Mechanoenzymatic degradation of polymers
A method of depolymerizing a polymer by combining together the polymer with an enzyme (a hydrolytic enzyme capable of catalyzing cleavage of said (CO)—O bond of an ester or carbonate linkage of the polymer) and an aqueous liquid to provide a reaction mixture. The polymer comprises a (CO)—O bond of an ester or carbonate linkage. The reaction mixture defines a ratio eta (η) of liquid volume, in μL, to total solids, in mg, that is less than 2 μL/mg. Then, allowing an enzyme-catalyzed reaction of the enzyme with the polymer to take place thereby forming a reaction product.
1. A method of depolymerizing a polymer, said method comprising:
A) combining together the polymer with an enzyme and an aqueous liquid to provide a reaction mixture;
wherein said polymer comprises a (CO)—O bond of an ester or carbonate linkage; wherein said reaction mixture is defining a ratio eta (η) of liquid volume, in μL, to total solids, in mg, that is less than 2 μL/mg;
said enzyme is a hydrolytic enzyme capable of catalyzing cleavage of said (CO)—O bond of an ester or carbonate linkage of said polymer; and
B) allowing an enzyme-catalyzed reaction of said enzyme with said polymer to take place thereby forming a reaction product.
2. The method according to claim 1 , wherein said polymer is in a form of powder, granule, film, cut or textile.
3. The method according to claim 1 , wherein the polymer comprises at least a polyester, and/or a polycarbonate segment or chain.
4. The method according to claim 1 , wherein the polymer is a polycarbonate.
5. The method according to claim 1 , wherein the polymer is selected from the group consisting of polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polytrimethylene terephthalate (PTT), polyethylene naphthalate (PEN), and any combination thereof.
6. The method according to claim 1 , wherein the polymer is selected from the group consisting of polylactic acid or polylactide (PLA), polyglycolide (PGA), polycaprolactone (PCL), polyhydroxyalkanoate (PHA), polyhydroxybutyrate (PHB), polyethylene adipate (PEA), polybutylene succinate (PBS), and any combination thereof.
7. The method according to claim 1 , wherein the polymer comprises polyethylene terephthalate (PET).
8. The method according to claim 1 , wherein the enzyme is a cutinase, esterase, lipase, PET hydrolase, PETase or any combination thereof.
9. The method according to claim 1 , wherein the step of combining to provide a reaction mixture comprises at least one of milling, extruding, resonance acoustic mixing, vortexing, grinding, or other methods of mixing solids, of said polymer with said enzyme and said aqueous liquid, either intermittently, or continuously.
10. The method according to claim 1 , wherein the step of allowing the enzyme-catalyzed reaction to take place is as aging at a temperature of between 20° C. to 70° C.
11. The method according to claim 10 , wherein said aging is for a duration of from 12 hours, and up to 30 days.
12. The method according to claim 1 , wherein the method comprises conducting at least one cycle of said steps of combining to provide a reaction mixture and the step of allowing the enzyme-catalyzed reaction to take place.
13. The method according to claim 1 , further comprising milling said polymer before said step of combining together the polymer with said enzyme and said aqueous liquid.
14. The method according to claim 1 , wherein said reaction product comprises at least a corresponding building block of said polymer.
15. The method according to claim 1 , wherein when said polymer comprises polyethylene terephthalate (PET), said monomer unit in the form of acid and/or ester comprises terephthalic acid (TPA).
16. The method according to claim 1 , further comprises after step B), a step of recovering said product.
17. The method according to claim 1 , wherein after step B), the method further comprises recovering the enzyme.
18. The method according to claim 7 , wherein the PET has a crystallinity of at least 5%, at least 20%, or at least 30%.
19. The method according to claim 11 , wherein said aging is for a duration of from 24 hours, and up to 30 days.
20. The method according to claim 12 , wherein at least one of said steps of combining to provide a reaction mixture is by milling and the step of allowing the enzyme-catalyzed reaction to take place is by aging.