Recovery of materials from spent batteries using a green solvent

Inventors: Ilias Belharouak (Oak Ridge, TN); Yaocai Bai (Oak Ridge, TN); Rachid Essehli (Oak Ridge, TN)
Assignee: UT-BATTELLE, LLC
H01M10/54H01M4/622H01M10/0525
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,444,780
App. No.
17/551,395
Granted
Oct 14, 2025
Kind
B2
Abstract

A method for recycling lithium-ion battery materials is provided. The method includes isolating a composite electrode that includes an electrode material adhered to a current collector. The isolated composite electrode is combined with a citrate-based solvent to form a mixture. The electrode material is delaminated from the current collector in the mixture to give a free electrode material and a free current collector. Each of the free electrode material and the free current collector is recovered from the mixture. The free electrode material may be reused to prepare another composite electrode, as well as a lithium-ion battery comprising the same, which are also disclosed.

Claims (25)

1. A method of recycling lithium-ion battery materials, the method comprising:

isolating a composite electrode, the composite electrode comprising an electrode material adhered to a current collector;

combining the composite electrode with a citrate-based solvent to form a mixture, wherein the citrate-based solvent includes one or more of acetyl tributyl citrate (ATBC), acetyl triethyl citrate (ATEC), triethyl citrate (TEC), and tributyl citrate (TRC);

delaminating the electrode material from the current collector in the mixture to give a free electrode material and a free current collector; and

recovering each of the free electrode material and the free current collector from the mixture.

2. The method of claim 1 , wherein the electrode material is delaminated from the current collector in the citrate-based solvent at a temperature in the range of 20 to 300° C. under continuous stirring.

3. The method of claim 1 , wherein the electrode material and the current collector are fully delaminated within a time of 60 minutes after forming the mixture.

4. The method of claim 1 , further comprising the step of shredding the composite electrode into a collection of smaller composite electrode fragments before the step of combining the composite electrode with the citrate-based solvent.

5. The method of claim 1 , wherein the composite electrode is one or both of a spent electrode from a spent lithium-ion battery and electrode scrap from an electrode manufacturing process.

6. The method of claim 1 , wherein the composite electrode is further defined as a composite cathode, and the electrode material is further defined as a cathode active material.

7. The method of claim 6 , wherein in the composite cathode: (i) the cathode active material comprises a lithium-bearing metal oxide; (ii) the current collector comprises aluminum; or (iii) both (i) and (ii).

8. The method of claim 1 , wherein the composite electrode is further defined as a composite anode, wherein the electrode material is further defined as an anode active material.

9. The method of claim 8 , wherein in the composite anode: (i) the anode active material comprises an electroconductive carbon compound; (ii) the current collector comprises copper; or (iii) both (i) and (ii).

10. The method of claim 1 , wherein isolating the composite electrode comprises:

(i) separating the composite electrode from one or more other components of the lithium-ion battery; (ii) washing the composite electrode with a solvent to remove a residual electrolyte therefrom; or (iii) both (i) and (ii).

11. The method of claim 1 , wherein recovering each of the free electrode material and the free current collector from the mixture comprises: (i) filtering the mixture to extract at least one of the free electrode material and the free current collector; (ii) rinsing the at least one of the free electrode material and the free current collector with a solvent to remove a residual amount of the citrate-based solvent therefrom; or (iii) both (i) and (ii).

12. The method of claim 1 , wherein the free electrode material recovered from the mixture: (i) comprises substantially the same morphology as the electrode material; (ii) comprises substantially the same chemical composition as the electrode material; (iii) comprises substantially the same electrochemical performance as the electrode material; (iv) is directly reusable in the preparation of a new composite electrode; or (v) any combination of (i)-(iv).

13. The method of claim 1 , wherein the free current collector recovered from the mixture is substantially free from: (i) corrosion; (ii) residual electrode material; or (iii) both (i) and (ii).

14. A method of recycling lithium-ion battery materials, the method comprising:

isolating a composite electrode, the composite electrode comprising an electrode material adhered to a current collector;

combining the composite electrode with a citrate-based solvent to form a mixture, wherein a binder that adheres the electrode material to the current collector is dissolved in the citrate-based solvent, the binder being one of a polyvinylidene fluoride (PVDF) binder and a carboxymethyl cellulose (CMC) binder;

delaminating the electrode material from the current collector in the mixture to give a free electrode material and a free current collector; and

recovering each of the free electrode material and the free current collector from the mixture.

15. The method of claim 1 , further comprising preparing a new composite electrode using the free electrode material.

16. The method of claim 15 , further comprising preparing a new lithium-ion battery using the new composite electrode.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 17, 2022
From: BELHAROUAK, ILIAS; BAI, YAOCAI; ESSEHLI, RACHID
To: UT-BATTELLE, LLC
Reel/Frame 060828/0015 →
CONFIRMATORY LICENSE Recorded Apr 14, 2022
From: UT-BATTELLE, LLC
To: U. S. DEPARTMENT OF ENERGY
Reel/Frame 059594/0966 →
Continuity (2)
Provisional Application 63126695 · Dec 17, 2020
Related Publication 20220200073A1 · Jun 23, 2022
References Cited (7)
US 6150050A · Mathew · 2000 [cited by examiner]
US 6447669B1 · Lain · 2002 [cited by examiner]
US 9484606B1 · Sloop · 2016 [cited by examiner]
US 20180013181A1 · Ho · 2018 [cited by examiner]
US 20210083336A1 · Baek · 2021 [cited by examiner]
CN 108281730A · 2018 [cited by examiner]
Sawada et al., Effect of citrate-based non-toxic solvents on poly(vinylidene fluoride) membrane preparation via thermally induced phase separation, Nov. 1, 2015, Journal of Membrane Science, vol. 493, pp. 232-242 (Year:… [cited by examiner]