Methods and Systems for Reducing Turbidity of Hydraulic Fracturing Sands

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
18/916,343
Abstract

A method for reducing the turbidity of as-mined sand comprising adding water to the as-mined sand to increase its moisture content to between about 5% and about 40% by weight, mixing the sand and water, piling the wet sand on the ground, allowing the sand to rest for a predetermined period of between about 12 hours and about 3 days, then harvesting less than all of the sand from the pile as reduced turbidity sand.

Claims (25)

1 . A method of reducing the turbidity of as-mined sand, comprising the steps of:

mining sand having an as-mined turbidity of more than 250 FTU or its equivalent;

wetting the as-mined sand with water having a turbidity of at least half of the as-mined turbidity of the sand;

creating a pile of the wetted sand;

allowing the pile of wetted sand to rest for a predetermined period of more than 24 hours;

harvesting after the predetermined period a portion of the sand from the pile, the harvested sand having a turbidity less than the turbidity of the as-mined sand.

2 . The method of claim 1 comprising wherein wetting the as-mined sand comprises raising the moisture content of the sand to between about 5% and about 40% by weight.

3 . The method of claim 2 , comprising providing a sand washing assembly having a body for containing the as-mined sand long with a predetermined volume of water, the sand washing assembly comprising a sand and water mixing component that also transports the sand and water from an inlet to an outlet.

4 . The method of claim 3 , comprising covering the pile of sand to reduce moisture loss during at least a portion of the predetermined period.

5 . The method of claim 2 , comprising determining a turbidity of the harvested sand.

6 . The method of claim 2 , comprising allowing the pile of wetted sand to rest for a predetermined period of more than 48 hours.

7 . The method of claim 5 , comprising allowing the pile of wetted sand to rest for a predetermined period of less than 72 hours.

8 . The method of claim 6 , comprising allowing the pile of wet sand to rest for a predetermined period of more than 72 hours.

9 . The method of claim 2 , comprising harvesting at least 50% of the pile after the predetermined period.

10 . The method of claim 8 , comprising harvesting at 90% or less of the pile after the predetermined period.

11 . The method of claim 2 , comprising wetting the harvested sand to raise its moisture content to between about 5% and about 40% by weight; creating a pile of the wetted sand; allowing the pile of wetted sand to rest for a predetermined period of more than 24 hours; harvesting after the predetermined period a portion of the pile having a turbidity less than turbidity of the harvested sand.

12 . The method of claim 2 , wherein creating the pile of sand comprises transporting the wet sand along a belt conveyor to a discharge end.

13 . The method of claim 12 , wherein the belt conveyor comprises a water spray system arranged to apply the water to the as-mined sand on the belt.

14 . The method of claim 13 , wherein the belt conveyor comprises a dewatering belt.

15 . The method of claim 3 , wherein the washing assembly discharges wet sand to a belt conveyor for creating the pile of wet sand.

16 . The method of claim 15 , wherein the belt conveyor comprises a dewatering belt.

17 . The method of claim 16 , wherein the belt conveyor comprises a water spray system arranged to apply additional water to wet sand on the belt.

18 . The method of claim 1 , wherein the water added to the as-mined sand does not create a sand-water slurry.

19 . The method of claim 18 , wherein the water added to the as-mined sand raises the moisture content of the as-mined sand by up to about 40% by weight.

20 . The method of claim 1 , further comprising removing non-sand debris and contaminants from the as-mined sand prior to or after wetting the sand.

Assignments (2)
SECURITY INTEREST Recorded Aug 28, 2025
From: PROPFLOW, LLC
To: STONEBRIAR COMMERCIAL FINANCE LLC, AS ADMINISTRATIVE AGENT
Reel/Frame 072696/0475 →
NUNC PRO TUNC ASSIGNMENT Recorded Jun 12, 2025
From: MITCHELL, JEREMY BRITT; MARTIN, CHRISTOPHER SHANE
To: PROPFLOW, LLC
Reel/Frame 071574/0225 →