Composite nonwoven mat and method of making the same
A composite nonwoven mat and a method of making a composite nonwoven mat are provided. The composite nonwoven mat includes a nonwoven base layer having a first surface and a second surface, and a polymer layer formed on and adhered to the first surface of the nonwoven base layer. The polymer layer extends partially into the nonwoven base layer. The composite nonwoven mat has an average Gurley porosity of at least 2,000 seconds.
1 . A composite nonwoven mat comprising:
a nonwoven base layer comprising:
glass fibers having an average diameter of from about 13 microns to about 16 microns; and
a binder composition coating at least a portion of the glass fibers, the binder composition comprising:
a binder resin material,
a coupling agent, and
optionally one or more additives;
wherein the nonwoven base layer has a first surface and a second, opposing surface; and
a polymer layer adhered to the first surface, wherein the polymer layer comprises at least 97 wt. % of a polymer material;
wherein the polymer layer seals the first surface such that it prevents bleed-through of liquid/flowable material and is impervious to air;
wherein the polymer layer extends partially into the nonwoven base layer;
wherein the nonwoven base layer has a basis weight of 30 g/m 2 to 200 g/m 2 and the polymer layer has a basis weight of 10 g/m 2 to 100 g/m 2 ;
wherein the second surface is porous and permits penetration by liquid/flowable material; and
wherein the composite nonwoven mat has an average Gurley porosity of 1,000 seconds to 30,000 seconds.
2 . The composite nonwoven mat of claim 1 , wherein the polymer layer comprises one or more of a polyolefin, a polyester, a polyamide, a polyimide, a polyacrylate, and a polyurethane.
3 . The composite nonwoven mat of claim 1 , wherein the polymer layer comprises one or more of a polyethylene, a polypropylene, and a polymethacrylate.
4 . The composite nonwoven mat of claim 1 , wherein the polymer layer comprises one or more additives in an amount of less than 3% by weight of the polymer layer, and wherein the additives comprise one or more of a fire retardant, a dye, a pigment, a UV stabilizer, an anti-static agent, and a filler.
5 . The composite nonwoven mat of claim 1 , wherein the second surface of the nonwoven base layer is free of the polymer layer.
6 . A flooring material comprising a composite nonwoven mat according to claim 1 .
7 . A polyisocyanurate foam board comprising at least one facer, wherein the at least one facer comprises a composite nonwoven mat according to claim 1 .
8 . A composite nonwoven mat comprising:
a nonwoven base layer comprising:
glass fibers;
a plurality of additional fibers selected from polyester fibers, polyethylene fibers, polypropylene fibers, and polyethylene terephthalate fibers; and
a binder composition coating at least a portion of the glass fibers and the plurality of additional fibers, the binder composition comprising:
a binder resin material,
a coupling agent, and
optionally one or more additives,
wherein the nonwoven base layer has a first surface and a second, opposing surface; and
a polymer layer adhered to the first surface, wherein the polymer layer comprises at least 97 wt. % of a polymer material;
wherein the polymer layer seals the first surface such that it prevents bleed-through of liquid/flowable material and is impervious to air;
wherein the polymer layer extends partially into the nonwoven base layer;
wherein the second surface is porous and permits penetration by liquid/flowable material;
wherein the only binder composition in the nonwoven base layer is the binder composition that is coating at least a portion of the glass fibers and the plurality of additional fibers; and
wherein the composite nonwoven mat has an average Gurley porosity of 1,000 seconds to 30,000 seconds.