Modification of particles for additive manufacturing
Atomic Layer Deposition (ALD) and Molecular Layer Deposition (MLD) provide precise and conformal coatings that are employed to modify the properties of powders for additive manufacturing (AM). We have surprisingly discovered that use of a limited number of ALD cycles can impart improved flowability. In various aspects, the coating may provide one or more advantages such as novel material properties, increased flowability, improved sintering, enhanced stability during storage, and prevention of premature sintering.
1. A method of making a shaped object, comprising:
providing a powder comprising core particles comprising a metal or ceramic core;
reacting the powder with a first reactant (reactant A) following by reaction with a second reactant (reactant B) in a process of atomic (ALD) or molecular layer deposition (MLD) in a sequential manner to produce a powder comprising an ALD/MLD coating having alternating, bonded reactant A moieties and reactant B moieties;
subjecting the coated powder to an additive manufacturing process to produce a shaped green product comprising core particles adhered together, either: suspended in a matrix comprising the ALD/MLD coating, or sintered together in the shaped green product suspended in a powder bed, wherein the powder bed comprises the powder comprising core particles having the metal or ceramic core and the ALD/MLD coating having alternating, bonded reactant A moieties and reactant B moieties; and wherein the method is further characterized by the following features: wherein ALD or MLD is conducted for 2 to 25 cycles; and further comprising a step of atomic layer etching.
2. The method of claim 1 wherein the powder comprising the ALD/MLD coating has a flowability that is at least 10% higher than the flowability of the powder having a metal or ceramic core without the ALD/MLD coating.
3. The method of claim 1 further comprising: heating the shaped green product to cause the core particles to sinter together.
4. The method of claim 1 wherein the core particles are metal and comprise at least 0.5 mass % of one or more rare earth element.
5. The method of claim 1 wherein the coating has a higher melting temperature than the core.
6. A method of making a shaped object, comprising:
providing a powder comprising core particles comprising a metal or ceramic core;
reacting the powder with a first reactant (reactant A) following by reaction with a second reactant (reactant B) in a process of atomic (ALD) or molecular layer deposition (MLD) in a sequential manner to produce a powder comprising an ALD/MLD coating having alternating, bonded reactant A moieties and reactant B moieties;
subjecting the coated powder to an additive manufacturing process to produce a shaped green product comprising core particles adhered together, either: suspended in a matrix comprising the ALD/MLD coating, or sintered together in the shaped green product suspended in a powder bed, wherein the powder bed comprises the powder comprising core particles having the metal or ceramic core and the ALD/MLD coating having alternating, bonded reactant A moieties and reactant B moieties; and wherein the method is further characterized by the following features: wherein ALD or MLD is conducted for 2 to 25 cycles; wherein a laser is used to bind the powder to form a green intermediate product; and wherein the coating is a nano-laminate comprising alternating high and low indices of refraction.
7. The method of claim 6 wherein the ALD/MLD coating comprises an ABC configuration deposited by the ALD/MLD process.