Method of manufacturing a printable composition of a liquid or gel suspension of diodes

Inventors: Mark D. Lowenthal (Gilbert, AZ); William Johnstone Ray (Fountain Hills, AZ); Neil O. Shotton (Tempe, AZ); Richard A. Blanchard (Los Altos, CA); Mark Allan Lewandowski (North Port, FL); Brad Oraw (Mesa, AZ); Jeffrey Baldridge (Chandler, AZ); Eric Anthony Perozziello (Stanford, CA)
Assignee: NthDegree Technologies Worldwide Inc
H01L27/3281H01L2924/09701H01L51/52Y02E10/544H01L31/184H01L33/382H01L27/1422H01L33/20H01L31/035281H01L31/02363H01L31/1848H01L31/022408H01L51/5203H01L51/56H01L21/6836H01L24/95H01L25/048H01L31/1844H01L33/38
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,852,467
App. No.
13/223,286
Granted
Oct 7, 2014
Kind
B2
Abstract

An exemplary printable composition of a liquid or gel suspension of diodes comprises a plurality of diodes, a first solvent and/or a viscosity modifier. An exemplary method of making a liquid or gel suspension of diodes comprises: adding a viscosity modifier to a plurality of diodes in a first solvent; and mixing the plurality of diodes, the first solvent and the viscosity modifier to form the liquid or gel suspension of the plurality of diodes. Various exemplary diodes have a lateral dimension between about 10 to 50 microns and about 5 to 25 microns in height. Other embodiments may also include a plurality of substantially chemically inert particles having a range of sizes between about 10 to about 50 microns.

Claims (112)

1. A method of making a liquid or gel suspension of diodes for printing, the method comprising:

adding a viscosity modifier to a plurality of diodes in a first solvent, each diode of the plurality of diodes comprising:

a light emitting or absorbing region, the light emitting or absorbing region having a mesa region;

at least one first terminal coupled to the light emitting or absorbing region on a first side and located peripherally to the mesa region; and

a second terminal coupled centrally to the mesa region on the first side;

wherein each diode has a lateral dimension less than about 50 microns and a height less than about 25 microns; and

mixing the plurality of diodes, the first solvent and the viscosity modifier to form the liquid or gel suspension of the plurality of diodes.

2. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes is mixed until the viscosity is at least about 100 centipoise (cps) measured at about 25° C.

3. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes is mixed until the viscosity is at least about 1,000 centipoise (cps) measured at about 25° C.

4. The method of claim 1 , further comprising:

adding a plurality of substantially chemically inert particles to the mixture of the plurality of diodes, the first solvent and the viscosity modifier.

5. The method of claim 4 , wherein each particle of the plurality of substantially chemically inert particles has a size between about 10 microns to about 70 microns in any dimension.

6. The method of claim 4 , wherein the plurality of substantially chemically inert particles are substantially optically transmissive and each particle of the plurality of substantially chemically inert particles has a size between about 10 microns to about 30 microns in any dimension.

7. The method of claim 6 , wherein the plurality of substantially chemically inert particles are comprised of a silica glass.

8. The method of claim 1 , wherein the first solvent comprises at least one solvent selected from the group consisting of: water; alcohols, cyclic alcohols, ethers, esters, glycols, glycerols, carbonates, acetonitrile, tetrahydrofuran (THF), dimethyl formamide (DMF), N-methyl formamide (NMF), dimethyl sulfoxide (DMSO), and mixtures thereof.

9. The method of claim 1 , wherein the viscosity modifier comprises at least one viscosity modifier selected from the group consisting of: clays, saccharides, polysaccharides, celluloses, modified celluloses, acrylate polymers and copolymers, (meth)acrylate polymers and copolymers, polyvinyl polymers and copolymers, polyethylene polymers and copolymers, ethers, esters, acetates, glycols, glycerols, fumed silica, silica powders, modified ureas, and mixtures thereof.

10. The method of claim 1 , further comprising:

adding a second solvent to the plurality of diodes, the first solvent and the viscosity modifier, the second solvent different from the first solvent; and

mixing the plurality of diodes, the first solvent, the second solvent, and the viscosity modifier.

11. The method of claim 10 , wherein the second solvent is at least one solvent selected from the group consisting of: water; alcohols, cyclic alcohols, ethers, esters, glycols, glycerols, carbonates, acetonitrile, tetrahydrofuran (THF), dimethyl formamide (DMF), N-methyl formamide (NMF), dimethyl sulfoxide (DMSO), and mixtures thereof.

12. The method of claim 10 , further comprising:

mixing the plurality of diodes, the first solvent, the second solvent, and the viscosity modifier for about 25 to 30 minutes in an air atmosphere.

13. The method of claim 10 , wherein the first solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 5% to 50% by weight; wherein the viscosity modifier comprises methoxy propyl methylcellulose resin or hydroxy propyl methylcellulose resin or mixtures thereof, and present in an amount of about 0.10% to 5.0% by weight; wherein the second solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 0.3% to 50% by weight.

14. The method of claim 13 , further comprising:

adding a plurality of substantially optically transparent and chemically inert particles having a range of sizes between about 10 to about 50 microns and present in an amount of about 0.1% to 2.5% by weight.

15. The method of claim 10 , wherein the first solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2- propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 5% to 30% by weight; wherein the viscosity modifier comprises methoxy propyl methylcellulose resin or hydroxy propyl methylcellulose resin or mixtures thereof, and present in an amount of about 1.0% to 3.0% by weight; wherein the second solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 0.2% to 8.0% by weight; and wherein the balance of the method further comprises water.

16. The method of claim 15 , further comprising:

adding a plurality of substantially optically transparent and chemically inert particles having a range of sizes between about 10 to about 50 microns and present in an amount of about 0.1% to 2.5% by weight.

17. The method of claim 10 , wherein the first solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 40% to 60% by weight; wherein the viscosity modifier comprises methoxy propyl methylcellulose resin or hydroxy propyl methylcellulose resin or mixtures thereof, and present in an amount of about 0.10% to 1.5% by weight; wherein the second solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 40% to 60% by weight.

18. The method of claim 17 , further comprising:

adding a plurality of substantially optically transparent and chemically inert particles having a range of sizes between about 10 to about 50 microns and present in an amount of about 0.1% to 2.5% by weight.

19. The method of claim 10 , wherein the second solvent is at least one dibasic ester.

20. The method of claim 10 , wherein the second solvent comprises:

dimethyl glutarate; and

dimethyl succinate;

wherein the ratio of dimethyl glutarate to dimethyl succinate is about two to one (2:1).

21. The method of claim 10 , wherein the second solvent is present in an amount of about 0.1% to 10% by weight.

22. The method of claim 10 , wherein the second solvent is present in an amount of about 10% to 50% by weight.

23. The method of claim 1 , wherein prior to the step of adding a viscosity modifier, the method further comprising:

releasing the plurality of diodes from a wafer into a third solvent.

24. The method of claim 23 , wherein the step of releasing the plurality of diodes from the wafer further comprises using a laser to perform a laser lift-off of the plurality of diodes from a second, back of the wafer.

25. The method of claim 23 , further comprising:

substantially removing the third solvent; and

adding the first solvent.

26. The method of claim 25 , further comprising:

repeating the steps of substantially removing the third solvent and adding the first solvent until the amount of the third solvent remaining is under 1.0% by weight.

27. The method of claim 1 , wherein the light emitting or absorbing region of the diode comprises GaN and has a shape selected from the group consisting of: substantially hexagonal, substantially square, substantially triangular, substantially rectangular, substantially lobed, substantially stellate, substantially toroidal, and combinations thereof.

28. The method of claim 1 , wherein the light emitting or absorbing region of each diode of the plurality of diodes has a surface texture selected from the group consisting of: a plurality of circular rings, a plurality of substantially curvilinear trapezoids, a plurality of parallel stripes, a stellate pattern, and combinations thereof.

29. The method of claim 1 , wherein each diode of the plurality of diodes has a diameter between about 20 to 30 microns and a height between about 5 to 15 microns.

30. The method of claim 1 , wherein each diode of the plurality of diodes has a diameter between about 10 to 50 microns and a height between about 5 to 25 microns.

31. The method of claim 1 , wherein each diode of the plurality of diodes is substantially hexagonal laterally, has a diameter between about 10 to 50 microns measured opposing face-to face, and a height between about 5 to 25 microns.

32. The method of claim 1 , wherein each diode of the plurality of diodes is substantially hexagonal laterally, has a diameter measured opposing face-to face between about 20 to 30 microns and a height between about 5 to 15 microns.

33. The method of claim 1 , wherein each diode of the plurality of diodes has a width and length each between about 10 to 50 microns each and a height between about 5 to 25 microns.

34. The method of claim 1 , wherein each diode of the plurality of diodes has a width and length each between about 20 to 30 microns each and a height between about 5 to 15 microns.

35. The method of claim 1 , wherein a contact of the second terminal is spaced apart from at least one contact of the at least one first terminal by about 1 to 7 microns in height.

36. The method of claim 35 , wherein the at least one first terminal is between 0.5 to 2 microns in height, the second terminal is between about 1 to 8 microns in height, and the second metal terminal has one or more sides which are passivated.

37. The method of claim 1 , wherein each diode of the plurality of diodes has a plurality of lateral sides which are less than 10 microns in height.

38. The method of claim 1 , wherein each diode of the plurality of diodes has a plurality of lateral sides which are between about 2.5 to 6 microns in height.

39. The method of claim 1 , wherein each diode of the plurality of diodes has a plurality of lateral sides which are substantially sigmoidal and terminate in a curved point.

40. The method of claim 1 , wherein the viscosity modifier, when dried or cured, forms a polymer or resin lattice or structure substantially about the periphery of each diode of the plurality of diodes.

41. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes is visually opaque when wet and substantially optically clear when dried or cured.

42. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes has a contact angle greater than about 25 degrees or greater than about 40 degrees.

43. The method of claim 1 , wherein the plurality of diodes comprises at least one inorganic semiconductor selected from the group consisting of:

silicon, gallium arsenide (GaAs), gallium nitride (GaN), GaP, InAlGaP, AlInGaAs, InGaNAs, and AlInGaSb, and mixtures thereof.

44. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes has a relative evaporation rate less than one, wherein the evaporation rate is relative to butyl acetate having a rate of one.

45. The method of claim 1 , wherein the first solvent comprises at least one solvent selected from the group consisting of: cyclohexanol, dipropylene glycol, N-propanol, 1-octanol, 1-methoxy-2-propanol, propylene glycol, and mixtures thereof.

46. The method of claim 1 , wherein the first solvent is present in an amount of about 0.3% to 60% by weight.

47. The method of claim 1 , wherein the viscosity modifier comprises a methylcellulose resin.

48. The method of claim 1 , wherein the viscosity modifier comprises at least one viscosity modifier selected from the group consisting of: a hydroxy propyl methylcellulose resin, a methoxy propyl methylcellulose resin, a polyvinyl polymer, a polyvinyl copolymer, and mixtures thereof.

49. The method of claim 1 , wherein the viscosity modifier is present in an amount of about 0.10% to 5% by weight.

50. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes has a viscosity greater than about 100 centipoise (cps) measured at about 25° C.

51. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes has a viscosity between about 1,000 centipoise (cps) and about 25,000 centipoise (cps) measured at about 25° C.

52. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes has a viscosity between about 1,000 centipoise (cps) and about 10,000 centipoise (cps) measured at about 25° C.

53. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes has a viscosity between about 10,000 centipoise (cps) and about 25,000 centipoise (cps) measured at about 25° C.

54. The method of claim 1 , wherein the liquid or gel suspension of the plurality of diodes has a viscosity between about 20,000 centipoise (cps) and about 60,000 centipoise (cps) measured between about 5° C. and 10° C.

55. The method of claim 1 , wherein the first solvent comprises cyclohexanol.

56. The method of claim 1 , wherein the light emitting or absorbing region of each diode, of the plurality of diodes, has a lateral dimension less than about 50 microns and a height between 2.5 to 7 microns.

57. The method of claim 1 , wherein the at least one first terminal of each diode, of the plurality of diodes, further comprises a plurality of first terminals, the plurality of first terminals spaced apart from each other and coupled to the light emitting or absorbing region peripherally to the mesa region on the first side, and wherein each first terminal of the plurality of first terminals has a height between about 0.5 to 2 microns.

58. A method of making a liquid or gel suspension of diodes for printing, the method comprising:

adding a second solvent to a plurality of diodes in a first solvent, the second solvent different from the first solvent, each diode of the plurality of diodes comprising:

a light emitting or absorbing region, the light emitting or absorbing region having a mesa region;

at least one first terminal coupled to the light emitting or absorbing region on a first side and located peripherally to the mesa region; and

a second terminal coupled centrally to the mesa region on the first side;

wherein each diode has a lateral dimension less than about 50 microns and a height less than about 25 microns;

adding a viscosity modifier to the plurality of diodes, the first solvent and the second solvent;

adding a plurality of substantially chemically inert particles to the plurality of diodes, the first solvent, the second solvent and the viscosity modifier; and

mixing the plurality of diodes, the first solvent, the second solvent, the viscosity modifier, and the plurality of substantially chemically inert particles until the viscosity is at least about 100 centipoise (cps) measured at about 25° C. to form the liquid or gel suspension of the plurality of diodes.

59. The method of claim 58 , wherein each diode of the plurality of diodes has a lateral dimension between about 10 to 50 microns and a height between about 5 to 25 microns.

60. The method of claim 58 , wherein each particle of the plurality of substantially chemically inert particles has a size between about 10 microns to about 70 microns in any dimension.

61. The method of claim 58 , wherein the first solvent comprises at least one solvent selected from the group consisting of: water; alcohols, cyclic alcohols, ethers, esters, glycols, glycerols, carbonates, acetonitrile, tetrahydrofuran (THF), dimethyl formamide (DMF), N-methyl formamide (NMF), dimethyl sulfoxide (DMSO), and mixtures thereof.

62. The method of claim 58 , wherein the viscosity modifier comprises at least one viscosity modifier selected from the group consisting of: clays, saccharides, polysaccharides, celluloses, modified celluloses, acrylate polymers and copolymers, (meth)acrylate polymers and copolymers, polyvinyl polymers and copolymers, polyethylene polymers and copolymers, ethers, esters, acetates, glycols, glycerols, fumed silica, silica powders, modified ureas, and mixtures thereof.

63. The method of claim 58 , wherein the second solvent is at least one solvent selected from the group consisting of: water; alcohols, cyclic alcohols, ethers, esters, glycols, glycerols, carbonates, acetonitrile, tetrahydrofuran (THF), dimethyl formamide (DMF), N-methyl formamide (NMF), dimethyl sulfoxide (DMSO), and mixtures thereof.

64. The method of claim 58 , wherein the first solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 5% to 60% by weight; wherein the viscosity modifier comprises methoxy propyl methylcellulose resin or hydroxy propyl methylcellulose resin or mixtures thereof, and present in an amount of about 0.10% to 5.0% by weight; wherein the second solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 0.3% to 60% by weight.

65. The method of claim 58 , wherein each diode of the plurality of diodes has a plurality of lateral sides which are less than 10 microns in height.

66. The method of claim 58 , wherein each diode of the plurality of diodes has a plurality of lateral sides which are substantially sigmoidal and terminate in a curved point.

67. The method of claim 58 , wherein the first solvent comprises cyclohexanol.

68. The method of claim 58 , wherein the light emitting or absorbing region of each diode, of the plurality of diodes, has a lateral dimension less than about 50 microns and a height between 2.5 to 7 microns.

69. The method of claim 58 , wherein the at least one first terminal of each diode, of the plurality of diodes, further comprises a plurality of first terminals, the plurality of first terminals spaced apart from each other and coupled to the light emitting or absorbing region peripherally to the mesa region on the first side, and wherein each first terminal of the plurality of first terminals has a height between about 0.5 to 2 microns.

70. A method of making a liquid or gel suspension of diodes for printing, the method comprising:

adding a viscosity modifier to a plurality of diodes, a first solvent and a second solvent, the second solvent different from the first solvent, each diode of the plurality of diodes comprising:

a light emitting or absorbing region, the light emitting or absorbing region having a mesa region;

at least one first terminal coupled to the light emitting or absorbing region on a first side and located peripherally to the mesa region; and

a second terminal coupled centrally to the mesa region on the first side;

wherein each diode has a lateral dimension less than about 50 microns and a height less than about 25 microns;

adding a plurality of substantially chemically inert particles to the plurality of diodes, the first solvent, the second solvent and the viscosity modifier, wherein each particle of the plurality of substantially chemically inert particles has a size between about 10 microns to about 70 microns in any dimension; and

mixing the plurality of diodes, the first solvent, the second solvent, the viscosity modifier, and the plurality of substantially chemically inert particles until the viscosity is at least about 1,000 centipoise (cps) measured at about 25° C. to form the liquid or gel suspension of the plurality of diodes.

71. The method of claim 70 , wherein the first solvent comprises at least one solvent selected from the group consisting of: water; alcohols, cyclic alcohols, ethers, esters, glycols, glycerols, carbonates, acetonitrile, tetrahydrofuran (THF), dimethyl formamide (DMF), N-methyl formamide (NMF), dimethyl sulfoxide (DMSO), and mixtures thereof.

72. The method of claim 70 , wherein the viscosity modifier comprises at least one viscosity modifier selected from the group consisting of: clays, saccharides, polysaccharides, celluloses, modified celluloses, acrylate polymers and copolymers, (meth)acrylate polymers and copolymers, polyvinyl polymers and copolymers, polyethylene polymers and copolymers, ethers, esters, acetates, glycols, glycerols, fumed silica, silica powders, modified ureas, and mixtures thereof.

73. The method of claim 70 , wherein the second solvent is at least one solvent selected from the group consisting of: water; alcohols, cyclic alcohols, ethers, esters, glycols, glycerols, carbonates, acetonitrile, tetrahydrofuran (THF), dimethyl formamide (DMF), N-methyl formamide (NMF), dimethyl sulfoxide (DMSO), and mixtures thereof.

74. The method of claim 70 , wherein the first solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 5% to 60% by weight; wherein the viscosity modifier comprises methoxy propyl methylcellulose resin or hydroxy propyl methylcellulose resin or mixtures thereof, and present in an amount of about 0.10% to 5.0% by weight; wherein the second solvent comprises N-propanol, isopropanol, dipropylene glycol, diethylene glycol, propylene glycol, 1-methoxy-2-propanol, 1-octanol, ethanol, tetrahydrofurfuryl alcohol, or cyclohexanol, or mixtures thereof, and present in an amount of about 0.3% to 60% by weight.

75. The method of claim 70 , wherein each diode of the plurality of diodes has a plurality of lateral sides which are less than 10 microns in height.

76. The method of claim 70 , wherein each diode of the plurality of diodes has a plurality of lateral sides which are substantially sigmoidal and terminate in a curved point.

Assignments (4)
SECURITY INTEREST Recorded Mar 25, 2016
From: NTHDEGREE TECHNOLOGIES WORLDWIDE INC
To: PLANNING FOR SUCCESS LLC
Reel/Frame 038260/0049 →
TERMINATION OF SECURITY AGREEMENT Recorded Mar 25, 2014
From: MILLER INVESTMENT GROUP, LLC
To: NTHDEGREE TECHNOLOGIES WORLDWIDE INC.
Reel/Frame 032520/0108 →
SECURITY INTEREST Recorded May 1, 2012
From: NTHDEGREE TECHNOLOGIES WORLDWIDE INC
To: MILLER INVESTMENT GROUP, LLC; DACURO, LLC; JUST INK, LLC; JOSEPH A. NATHAN, INDIVIDUALLY AND AS TRUSTEE OF THE JOSEPH A. NATHAN LIVING TRUST; INSIGHT 2811 TECHNOLOGY ENTREPRENEUR FUND, LP; ALPHA CAPITAL, INC.; LOLE, CHRISTOPHER; PALISADE CONCENTRATED EQUITY PARTNERSHIP II, LP; MARGULIS, BRUCE A.; BIG BASIN PARTNERS LP; TIMARK LP; RICHARD A. BLANCHARD TRUSTEE OF THE RICHARD & ESTHER BLANCHARD 1990 TRUST 10/01/90; INSIGHT TECHNOLOGY CAPITAL PARTNERS, LP; BYRNE, ARTHUR; JAMES C. HOLMES JR., AS TRUSTEE OF THE JAMES C. HOLMES JR. TRUST, UTA DATED JANUARY 30, 1986, AS AMENDED; GORDON RAINS; INDIAN GROVE PRODUCTIONS; SIMONS, PETER; CHYE KIAT ANG; ROBINSON, PETER; JOSEPH A. NATHAN IRA ROLLOVER, MS & CO., CUSTODIAN; CORR INVESTMENTS LLC; DUNN INVESTMENT COMPANY INC; MIG, LLC; RUBAIYAT TRADING COMPANY, LTD.; TIMBERLINE HOLDINGS LLC; TIMBERLINE PRIVATE EQUITY INVESTMENTS LLC; DOLLY RIDGE LLC; FOSTER, A. KEY; CHARLES AND LYNDRA DANIEL, JTWROS; HARSH, MILTON; G. RUFFNER PAGE, JR.; PORTER, MARGARET M.; WHITE, JAMES H. III; PRICE, JOSEPH T.; P.C. JACKSON, JR.; RUSSELL, BENJAMIN; MILAGRO DE LADERA, L.P.; OAKWORTH CAPITAL BANK, AS TRUSTEE FOR RICHARD H. MONK, JR., INDIVIDUAL RETIREMENT ACCOUNT; SOCOLOF, JOSEPH D.; THOMPSON INVESTMENT COMPANY, LLC; LOGAN, GREG P.; JONES FOUNDATION III, LLC, THE; GORRIE, M. JAMES; JOHN STEINER TRUST U/W DOROTHY L. STEINER; STEWART MOTT DANSBY REVOCABLE TRUST
Reel/Frame 028146/0908 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 19, 2012
From: RAY, WILLIAM JOHNSTONE; LOWENTHAL, MARK DAVID; SHOTTON, NEIL O.; BLANCHARD, RICHARD A.; LEWANDOWSKI, MARK ALLAN; ORAW, BRAD; BALDRIDGE, JEFFREY; PEROZZIELLO, ERIC ANTHONY
To: NTHDEGREE TECHNOLOGIES WORLDWIDE INC
Reel/Frame 027888/0505 →
Continuity (18)
Continuation In Part 11756616 · May 31, 2007
Continuation In Part 12601268 · May 22, 2010
Continuation In Part 13149681 · May 31, 2011
Continuation In Part 12601271 · May 22, 2010
Continuation In Part 11756616
Continuation 11756619 · May 31, 2007
Continuation In Part 11756619 · May 31, 2007
Continuation In Part 11756616 · May 31, 2007
Continuation In Part 11756619 · May 31, 2007
Continuation In Part 11756619 · May 31, 2007
Continuation In Part 11756616 · May 31, 2007
Continuation In Part 11756619 · May 31, 2007
Continuation In Part 11756616 · May 31, 2007
Provisional Application 61379225 · Sep 1, 2010
Provisional Application 61379284 · Sep 1, 2010
Provisional Application 61379830 · Sep 3, 2010
Provisional Application 61379820 · Sep 3, 2010
Related Publication 20120164796A1 · Jun 28, 2012