Coal Combustion Residuals, Leachate and Wet Ash Wastes Solidification Devices, Kits, and Assemblies
Environmental waste solidification devices, system, kits and methods are shown and described. Absorbent compositions for solidification of environmental wastes are shown and described.
1 .- 20 . (canceled)
21 . A composition for environmental waste solidification, comprising:
a population of superabsorbent polymer particles (SAP); and
wood flour,
wherein the SAP and the wood flour are together configured to absorb moisture from coal combustion residuals and form a solidified mixture.
22 . The composition of claim 21 , wherein the composition includes 5-10% wood flour.
23 . The composition of claim 21 , wherein the composition has a higher composition percentage of the wood flour than of the SAP.
24 . The composition of claim 21 , wherein the composition includes 70-80% SAP.
25 . The composition of claim 21 , further comprising bentonite.
26 . The composition of claim 25 , wherein the composition includes 5-10% bentonite.
27 . The composition of claim 21 , wherein the SAP is contained in a pellet form.
28 . The composition of claim 27 , wherein the pellet form includes 2-8% SAP.
29 . The composition of claim 21 wherein the SAP is cross-linked internally and on its surface.
30 . The composition of claim 21 wherein the SAP is contained inside a water-soluble packet.
31 . A method for solidification of environmental waste, comprising:
mixing a population of superabsorbent polymer particles (SAP) with wood flour, to form an absorbent composition comprising the SAP and the wood flour; and
mixing the absorbent composition with coal combustion residuals, wherein the SAP and the wood flour are together configured to absorb moisture from the coal combustion residuals and form a solidified mixture.
32 . The method of claim 31 , wherein the absorbent composition includes 5-10% wood flour.
33 . The method of claim 31 , wherein the absorbent composition has a higher composition percentage of the wood flour than of the SAP.
34 . The method of claim 31 , wherein the solidified mixture passes an EPA Test Method 9095 paint filter test.
35 . The method of claim 31 , comprising forming the absorbent composition into a pellet form.
36 . The method of claim 35 , wherein the pellet form includes 2-8% SAP.
37 . The method of claim 31 , comprising mixing bentonite with the SAP and the wood flour, to include the bentonite in the absorbent composition.
38 . The method of claim 37 , wherein the absorbent composition includes 5-10% bentonite.
39 . The method of claim 31 , wherein a mixture of the absorbent composition and the coal combustion residuals includes between 0.5% and 2% of the SAP by dry weight.
40 . The method of claim 31 , wherein the absorbent composition includes 70-80% SAP.