IP Library › Granted Patent US 11,761,066
Granted Patent B2
US 11,761,066 · App. 17/359,455 · Granted Sep 19, 2023

Alloy and a method of preparing the same

Inventors: Yong Yang (Kowloon, HK); Shuo Shuang (Kowloon, HK); Dukhyun Chung (Kowloon, HK)
Assignee: CITY UNIVERSITY OF HONG KONG
C22C30/00C22B9/20C22C2200/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,761,066
App. No.
17/359,455
Granted
Sep 19, 2023
Kind
B2
Abstract

A novel medium entropy alloy having the chemical formula Mo x CrNiCo (atomic %) where (x ranges from ˜0.4 to ˜1.0).

Claims (7)

1. An alloy of Mo 0.6 CrNiCo characterized in having a dual phase consisting of a face centered cubic (fcc) phase and a sigma phase, wherein

the sigma phase is the minority phase volumetrically and the fcc phase is the majority phase volumetrically; and

the sigma phase forms a network around parcels of the fcc phase.

2. A method of preparing the alloy of claim 1 , comprising:

arc melting molybdenum, chromium, nickel, and cobalt into a molten alloy;

heating the molten alloy to a temperature between 750 degrees Celsius and 1350 degrees Celsius to precipitate the dual phase; and

quick quenching the molten alloy from above 750 degrees Celsius.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 1, 2023
From: YANG, YONG; SHUANG, SHUO; CHUNG, DUKHYUN
To: CITY UNIVERSITY OF HONG KONG
Reel/Frame 064448/0495 →
Continuity (2)
Provisional Application 63044462 · Jun 26, 2020
Related Publication 20220018000A1 · Jan 20, 2022