IP Library Granted Patent US 8,025,160
Granted Patent B2
US 8,025,160 · App. 12/116,405 · Granted Sep 27, 2011

Sulfur-impregnated organoclay mercury and/or arsenic ion removal media

Assignee: Amcol International Corporation
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,025,160
App. No.
12/116,405
Granted
Sep 27, 2011
Kind
B2
Abstract

The use of a sulfur-impregnated organoclay provides a mercury or arsenic removal media having increased reactivity, stability, and mercury removal ability. The Hg/As removal media described herein is prepared by impregnating an organophilic clay with elemental (free state) sulfur. Alternatively, the clay can be made organophilic by onium ion reaction prior to or simultaneously with impregnating the organoclay with sulfur.

Claims (36)

1. A contaminant removal media for removing mercury and/or arsenic from water or removing mercury from a gas, by contact, comprising: an intimate mixture of an organoclay and elemental sulfur in its free state.

2. The contaminant removal media of claim 1 , wherein the percentage of components is as follows:

a) organoclay: 50 to 99.5 wt. %;

b) elemental sulfur: 0.5 to 50 wt. %.

3. The contaminant removal media of claim 2 , wherein the organoclay comprises a layered phyllosilicate intercalated with an intercalant agent, and wherein the percentage of components is as follows:

a) phyllosilicate: 1-90%; intercalant agent 10-50%;

b) elemental sulfur: 0.5-50%.

4. The contaminant removal media of claim 3 , wherein the percentage of components is as follows:

a) phyllosilicate: 35-83%; intercalant agent 15-45%;

b) elemental sulfur: 2-20%.

5. The contaminant removal media of claim 4 , wherein the percentage of components is as follows:

a) phyllosilicate: 50-77%; intercalant agent 20-40%;

b) elemental sulfur: 3-10%.

6. The contaminant removal media of claim 5 , wherein the percentage of components is as follows:

a) phyllosilicate: 59-71%; intercalant agent 25-35%;

b) elemental sulfur: 4-6%.

7. The contaminant removal media of claim 6 , wherein the percentage of components is as follows:

a) phyllosilicate: 65%; intercalant agent 30%;

b) elemental sulfur: 5%.

8. The contaminant removal media of claim 1 , wherein the mixture is compacted in an extruder.

9. The contaminant removal media of claim 1 , wherein the elemental sulfur has a particle size such that at least 80% by weight of the particles are finer than 18 mesh, U.S. Sieve Series.

10. The contaminant removal media of claim 9 , wherein the elemental sulfur has a particle size such that at least 80% by weight of the particles are finer than 50 mesh, U.S. Sieve Series.

11. The contaminant removal media of claim 10 , wherein the elemental sulfur has a particle size such that at least 80% by weight of the particles are finer than 70 mesh, U.S. Sieve Series.

12. The contaminant removal media of claim 11 , wherein the elemental sulfur has a particle size such that at least 80% by weight of the particles are finer than 80 mesh, U.S. Sieve Series.

13. The contaminant removal media of claim 12 , wherein the elemental sulfur has a particle size such that at least 80% by weight of the particles are finer than 100 mesh, U.S. Sieve Series.

14. The contaminant removal media of claim 1 , wherein the media comprises particles having a particle size such that at least 80% by weight of the particles are finer than 5 mm.

15. The contaminant removal media of claim 14 , wherein the media comprises particles having a particle size such that at least 80% by weight of the particles are finer than 3 mm.

16. The contaminant removal media of claim 15 , wherein the media comprises particles having a particle size such that at least 80% by weight of the particles are finer than 2 mm.

17. A contaminant removal media for removing mercury or arsenic from water or for removal of mercury from a gas, by contact, comprising: an intimate mixture of a layered phyllosilicate intercalated with a surface-modifying, layer-expanding intercalant and elemental sulfur in its free state.

18. The contaminant removal media of claim 17 , wherein the mixture is compacted in an extruder.

19. The contaminant removal media of claim 17 , wherein the layer-expanding intercalant is selected from the group consisting of onium ions, a polymer, and a mixture thereof.

20. The mercury removal media of claim 16 , wherein the elemental sulfur has a particle size such that at least 80% of the particles are finer than 18 mesh, U.S. Sieve Series.

21. The mercury removal media of claim 20 , wherein the elemental sulfur has a particle size such that at least 80% of the particles are finer than 50 mesh, U.S. Sieve Series.

22. The mercury removal media of claim 21 , wherein the elemental sulfur has a particle size such that at least 80% of the particles are finer than 70 mesh, U.S. Sieve Series.

23. The mercury removal media of claim 22 , wherein the elemental sulfur has a particle size such that at least 80% of the particles are finer than 80 mesh, U.S. Sieve Series.

24. The mercury removal media of claim 23 , wherein the elemental sulfur has a particle size such that at least 80% of the particles are finer than 100 mesh, U.S. Sieve Series.

Assignments (2)
SECURITY INTEREST Recorded May 15, 2014
From: AMCOL INTERNATIONAL CORPORATION
To: JPMORGAN CHASE BANK, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 032918/0776 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 7, 2008
From: WANG, ZHEN; ABRAHAM, ROBERT
To: AMCOL INTERNATIONAL CORPORATION
Reel/Frame 020912/0704 →
Continuity (2)
Continuation In Part 11810363 · Jun 5, 2007
Related Publication 20080302730A1 · Dec 11, 2008