Treated geothermal brine compositions with reduced concentration of silica, iron and lithium
This invention relates to treated geothermal brine compositions containing reduced concentrations of lithium, iron and silica compared to the untreated brines. Exemplary compositions contain concentration of lithium ranges from 0 to 200 mg/kg, concentration of silica ranges from 0 to 30 mg/kg, concentration of iron ranges from 0 to 300 mg/kg. Exemplary compositions also contain reduced concentrations of elements like arsenic, barium, and lead.
1. A method for producing lithium hydroxide or lithium carbonate from a brine solution, the method comprising the steps of,
providing a brine solution comprising lithium and silica;
supplying the brine solution to a silica management step to remove silica from the brine solution to produce a silica-lean lithium containing solution;
supplying the silica-lean lithium containing solution to a lithium capture step, the lithium capture step being operable to capture lithium from the silica-lean lithium containing solution, wherein the lithium capture step selectively isolates lithium from the silica-lean lithium containing solution;
wherein the lithium capture step includes the step of contacting the silica-lean lithium containing solution with an intercalate operable to capture the lithium from the silica-lean lithium containing solution;
recovering the lithium from the lithium capture step using wash water to produce a lithium-rich stream comprising at least one of calcium, magnesium, manganese or zinc, and
contacting the lithium-rich stream with a base and a carbonate such that a portion of the at least one of calcium, magnesium, manganese or zinc present in the lithium-rich stream is removed as a solid precipitate to produce a purified lithium-rich stream comprising lithium hydroxide or lithium carbonate.
2. The method of claim 1 , wherein the brine solution is a geothermal brine.
3. The method of claim 1 , wherein the brine solution is a Salton Sea geothermal brine.
4. The method of claim 1 , wherein the silica-lean lithium containing solution is substantially free of silica.
5. The method of claim 1 , wherein the silica-lean lithium containing solution comprises a lithium chloride containing solution.
6. The method of claim 1 , further comprising the step of:
increasing the concentration of lithium in the lithium-rich stream by removing at least a portion of the water in the lithium-rich stream.
7. The method of claim 1 , wherein the intercalate is an intercalated lithium absorbent.
8. The method of claim 1 , wherein the intercalate is a lithium aluminate intercalate.
9. The method of claim 1 , further comprising:
separating precipitate from the lithium-rich stream to produce a solid waste precipitate and a purified lithium-rich stream, the purified lithium-rich stream having a lower concentration of the at least one of calcium, magnesium, manganese or zinc, wherein the purified lithium-rich stream comprises at least one of ions selected from the group consisting of borate, calcium, magnesium, manganese and zinc; and
contacting the purified lithium-rich stream with an ion selective media to reduce the concentration of at least one of the ions selected from the group consisting of borate, calcium, magnesium, manganese and zinc.