IP Library Granted Patent US 8,535,395
Granted Patent B2
US 8,535,395 · App. 13/069,639 · Granted Sep 17, 2013

Beam welding of a multi-sheet work stack having a reduced thickness feature

Inventors: Wayne W. Cai (Troy, MI); Thomas B. Stoughton (Birmingham, MI); David Yang (Pudong, CN); Xiang Zhao (Novi, MI)
Assignee: GM Global Technology Operations LLC
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,535,395
App. No.
13/069,639
Filed
Mar 23, 2011
Granted
Sep 17, 2013
Kind
B2
Art Unit
3742
USPC
219/121.14
Abstract

A method for beam welding a multi-sheet work stack includes providing a reduced thickness feature in a first sheet, positioning the first sheet adjacent to a second sheet to define a first welding interface, and positioning a third sheet adjacent to the second sheet to define a second welding interface. A laser or electron beam is directed through the first sheet at the feature to form a fusion weld at one of the welding interfaces. A second beam may be directed onto the other interface to form a second fusion weld. Providing a reduced thickness feature in the first sheet may include forming the feature with the beam and mechanically pre-forming the feature. One of the interfaces may be pre-heated using the beam, and the beam may be split using a beam splitter to form multiple beams. A welded assembly formed via the method is also disclosed.

Claims (36)

1. A method for beam welding a multi-sheet work stack, comprising:

positioning a first sheet having a reduced thickness feature adjacent to a second sheet to thereby define a first welding interface;

positioning a third sheet of the work stack adjacent to the second sheet to thereby define a second welding interface; and

directing an energy beam through the reduced thickness feature of the first sheet to thereby form a first fusion weld at the first welding interface.

2. The method of claim 1 , further comprising:

directing another energy beam through the third sheet to thereby form a second fusion weld at the second welding interface.

3. The method of claim 1 , further comprising one of: forming the reduced thickness feature using the energy beam and mechanically pre-forming the reduced thickness feature.

4. The method of claim 1 , further comprising:

pre-heating the first welding interfaces using the energy beam.

5. The method of claim 1 , further comprising:

splitting the energy beam using a beam splitter to thereby form multiple energy beams.

6. The method of claim 1 , wherein the reduced thickness feature includes one of a hole, a groove, a slot, and a trench defined by the first sheet.

7. The method of claim 1 , further comprising:

positioning a first beam source adjacent to the third sheet;

positioning a second beam source adjacent to the first sheet; and

independently controlling the first and second beam sources.

8. The method of claim 1 , wherein the reduced surface feature is annular, the method further comprising:

generating the energy beam using a beam source; and

rotating the beam source to thereby direct the energy beam in an annular pattern through the reduced surface feature.

9. A method for beam welding a battery module having a first battery tab, a second battery tab, and a conductive interconnect member, comprising:

positioning the interconnect member adjacent to the first battery tab to thereby define a first welding interface, wherein the interconnect member has a reduced thickness feature;

positioning the second battery tab adjacent to the first battery tab to thereby define a second welding interface; and

directing an energy beam through the reduced thickness feature to thereby form a first fusion weld at the first welding interface, wherein the energy beam is one of a laser beam and an electron beam.

10. The method of claim 9 , further comprising:

directing another energy beam through the second battery tab to thereby form a second fusion weld at the second welding interface.

11. The method of claim 9 , further comprising one of: forming the reduced thickness feature using the energy beam and mechanically pre-forming the reduced thickness feature.

12. The method of claim 9 , further comprising:

pre-heating the first welding interfaces using the energy beam.

13. The method of claim 9 , further comprising:

splitting the energy beam using a beam splitter to thereby form multiple energy beams.

14. The method of claim 13 , further comprising:

using one energy beam of the multiple beams to form the reduced thickness feature and to preheat the first welding interface, and using another energy beam of the multiple beams to form the first fusion weld.

15. The method of claim 9 , further comprising:

positioning a first beam source adjacent to the second battery tab;

positioning a second beam source adjacent to the interconnect member; and

independently controlling the first and second beam sources to form fusion welds at the first and the second welding interfaces.

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Nov 7, 2014
From: WILMINGTON TRUST COMPANY
To: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Reel/Frame 034287/0159 →
SECURITY AGREEMENT Recorded Jun 28, 2012
From: GM GLOBAL TECHNOLOGY OPERATIONS LLC
To: WILMINGTON TRUST COMPANY
Reel/Frame 028466/0870 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 23, 2011
From: CAI, WAYNE W.; STOUGHTON, THOMAS B.; YANG, DAVID; ZHAO, XIANG
To: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Reel/Frame 026004/0732 →
Continuity (1)
Related Publication 20120241422A1 · Sep 27, 2012