IP Library › Granted Patent US 11,942,637
Granted Patent B2
US 11,942,637 · App. 17/417,240 · Granted Mar 26, 2024

Positive electrode active material for nonaqueous electrolyte secondary battery and nonaqueous electrolyte secondary battery

Inventors: Hidekazu Hiratsuka (Hyogo, JP); Hiroki Watanabe (Hyogo, JP); Kazunori Donoue (Hyogo, JP)
Assignee: PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO., LTD.
H01M4/525H01M4/364H01M4/505H01M10/0525H01M2004/021H01M2004/028
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,942,637
App. No.
17/417,240
Granted
Mar 26, 2024
Kind
B2
Abstract

A positive electrode active material for a nonaqueous electrolyte secondary battery, the positive electrode active material comprising a Ni-containing lithium composite oxide a, b, wherein the Ni-containing lithium composite oxide a has an average primary particle size of 1 μm or more which is larger than the average primary particle size of the Ni-containing lithium composite oxide b, the Ni-containing lithium composite oxide a has an average secondary particle size of 2 to 6 μm, the Ni-containing lithium composite oxide b has an average primary particle size of 0.05 μm or more and an average secondary particle size of 10 to 20 μm, the Ni-containing lithium composite oxide a contains Mn and at least one of B and Al, the Ni-containing lithium composite oxide b contains Mn, and the ratio of the Ni-containing lithium composite oxide a to the Ni-containing lithium composite oxide b is 5:95 to 55:45.

Claims (13)

1. A positive electrode active material for a non-aqueous electrolyte secondary battery, including Ni-containing lithium composite oxides a and b, wherein

an average primary particle size of the Ni-containing lithium composite oxide a is 1 μm or more and larger than an average primary particle size of the Ni-containing lithium composite oxide b,

an average secondary particle size of the Ni-containing lithium composite oxide a is 2 μm to 6 μm,

the Ni-containing lithium composite oxide b has an average primary particle size of 0.05 μm or more and an average secondary particle size of 10 μm to 20 μm,

the Ni-containing lithium composite oxide a includes Mn, includes at least either one of B and Al, contains 55 mol % or more of Ni based on the total number of moles of the metal elements except for Li, and has a crystallite size of 100 nm to 200 nm,

the Ni-containing lithium composite oxide b includes Mn, is free of B and Al or has smaller contents of B and Al than those in the Ni-containing lithium composite oxide a, contains 55 mol % or more of Ni based on the total number of moles of the metal elements except for Li, and has a crystallite size of 100 nm to 200 nm, and

a mass ratio between the Ni-containing lithium composite oxide a and the Ni-containing lithium composite oxide b is 5:95 to 55:45.

2. The positive electrode active material for a non-aqueous electrolyte secondary battery according to claim 1 , wherein

a proportion by mass of each of B and Al included in the Ni-containing lithium composite oxide a is in a range of 200 ppm to 1000 ppm with respect to the Ni-containing lithium composite oxide a.

3. A non-aqueous electrolyte secondary battery, comprising:

a positive electrode including the positive electrode active material for a non-aqueous electrolyte secondary battery according to claim 1 ;

a negative electrode; and

a non-aqueous electrolyte.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 5, 2021
From: HIRATSUKA, HIDEKAZU; WATANABE, HIROKI; DONOUE, KAZUNORI
To: PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO., LTD.
Reel/Frame 057708/0655 →
Priority Claims (1)
JP 2018-247348 · Dec 28, 2018 · national
Continuity (1)
Related Publication 20220059836A1 · Feb 24, 2022
Cited By (1)
US 12,738,478