IP Library Granted Patent US 7,056,563
Granted Patent B2
US 7,056,563 · App. 10/846,761 · Granted Jun 6, 2006

Hot cup made from an insulating paperboard

Assignee: Weyerhaeuser Company
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,056,563
App. No.
10/846,761
Granted
Jun 6, 2006
Kind
B2
Abstract

An insulating paperboard contains at least one layer of cellulose fibers. The one layer is at least partially composed of bulky fibers. The paperboard is sufficiently insulated to provide a hot water ΔT across the paperboard of at least 0.7° C.±2.3° C. per 0.1 mm of caliper. The paperboard may be embossed to decrease surface transmission of heat. A hot cup may be produced from the insulating paperboard.

Claims (7)

1. A container made from an insulating paperboard comprising:

a sidewall and a bottom wall, said sidewall comprising an insulating paperboard having at least one layer of cellulose fibers, at least some of the cellulose fibers in said at least one layer being crosslinked cellulosic fibers present in an amount from 25% to 100% of said at least one layer, said paperboard being sufficiently insulating to provide a hot water ΔT across said paperboard of at least 0.7° C.±2.3° C. per 0.1 mm of caliper, said paperboard having a density of less than 0.5 g/cc, said paperboard having a basis weight of from 200 gsm to 500 gsm, the caliper of said paperboard being greater than or equal to 0.5 mm.

2. The container of claim 1 , wherein said paperboard has a basis weight greater than or equal to 250 gsm.

3. The container of claim 2 , wherein said paperboard has a hot water ΔT of 9° C.±2.3° C. at a caliper of 0.6 mm and a hot water ΔT of 14° C.±2.3° C. at a caliper of 1.25 mm, said hot water ΔT being a substantially linear progression relative to caliper in the temperature range from below 9° C. to above 14° C.

4. The container of claim 3 , wherein said linear progression extends from a ΔT of 9° C. to a ΔT of 14° C.

5. The container of claim 1 , wherein said paperboard is at least a two-ply board, at least one ply containing said crosslinked cellulose fibers.

6. The container of claim 1 comprising a hot cup.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 14, 2004
From: HALABISKY, DONALD D.
To: WEYERHAEUSER COMPANY
Reel/Frame 015339/0428 →
Continuity (2)
Continuation In Part 1040756900 · Apr 4, 2003
Related Publication 20040213930A1 · Oct 28, 2004