Additive Manufacturing Using Multiple Metallic Materials
Powder-based additive manufacturing processes for producing integral parts with multiple metallic materials are disclosed. The integral parts are printed as single pieces by joining different metallic materials together during printing. A combination of different powder-based additive manufacturing processes or the same process can be used to produce the integral part.
1 . A multi-material part for a combustion device, comprising:
an injector plate penetrated by at least one propellant channel, wherein the injector plate comprises a copper based alloy;
a propellant manifold configured to provide a propellant to the at least one propellant channel, wherein the propellant manifold comprises a nickel based alloy; and
a diffusion region between a portion of the injector plate and a portion of the propellant manifold, wherein the diffusion region comprises a gradient of compositions between the copper based alloy and the nickel based alloy.
2 . The multi-material part of claim 1 , wherein the copper based alloy is selected from the group consisting of: a Cu—Ni-based alloy, a Cu—Cr—Nb alloy, a Cu—Co—Nb-based alloy, a GRCop alloy, GRCop-42, and GRCop-84, and further wherein the nickel based alloy is selected from the group consisting of: a Ni-based superalloy, an Inconel® alloy, a Haynes® alloy, a Ni—Cr based alloy, Inconel-625®, Inconel-718®, and Haynes-230®.
3 . The multi-material part of claim 1 , wherein the diffusion region further comprises a gradient of a mechanical property.
4 . The multi-material part of claim 1 , wherein the diffusion region further comprises a gradient of microstructure.
5 . The multi-material part of claim 1 , wherein the injector plate is configured to be at least a portion of a main injector for a combustion chamber, and wherein the propellant manifold is configured to be at least a portion of an oxidizer dome.
6 . A method for additively manufacturing a multi-material part, comprising:
depositing, using a first print system, a first metallic material comprising a copper based alloy on a build plate to form an injector plate penetrated by at least one propellant channel; and
depositing, using a second print system, a second metallic material comprising a nickel based alloy on the injector plate to form a propellant manifold configured to provide a propellant to the at least one propellant channel, such that the part is printed as an integral piece;
wherein a diffusion region is formed between a portion of the injector plate and a portion of the propellant manifold, and wherein the diffusion region comprises a gradient of compositions between the copper based alloy and the nickel based alloy.
7 . The method of claim 6 , further comprising removing the build plate and the injector plate from the first print system and aligning the build plate with the second print system.
8 . The method of claim 6 , wherein the first print system is selected from the group consisting of: powder bed fusion, laser powder bed fusion, laser powder bed, direct metal laser melting, direct metal laser sintering, selective laser sintering, selective heat sintering, laser metal fusion, laser metal deposition, selective laser melting, electron beam melting, direct metal deposition, binder jetting, multi jet fusion, and any combination thereof.
9 . The method of claim 6 , wherein the second print system is selected from the group consisting of: powder bed fusion, laser powder bed fusion, laser powder bed, direct metal laser melting, direct metal laser sintering, selective laser sintering, selective heat sintering, laser metal fusion, laser metal deposition, selective laser melting, electron beam melting, direct metal deposition, binder jetting, multi jet fusion, and any combination thereof.
10 . The method of claim 6 , wherein the copper based alloy is selected from the group consisting of: a Cu—Ni-based alloy, a Cu—Cr—Nb alloy, a Cu—Co—Nb-based alloy, a GRCop alloy, GRCop-42, and GRCop-84; and further wherein the nickel based alloy is selected from the group consisting of: a Ni-based superalloy, an Inconel® alloy, a Haynes® alloy, a Ni—Cr based alloy, Inconel-625®, Inconel-718®, and Haynes-230®.
11 . The method of claim 6 , wherein each of the first and the second metallic materials comprise powders with an average diameter from 10 microns to 100 microns.
12 . The method of claim 7 , wherein the aligning uses a plurality of alignment pins and an open loop feedback system.
13 . The method of claim 6 , further comprising post processing the injector plate using a technique selected from the group consisting of blasting, brushing, rinsing, washing, polishing, machining, dying, heating, annealing, solution annealing, normalizing, stress relieving, aging, tempering, selective heat treating, cold treating, cryogenic treating, carburizing, decarburization, case hardening, precipitation strengthening, hot isostatic pressing, quenching, cooling, and any combinations thereof.
14 . The method of claim 6 , further comprising tuning at least one print parameter of the first print system to achieve a surface roughness of the injector plate.
15 . The method of claim 14 , wherein the at least one print parameter is selected from the group consisting of: laser power, laser scan speed, laser beam waist, hatch spacing, material layer thickness, and exposure quantity.
16 . The method of claim 6 , wherein the injector plate is configured to be a portion of a main injector for a combustion chamber, and wherein the propellant manifold is configured to be a portion of an oxidizer dome.
17 . The method of claim 6 , wherein the multi-material part is configured to inject a fuel into a combustion chamber of a combustion device.
18 . The method of claim 6 , further comprising receiving a 3D model of the multi-material part.
19 . The method of claim 6 , further comprising depositing the first and second metallic materials in an inert environment.
20 . A method for additively manufacturing a multi-material part, comprising:
depositing, using a first print system, a first metallic material comprising a nickel based alloy on a build plate to form a propellant manifold configured to provide a propellant to at least one propellant channel; and
depositing, using a second print system, a second metallic material comprising a copper based alloy to form, on the propellant manifold, an injector plate penetrated by the at least one propellant channel, such that the part is printed as an integral piece;
wherein a diffusion region is formed between a portion of the propellant manifold and a portion of the injector plate, and wherein the diffusion region comprises a gradient of compositions between the nickel based alloy and the copper based alloy.