ELECTROLYTE AND ELECTRODE PASTE FOR LITHIUM-ION BATTERY, LITHIUM-ION BATTERY, AND METHOD OF MANUFACTURING LITHIUM-ION BATTERY WITH ENHANCED PERFORMANCE

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
17/890,263
Abstract

This disclosure relates to improved electrolytes and electrode pastes that include ground state metal nanoparticles formed by laser ablation, improved rechargeable lithium-ion batteries made using the improved electrolytes and/or electrode pastes that include ground state metal nanoparticles formed by laser ablation, and methods for manufacturing rechargeable batteries of improved performance. The metal nanoparticles may comprise or consist of gold. The metal nanoparticles may by spherical-shaped and/or coral-shaped.

Claims (37)

1 . An electrolyte for use in lithium-ion batteries comprising:

a carrier that is a liquid, gel, or solid;

one or more complexes of lithium ions selected from lithium hexafluorophosphate (LiPF 6 ), lithium hexafluoroarsenate monohydrate (LiAsF 6 ), lithium perchlorate (LiClO 4 ), lithium tetrafluoroborate (LiBF 4 ), and lithium triflate (LiCF 3 SO 3 ); and

ground state metal nanoparticles formed by laser ablation.

2 . The electrolyte of claim 1 , wherein the carrier includes one or more organic carbonates selected from ethylene carbonate and diethyl carbonate.

3 . The electrolyte of claim 1 , wherein carrier comprises a polymer.

4 . The electrolyte of claim 1 , wherein the ground state metal nanoparticles comprise spherical-shaped gold nanoparticles.

5 . The electrolyte of claim 4 , wherein the spherical-shaped nanoparticles a diameter of less than about 20 nm, or less than about 15 nm, less than about 10 nm, or less than about 7 nm,

6 . The electrolyte of claim 1 , wherein the ground state metal nanoparticles are included in a concentration of at least 100 ppb and up to 100 ppm, or up to 50 ppm, or up to 25 ppm, or up to 10 ppm, or up to 5 ppm by weight of the electrolyte.

7 . An electrode paste for use in lithium-ion batteries comprising:

a carrier comprising a binder;

one or more electrode active materials selected from negative electrode active materials and positive electrode active materials; and

ground state metal nanoparticles formed by laser ablation.

8 . The electrode paste of claim 7 , wherein the one or more electrode active materials comprise one or more positive electrode active materials selected from LiCoO 2 , LiMnO 2 , LiMn 2 O 4 , Li 2 MnO 3 , LiNiO 2 , LiFePO 4 , LiNiMnCoO 2 , Li 4 Ti 5 O 12 and mixtures thereof.

9 . The electrode paste of claim 7 , wherein the one or more electrode active materials comprise one or more negative electrode active materials selected from mesophase carbon micro beads (MCMB), natural graphite powder, Li 4 Ti 5 O 12 and mixtures thereof.

10 . The electrode paste of claim 7 , wherein the ground state metal nanoparticles comprise spherical-shaped gold nanoparticles.

11 . A lithium-ion battery having enhanced performance, comprising:

at least one negative electrode comprising ground state lithium (Li);

at least one positive electrode comprising a metal oxide that includes and/or is capable of forming a lithium-metal oxide; and

an electrolyte and/or electrode paste in contact with and/or positioned between the at least one negative electrode and the at least one positive electrode; and

a container in which the at least one negative electrode, the at least one positive electrode, and the electrolyte and/or electrode paste are positioned,

wherein:

the electrolyte comprises (i) a carrier that is a liquid, gel, or solid; (ii) one or more complexes of lithium ions selected from lithium hexafluorophosphate (LiPF 6 ), lithium hexafluoroarsenate monohydrate (LiAsF 6 ), lithium perchlorate (LiClO 4 ), lithium tetrafluoroborate (LiBF 4 ), and lithium triflate (LiCF 3 SO 3 ); and (iii) ground state metal nanoparticles formed by laser ablation; and/or

the electrode paste comprising (i) a binder; (ii) one or more electrode active materials selected from negative electrode active materials and positive electrode active materials; (iii) and ground state metal nanoparticles formed by laser ablation.

12 . The lithium-ion battery of claim 11 , wherein the at least one negative electrode comprises lithium metal intercalated between layers of graphite.

13 . The lithium-ion battery of claim 11 , wherein the at least one positive electrode comprises at least one lithium-metal oxide selected from the group consisting of LiCoO 2 , LiMnO 2 , LiMn 2 O 4 , Li 2 MnO 3 , LiNiO 2 , LiFePO 4 , LiNiMnCoO 2 , Li 4 Ti 5 O 12 and combinations thereof.

14 . The lithium-ion battery of claim 13 , wherein the at least one positive electrode comprises the lithium-metal oxide in intercalated between layers of metal oxide.

15 . The lithium-ion battery of claim 11 , wherein the ground state metal nanoparticles comprise spherical-shaped gold nanoparticles.

16 . The lithium-ion battery of claim 11 , wherein the electrolyte and/or electrode paste includes ground state metal nanoparticles in a concentration of at least 100 ppb and up to 100 ppm, or up to 50 ppm, or up to 25 ppm, or up to 10 ppm, or up to 5 ppm.

17 . A method of manufacturing a lithium-ion battery of enhanced performance according to claim 11 , comprising:

providing the electrolyte and/or electrode paste;

placing the electrolyte and/or electrode paste in contact with the at least one negative electrode comprising ground state lithium (Li);

placing the electrolyte and/or electrode paste in contact with the at least one positive electrode comprising a metal oxide that includes and/or is capable of forming a lithium-metal oxide; and

positioning the negative and positive electrodes and the electrolyte and/or electrode paste within the electrically insulating container.

18 . The method of claim 17 , wherein the at least one negative electrode comprises lithium metal intercalated between layers of graphite.

19 . The method of claim 17 , wherein the at least one positive electrode comprises at least one lithium-metal oxide selected from the group consisting of LiCoO 2 , LiMnO 2 , LiMn 2 O 4 , Li 2 MnO 3 , LiNiO 2 , LiFePO 4 , LiNiMnCoO 2 , Li 4 Ti 5 O 12 and combinations thereof.

20 . The method of claim 17 , wherein the inclusion of the metal nanoparticles in the electrolyte and/or electrode paste increases at least one of battery lifespan, energy density, charge density per unit size or weight, safety, rate of discharge and production of current, rate of recharge, stability, longevity, and safety as compared to a same battery that omits the metal nanoparticles.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 17, 2022
From: NIEDERMEYER, WILLIAM H.
To: EVOQ NANO, INC.
Reel/Frame 060838/0365 →