Cationic copolymers with pendant N-allylimidazolium groups

Inventors: Claire Hartmann-Thompson (Lake Elmo, MN); Mark J. Pellerite (Woodbury, MN); Marina M. Kaplun (Woodbury, MN); John C. Thomas (St. Paul, MN)
Assignee: 3M Innovative Properties Company
C08F212/08B01J41/14H01M50/414
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,103,994
App. No.
17/593,703
Granted
Oct 1, 2024
Kind
B2
Abstract

Cationic copolymers having pendant N-allylimidazolium-containing groups are provided. The cationic copolymers can be used, for example, to provide anion exchange membranes for use in electrochemical cells such as fuel cells, electrolyzers, batteries, and electrodialysis cells. The anion exchange membranes typically have good mechanical properties and ionic conductivity.

Claims (28)

1. A cationic copolymer comprising:

a) a first monomeric unit of Formula (I) having a pendant N-allylimidazolium-containing group in an ortho, para, or meta position of a benzene ring; and

b) second monomeric units of Formula (II-1), Formula (II-2) or a mixture thereof; and

c) an optional third monomeric unit of Formula (III);

wherein

R 1 is halo, hydroxy, or alkoxy and the pendant group —CH 2 R 1 is in an ortho, para, or meta position;

group R 2 is a cationic, nitrogen-containing group and group —CH 2 R 2 is in an ortho, para, or meta position;

any cationic group in the copolymer has a corresponding anionic group;

each asterisk (*) is a point of attachment to another group or monomeric unit in the copolymer;

Formula (III) is different from Formula (I); and

the cationic copolymer is not crosslinked and comprises

20 to 50 mole percent monomeric units having a cationic, nitrogen-containing group comprising the first monomeric units of Formula (I) or a mixture of the first monomeric units of Formula (I) and the third monomeric units of Formula (III) based on total moles of monomeric units in the cationic copolymer;

50 to 80 mole percent second monomeric units of Formula (II-1) based on total moles of monomeric units in the cationic copolymer; and

0 to 20 mole percent second monomeric units of Formula (II-2) based on total moles of monomeric units in the cationic copolymer.

2. The cationic copolymer of claim 1 , wherein R 2 of the third monomeric units is a cationic, nitrogen-containing heterocyclic group optionally substituted with one or more alkyl groups.

3. The cationic copolymer of claim 2 , wherein the cationic, nitrogen-containing heterocyclic group is imidazolium substituted with one or more alkyl groups, pyridinium, or pyridinium substituted with one or more alkyl groups.

4. The cationic copolymer of claim 1 , wherein the third monomeric unit of Formula (III) is of Formula (IV)

wherein

R 3 is hydrogen or alkyl; and

R 4 is alkyl.

5. The cationic copolymer of claim 1 , wherein the third monomer of Formula (III) is of Formula (V)

wherein R 5 is hydrogen or alkyl.

6. The cationic copolymer of claim 1 , wherein R 2 is of formula —(NR 6 R 7 R 8 ) + wherein R 6 , R 7 , and R 8 are each independently an alkyl.

7. The cationic copolymer of claim 1 , wherein R 2 is a guanidinium group that is substituted with multiple alkyl groups.

8. The cationic copolymer of claim 1 , wherein the monomeric units having a cationic, nitrogen-containing groups are 5 to 100 mole percent first monomeric units of Formula (I) and 0 to 95 mole percent third monomeric units of Formula (III).

9. The cationic copolymer of claim 8 , wherein the monomeric units having a cationic, nitrogen-containing group are 10 to 100 mole percent first monomeric units of Formula (I) and 0 to 90 mole percent third monomeric units of Formula (III).

10. An anion exchange membrane formed by casting the cationic copolymer of claim 1 from a solvent.

11. An electrochemical cell comprising an anode, a cathode, and an anion exchange membrane positioned between the anode and the cathode, wherein the anion exchange membrane is formed by casting the cationic copolymer of claim 1 from a solvent.

Assignments (2)
CONFIRMATORY LICENSE Recorded Jul 15, 2024
From: 3M COMPANY
To: US DEPARTMENT OF ENERGY
Reel/Frame 068377/0117 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 23, 2021
From: HARTMANN-THOMPSON, CLAIRE; PELLERITE, MARK J.; KAPLUN, MARINA M.; THOMAS, JOHN C.
To: 3M INNOVATIVE PROPERTIES COMPANY
Reel/Frame 057578/0641 →
Continuity (2)
Provisional Application 62859397 · Jun 10, 2019
Related Publication 20220169764A1 · Jun 2, 2022