Modified asphalt binder material using crumb rubber and methods of manufacturing a modified asphalt binder
In a first aspect, bituminous asphalt binder materials which are modified by the addition of crumb rubber or ground tire rubber are described. In a second aspect, the present invention is directed to methods of producing a modified asphalt binder containing crumb rubber or ground tire rubber. The modified asphalt binders comprise neat asphalt, crumb rubber, one or more synthetic polymers, and one or more acids. The crumb rubber may be obtained from recycled truck and/or automobile tires.
1. A modified asphalt binder composition, comprising:
(a) about 40% by weight to about 98.9% by weight asphalt binder material;
(b) about 0.5% by weight to about 25% by weight crumb rubber;
(c) about 0.5% by weight to about 30% by weight of at least one synthetic polymer; and
(d) about 0.05% by weight to about 5% by weight of at least one acid selected from the group consisting of phosphoric acid, polyphoshoric acid, sulfuric acid at more than 90% wt, boric acid, adipic acid, citric acid, oxalic acid, tartaric acid, maleic acid, valeric acid, succinic acid, fumaric acid, glutamic acid, phatalic acid, acetic acid, and combinations thereof.
2. The composition of claim 1 , wherein a substantial portion of the crumb rubber has a particle size of less than 2 mm.
3. The composition of claim 2 , wherein the at least one synthetic polymer is selected from the group consisting of styrene butadiene, styrene butadiene styrene three block (SBS), ethylene vinyl acetate, ethylene propylene copolymers, polyvinylchorlide (PVC), nylon, polysterene, polybutadiene, acrylate resins, flurorocarbon resins, phenolic resins, alkyd resins, polyesters, linear polyethylene, crosslinked polyethylene, epoxy terpolymer, polypropylene, and combinations thereof.
4. The composition of claim 2 , wherein the synthetic polymer is styrene butadiene styrene and the acid is polyphosphoric acid.
5. The composition of claim 4 , wherein the asphalt binder composition comprises
(a) about 92% by weight to about 95% by weight asphalt binder material;
(b) about 3% by weight to about 5% by weight crumb rubber;
(c) about 0.5% by weight to about 2% by weight of at least one synthetic polymer; and
(d) about 0.1% by weight to about 1% by weight of at least one acid selected from the group consisting of phosphoric acid, polyphosphoric acid, sulfuric acid at more than 90% wt, boric acid, adipic acid, citric acid, oxalic acid, tartaric acid, maleic acid, valeric acid, succinic acid, fumaric acid, glutamic acid, phthalic acid, acetic acid, and combinations thereof.
6. The composition of claim 5 , wherein the synthetic polymer is styrene butadiene styrene and the acid is polyphosphoric acid.