Continuous manufacturing of surface wrinkle features
Provided are systems and methods for inducing strain fields to give rise to controllable wrinkle patterns in a variety of substrates. Also provided are articles having persistent wrinkling patterns thereon.
1. A method, comprising:
(a) with a working material that comprises an elastomeric material and a second material that defines the uppermost portion of the working material,
effecting a stress within the working material, the effecting being accomplished by transiently contacting the elastomeric material to a continuously revolving, curved support substrate,
at least partially releasing the stress within the working material so as to give rise to a plurality of persistent wrinkles in the uppermost portion of the working material, or
(b) applying a stimulus so as to change a mechanical property of an uppermost portion of a working material that comprises an elastomeric material,
effecting a stress within the working material, the effecting being accomplished by transiently contacting the elastomeric material to a continuously revolving, curved support substrate, and
at least partially releasing the stress within the working material so as to give rise to a plurality of persistent wrinkles in the uppermost portion of the working material; or
(c) any combination of (a) or (b).
2. The method of claim 1 , further comprising depositing the second material atop the elastomeric material so as to give rise to the working material.
3. The method of claim 1 , wherein the support substrate is characterized as cylindrical, spherical, toroidal, spheroidal, polyhedral, or any combination thereof.
4. The method of claim 1 , wherein the stimulus, if present, comprises a radiation, a molecular species, a chemical reaction, or any combination thereof.
5. The method of claim 1 , wherein (a) the second material is characterized as bonded to the elastomeric material, (b) the second material has a Young's modulus that is greater than the Young's modulus of the elastomeric material, or both (a) and (b).
6. The method of claim 1 , wherein (a) the plurality of persistent wrinkles has a wavelength of from about 100 nm to about 100 um, (b) the plurality of persistent wrinkles has an amplitude of from about 50 nm to about 20 um, or both (a) and (b).
7. The method of claim 1 , wherein the plurality of persistent wrinkles are characterized as parallel wrinkles, herringbone wrinkles, or disordered wrinkles.
8. The method of claim 1 , further comprising applying a stimulus so as to change a mechanical property of the uppermost portion of the working material.