applicant]
US 5259965A · Kishi · 1993 [cited by examiner]
US 20020183209A1 · Jee · 2002 [cited by examiner]
EP 0614195 · 1994 [cited by applicant]
EP 0614195A1 · 1994 [cited by examiner]
Office Action mailed Dec. 12, 2024 in related U.S. Appl. No. 17/986,263, 7 pages. [cited by applicant]