IP Library Granted Patent US 8,043,081
Granted Patent B2
US 8,043,081 · App. 11/581,448 · Granted Oct 25, 2011

Mold for forming developer blade, and developer blade formed with same

Assignee: Bridgestone Corporation
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,043,081
App. No.
11/581,448
Granted
Oct 25, 2011
Kind
B2
Abstract

The present invention provide a mold for forming a developer blade and a developer blade manufactured with such a mold which are able to give images of good quality even in the low-temperature low-humidity condition and to improve a mold releasability. A mold 10 for forming a developer blade has a plate accommodation space 14 in which the metal plate is accommodated and a belt-like cavity 15 for forming the elastic member adjacent to the plate accommodation space. At least a part 20 a of a cavity surface 20 defining the cavity 15 in the cross section taken along the cavity width direction is finished to have a surface roughness Ry of not more than 10 μm.

Claims (6)

1. A mold for forming a developer blade having a belt-like metal plate and an elastic member adhering to the metal plate in parallel with the metal plate, wherein the mold comprises a plate accommodation space in which the metal plate is accommodated and a belt-like cavity for forming the elastic member adjacent to the plate accommodation space, and wherein at least a part of a cavity surface defining the cavity in the cross section taken along the cavity width direction is finished to have a surface roughness Ry of not more than 10 μm, and wherein when the cavity surface is divided into two sides in the cross section taken along the cavity width direction with a given point on the surface being as their border, each side having a different roughness, only one side is finished to have a surface roughness Ry of not more than 10 μm and the cavity surface of the other side has a surface roughness of not more than 1.5 μm, and

border point ( 21 ) are arranged near point (Q) on the cavity surface corresponding to a development roller closet point (P) on the elastic member in a position where the developer blade is to be installed in a device, the border point on the cavity surface as a border is arranged such that the distance in either direction from the point (Q) on the cavity surface corresponding to the point (P) has a value of up to 2 mm in the cross section taken along the cavity width direction.

2. The mold for forming a developer blade according to claim 1 , wherein at least the part of the cavity surface is finished by a texturing process.

3. The mold for forming a developer blade according to claim 1 , wherein at least the part of the cavity surface is finished by a texturing process or a sandblasting process and then by a beadblasting process.

4. The mold for forming a developer blade according to claim 1 , wherein the finished surface has a surface roughness of 0.5-5.0 μm.

5. The mold for forming a developer blade according to claim 1 , wherein at least the part of the cavity surface comprises alternatively arranged projections and depressions.

Assignments (2)
ABSORPTION-TYPE COMPANY SPLIT Recorded Aug 26, 2022
From: BRIDGESTONE CORPORATION
To: ARCHEM INC.
Reel/Frame 061328/0297 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 3, 2007
From: GOTO, TAIHEI
To: BRIDGESTONE CORPORATION
Reel/Frame 018747/0774 →
Priority Claims (2)
JP 2005-301868 · Oct 17, 2005 · national
JP 2006-122984 · Apr 27, 2006 · national
Continuity (1)
Related Publication 20070114357A1 · May 24, 2007