IP Library Granted Patent US 11,583,892
Granted Patent B1
US 11,583,892 · App. 17/949,440 · Granted Feb 21, 2023

Coated oilfield operational components and methods for protecting and extending the service life of oilfield operational components

Inventors: Greg Andrews (Wilmington, DE); George D. Andrews (Wilmington, DE); Jeff Capell (Wilmington, DE)
Assignee: S+S INDUSTRIES TECHNOLOGY LLC
B05D7/586B05D1/02B05D1/18B05D1/38B05D3/12B05D5/00B05D7/14B05D7/16B05D7/22B05D7/222B05D7/225B05D7/26B05D7/544B05D7/546B05D7/584C08K5/5425C09D5/002C09D5/082C09D5/084C09D7/20C09D7/61C09D7/62C09D7/63C09D159/00C09D163/04C09D183/04C09D183/06C23F11/18E21B33/03E21B34/04E21B34/06E21B41/00E21B43/2607B05D2202/00B05D2202/10B05D2254/00B05D2350/60B05D2401/10B05D2504/00C08G59/022C08G59/063C08K3/11C08K3/36C08K5/541C08K5/544C08K5/5415C08K5/5435C09D163/00E21B17/02E21B43/26
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,583,892
App. No.
17/949,440
Granted
Feb 21, 2023
Kind
B1
Abstract

Coating compositions for coating an oilfield operational component, and related methods, may include in some aspects a coating composition having a trifunctional silane, a silanol, and a filler. The coating composition may be applied to a surface of the oilfield operational component that is configured to be exposed to a fluid. The coating composition may be applied to at least partially cover or coat the surface. The coating composition may be configured to chemically bond with a cured primer composition that includes an epoxy.

Claims (40)

1. A method for protecting a component, the method comprising:

applying a primer composition to the component;

at least partially curing the primer composition to form a primer layer, such that the primer layer at least partially mechanically bonds to the component;

applying a coating composition to the primer layer, the coating composition comprising trifunctional silane, silanol fluid, fillers, and titanium dioxide; and

at least partially curing the coating composition, thereby to form a coating layer and so that the coating layer at least partially chemically bonds to the primer layer to enhance wear resistance of the component, the coating composition comprising T-resin units each of which forms one or more bonds with one or more of other T-resin units, silanol fluid, fillers, or the titanium dioxide, such that the component exhibits a comparison factor indicative of an increased resistance to wear greater than about 2, the comparison factor being indicative of a first amount of time during which a portion of one or more of the coating layer or the primer layer wears to a first depth divided by a second amount of time during which a portion of the component without the one or more of the coating layer or the primer layer wears to a second depth equal to the first depth.

2. The method of claim 1 , wherein the T-resin units form two or more bonds with one or more of other T-resin units, silanol fluid, titanium dioxide, or fillers.

3. The method of claim 1 , wherein applying the primer composition to the component comprises applying the primer composition to at least a portion of the component, and wherein the comparison factor ranges from about 5 to about 30.

4. The method of claim 1 , wherein applying the primer composition to the component comprises applying one or more of an aliphatic amine, epichlorohydrin, a bisphenol, silane adhesion promoter, trimethoxysilane, triethoxysilane, or 3-glycidoxypropyltrimethoxysilane to the component.

5. The method of claim 1 , wherein applying the coating composition comprises spraying the coating composition onto the component via a spray head configured to atomize the coating composition as it is applied to the component.

6. The method of claim 5 , wherein spraying the coating composition onto the component via the spray head comprises:

pumping the coating composition via an airless pump at an output ratio ranging from about 40:1 to about 80:1 to a spray head configured to rotate and atomize the coating composition; and

supplying air to the spray head to cause the spray head to rotate as the coating composition is atomized and sprayed from the spray head.

7. The method of claim 1 , further comprising applying the coating composition to the coating layer to form a second coating layer and at least partially drying the second coating layer.

8. The method of claim 1 , wherein applying the primer composition to the component comprises applying the primer composition to at least a portion of an oilfield component, and the comparison factor ranges from about 3 to about 12.

9. The method of claim 1 , wherein applying the primer composition to the component comprises applying the primer composition to at least a portion of a component, wherein the component comprises one or more of a goat head, a fluid end, a frac iron, a pipeline, or a pipeline component, and wherein the comparison factor ranges from about 2 to about 20.

10. The method of claim 2 , further comprising:

applying the coating composition to the coating layer to form a second coating layer and at least partially drying the second coating layer; and

applying the coating composition to the second coating layer to form a third coating layer and at least partially drying the third coating layer.

11. A method for protecting a component, the method comprising:

spraying a primer composition onto the component via a spray head configured to atomize the primer composition as it is applied to the component;

at least partially curing the primer composition to form a primer layer, such that the primer layer at least partially mechanically bonds to the component;

spraying a coating composition onto the primer layer, the coating composition comprising trifunctional silane, silanol fluid, fillers, and titanium dioxide; and

at least partially curing the coating composition to form a coating layer, so that the coating layer at least partially chemically bonds to the primer layer to enhance wear resistance of the component, the coating composition comprising T-resin units each of which forms one or more bonds with one or more of other T-resin units, silanol fluid, fillers, or the titanium dioxide, and so that the component exhibits a comparison factor indicative of an increased resistance to wear, the comparison factor being indicative of a first amount of time during which a portion of one or more of the coating layer or the primer layer wears to a first depth divided by a second amount of time during which a portion of the component without the one or more of the coating layer or the primer layer wears to a second depth equal to the first depth.

12. The method of claim 11 , wherein spraying the coating composition onto the component via the spray head comprises:

pumping the coating composition via an airless pump at an output ratio ranging from about 40:1 to about 80:1 to a spray head configured to rotate and atomize the coating composition; and

supplying air to the spray head to cause the spray head to rotate as the coating composition is atomized and sprayed from the spray head.

13. The method of claim 11 , further comprising spraying the coating composition onto the coating layer to form a second coating layer and at least partially drying the second coating layer.

14. The method of claim 11 , wherein spraying the primer composition onto the component comprises spraying one or more of an aliphatic amine, epichlorohydrin, a bisphenol, silane adhesion promoter, trimethoxysilane, triethoxysilane, or 3-glycidoxypropyltrimethoxysilane onto the component.

15. The method of claim 14 , wherein the comparison factor ranges from about 2 to about 20.

16. The method of claim 11 , wherein the T-resin units form two or more bonds with one or more of other T-resin units, silanol fluid, titanium dioxide, or fillers.

17. A method for protecting a component prior to being exposed to fluid flow, the method comprising:

applying a primer composition to the component;

at least partially curing the primer composition to form a primer layer, such that the primer layer at least partially mechanically bonds to the component;

applying a coating composition to the primer layer, the coating composition comprising trifunctional silane, silanol fluid, fillers, and one or more pigments; and

at least partially curing the coating composition to form a coating layer, so that the coating layer at least partially chemically bonds to the primer layer to enhance wear resistance of the component, the coating composition comprising T-resin units each forming one or more bonds with one or more of other T-resin units, silanol fluid, fillers, or one or more pigments, and so that the component exhibits a comparison factor indicative of an increased resistance to wear greater than about 2, the comparison factor being indicative of a first amount of time during which a portion of one or more of the coating layer or the primer layer wears to a first depth divided by a second amount of time during which a portion of the component without the one or more of the coating layer or the primer layer wears to a second depth equal to the first depth.

18. A method for protecting a component prior to being exposed to fluid flow, the method comprising:

spraying a primer composition onto the component via a spray head configured to atomize the primer composition as it is applied to the component;

at least partially curing the primer composition to form a primer layer, such that the primer layer at least partially mechanically bonds to the component;

spraying a coating composition onto the primer layer, the coating composition comprising trifunctional silane, silanol fluid, and fillers; and

at least partially curing the coating composition to form a coating layer, so that the coating layer at least partially chemically bonds to the primer layer to enhance wear resistance of the component, the coating composition comprising T-resin units each forming one or more bonds with one or more of other T-resin units, silanol fluid, or the fillers, and so that the component exhibits a comparison factor indicative of an increased resistance to wear, the comparison factor being indicative of a first amount of time during which a portion of one or more of the coating layer or the primer layer wears to a first depth divided by a second amount of time during which a portion of the component without the one or more of the coating layer or the primer layer wears to a second depth equal to the first depth.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 1, 2022
From: ANDREWS, GREG; ANDREWS, GEORGE D.; CAPELL, JEFF
To: FORMULA NO. 37, LLC
Reel/Frame 061609/0449 →
CHANGE OF NAME Recorded Nov 1, 2022
From: S+S INDUSTRIES LLC
To: S+S INDUSTRIES TECHNOLOGY LLC
Reel/Frame 061828/0667 →
CHANGE OF NAME Recorded Nov 1, 2022
From: FORMULA NO. 37, LLC
To: S+S INDUSTRIES LLC
Reel/Frame 061828/0692 →
Continuity (13)
Continuation 17859048 · Jul 7, 2022
Continuation 17225543 · Apr 8, 2021
Provisional Application 63198044 · Sep 25, 2020
Provisional Application 63065577 · Aug 14, 2020
Provisional Application 63065545 · Aug 14, 2020
Provisional Application 63065565 · Aug 14, 2020
Provisional Application 63065591 · Aug 14, 2020
Provisional Application 63065542 · Aug 14, 2020
Provisional Application 63008046 · Apr 10, 2020
Provisional Application 63008038 · Apr 10, 2020
Provisional Application 63008035 · Apr 10, 2020
Provisional Application 63008049 · Apr 10, 2020
Provisional Application 63008042 · Apr 10, 2020