IP Library Granted Patent US 8,292,763
Granted Patent B2
US 8,292,763 · App. 12/923,178 · Granted Oct 23, 2012

Composition of baseball's core

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,292,763
App. No.
12/923,178
Granted
Oct 23, 2012
Kind
B2
Abstract

A baseball includes a core comprised of coconut fiber, rubber, and solvent; and a cover sewn on the core by stitches. The coconut fiber having a predetermined percentage by weight is crushed, the rubber having a predetermined percentage by weight is gelled, the coconut fiber and the rubber are mixed with the solvent having a predetermined percentage by weight, and the mix is subjected to molding, heating, and cooling to produce the core.

Claims (7)

1. A baseball comprising:

a core comprised of coconut fiber, rubber, and solvent; and

a cover sewn on the core by stitches,

wherein the coconut fiber having a predetermined percentage by weight is crushed, the rubber having a predetermined percentage by weight is gelled, the coconut fiber and the rubber are mixed with the solvent having a predetermined percentage by weight, and the mix is subjected to molding, heating, and cooling to produce the core;

wherein the coconut fiber is comprised of cellulose, lignin, half-cellulose, and pectin with the remaining consisting of minerals in which cellulose has 46% to 64% by weight, lignin has 31% to 36% by weight, half-cellulose has 0.15% to 0.25% by weight, and pectin has 3% to 4% by weight.

2. The baseball of claim 1 , wherein the predetermined percentage by weight of the coconut fiber is 40% to 70%, the predetermined percentage by weight of the rubber is 25% to 55%, and the predetermined percentage by weight of the solvent is 1% to 2%.

3. The baseball of claim 1 , wherein the core further comprises sawdust having a predetermined percentage by weight, and wherein the predetermined percentage by weight of the coconut fiber is 25% to 55%, the predetermined percentage by weight of the rubber is 25% to 55%, the predetermined percentage by weight of the solvent is 1% to 2%, and the predetermined percentage by weight of the sawdust is 10% to 35%.