Method of forming solid state electrolyte having high lithium ion conduction and battery incorporating same

Inventor: Isaiah O. Oladeji (Gotha, FL)
Assignee: Sisom Thin Films, LLC
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,372,163
App. No.
13/573,094
Granted
Feb 12, 2013
Kind
B2
Abstract

A method for making ion conducting films includes the use of primary inorganic chemicals, which are preferably water soluble; formulating the solution with appropriate solvent, preferably deionized water; and spray depositing the solid electrolyte matrix on a heated substrate, preferably at 100 to 400° C. using a spray deposition system. In the case of lithium, the deposition step is then followed by lithiation or addition of lithium, then thermal processing, at temperatures preferably ranging between 100 and 500° C., to obtain a high lithium ion conducting inorganic solid state electrolyte. The method may be used for other ionic conductors to make electrolytes for various applications. The electrolyte may be incorporated into a lithium ion battery.

Claims (26)

1. A method of making a Li-ion battery comprising the steps of:

a) providing a first current collector comprising a metallic sheet;

b) depositing a cathode material on said first current collector;

c) depositing an electrolyte matrix material on said cathode material;

d) depositing Li onto said electrolyte matrix;

e) annealing at a temperature from 100 to 500° C. to react said Li and said electrolyte matrix to form a Li ion conducting electrolyte;

f) depositing an anode material onto said Li conducting electrolyte; and,

g) applying a second current collector to said anode material.

2. The method of claim 1 wherein said first current collector comprises a foil selected from the group consisting of Al, Cu, and their alloys.

3. The method of claim 1 wherein said cathode material is selected from the group consisting of: LiMn 2 O 4 , LiMnNiCoAlO 2 , and LiFePO 4 .

4. The method of claim 1 wherein said electrolyte matrix material comprises: a metal selected from the group consisting of: B, Al, Ga, Ge, and Si; sulfur; and an anion selected from the group consisting of: BO 3 3− and PO 4 3− .

5. The method of claim 1 wherein said anode material is selected from the group consisting of Li, Li-Al alloys, and Li-Mg alloys.

6. The method of claim 1 wherein said second current collector comprises a metal foil, and further comprising affixing said second current collector onto said anode material using conductive adhesive.

7. A method of making a Li-ion battery comprising the steps of:

a) providing a first current collector comprising a metallic sheet;

b) depositing an anode material on said first current collector;

c) depositing an electrolyte matrix material on said anode material;

d) depositing Li onto said electrolyte matrix;

e) annealing at a temperature from 100 to 500° C. to react said Li and said electrolyte matrix to form a Li ion conducting electrolyte;

f) depositing a cathode material onto said Li conducting electrolyte; and,

g) applying a second current collector to said cathode material.

8. The method of claim 7 wherein said first current collector comprises a foil selected from the group consisting of Al, Cu, and their alloys.

9. The method of claim 7 wherein said cathode material is selected from the group consisting of: LiMn 2 O 4 , LiMnNiCoAlO 2 , and LiFePO 4 .

10. The method of claim 7 wherein said electrolyte matrix material comprises: a metal selected from the group consisting of: B, Al, Ga, Ge, and Si; sulfur; and an anion selected from the group consisting of: BO 3 3− and PO 4 3− .

11. The method of claim 7 wherein said anode material is selected from the group consisting of Li, Li-Al alloys, and Li-Mg alloys.

12. The method of claim 7 wherein said second current collector comprises a metal foil, and further comprises affixing said second current collector onto said cathode material using conductive adhesive.

Assignments (4)
CHANGE OF NAME Recorded Mar 2, 2023
From: QUANTUMSCAPE SUBSIDIARY, INC.
To: QUANTUMSCAPE BATTERY, INC.
Reel/Frame 062915/0514 →
CHANGE OF NAME Recorded Feb 23, 2023
From: QUANTUMSCAPE CORPORATION
To: QUANTUMSCAPE SUBSIDIARY, INC.
Reel/Frame 062841/0762 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 13, 2014
From: SISOM THIN FILMS LLC
To: QUANTUMSCAPE CORPORATION
Reel/Frame 032073/0026 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 14, 2012
From: OLADEJI, ISAIAH O.
To: SISOM THIN FILMS, LLC
Reel/Frame 029405/0667 →
Continuity (3)
Division 12798515 · Apr 6, 2010
Continuation In Part 12656000 · Jan 12, 2010
Related Publication 20120317797A1 · Dec 20, 2012