Nonaqueous electrolyte secondary battery and method for manufacturing nonaqueous electrolyte secondary batteries
An object of the present disclosure is to provide a nonaqueous electrolyte secondary battery resistant to the occurrence of electrode plate deformation which can cause an internal short circuit. A nonaqueous electrolyte secondary battery according to an example embodiment of the present disclosure includes a wound electrode assembly including a positive electrode, a negative electrode and a separator, and a nonaqueous electrolyte. The separator is bonded to the positive electrode over a region from the end of the positive electrode on the coiling start side to a length corresponding to at least one loop in the winding direction.
1 . A method for manufacturing a cylindrical nonaqueous electrolyte secondary battery comprising a wound electrode assembly including a positive electrode having a positive electrode core and positive electrode mixture layers disposed on both faces of the positive electrode core, a negative electrode having a negative electrode core and negative electrode mixture layers disposed on both faces of the negative electrode core, and a separator interposed between the positive electrode and the negative electrode; a nonaqueous electrolyte; and a battery case accommodating the electrode assembly and the nonaqueous electrolyte, wherein
the method comprises:
a step of connecting an electrode lead to an end portion of the electrode assembly on a coiling start side,
a placement step of placing the electrode assembly and the nonaqueous electrolyte into the battery case, the electrode assembly including the separator comprising a resin layer in a non-adhesive state with respect to the positive electrode in the placement step, and
after the placement step, a step of heating the resin layer by discharging an electrical current at not less than 20 A through the electrode lead, wherein said heating causes the resin layer to exhibit adhesion to the positive electrode, so as to bond the separator to the positive electrode over a region from an end of the positive electrode mixture layer on a coiling start side to a length corresponding to at least one loop in a winding direction.