IP Library Granted Patent US 9,493,701
Granted Patent B2
US 9,493,701 · App. 14/329,793 · Granted Nov 15, 2016

Red phosphor, method for producing red phosphor, white light source, illuminating device, and liquid crystal display device

Inventors: Takamasa Izawa (Tochigi, JP); Hiraku Akiho (Tochigi, JP); Tsuneo Kusunoki (Tochigi, JP); Takahiro Igarashi (Tochigi, JP); Masaki Kanno (Tochigi, JP)
Assignee: Dexerials Corporation
C09K11/7728C09K11/0883C09K11/7734F21K9/56G02F1/133609G02F1/133603G02F2001/133614H01L33/502H01L2224/48091H01L2924/181Y02B20/181
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,493,701
App. No.
14/329,793
Granted
Nov 15, 2016
Kind
B2
Abstract

A red phosphor of high efficiency and a method for producing it are provided. A white light source and an illumination device that allow illumination with the pure white color using the red phosphor are also provided. In addition, a liquid crystal display device using the red phosphor and exhibiting good color reproducing performance is provided. The red phosphor contains an element A, europium (Eu), silicon (Si), carbon (C), oxygen (O) and nitrogen (N) in the ratios of the numbers of atoms of the following compositional formula (1): [Chemical Formula 1] [A (m-x) Eu x ][Si (9-y) C y ]O n N [12-2(n-m)/3]    compositional formula (1) where the element A is at least one of magnesium (Mg), calcium (Ca), strontium (Sr) and barium (Ba), and where m, x and n in the compositional formula (1) satisfy the relationships of 3<m<5, 0<x<1, 0<y<2 and 0<n<10 (FIG. 5 A).

Claims (41)

1. A method for producing a red phosphor comprising:

mixing a carbonate of an element A, europium nitride, silicon nitride and melamine to form a mixture so that the element A, europium (Eu), silicon (Si) and carbon (C) have the ratios of the numbers of atoms according to the compositional formula (1):

[Chemical Formula 2]

[A (m-x) Eu x ][Si (9-y) C y ]O n N [12-2(n-m)/3]    compositional formula (1)

 where the element A is at least one of magnesium (Mg), calcium (Ca), strontium (Sr) and barium (Ba), and where m, x, y and n in the compositional formula (1) satisfy the relationships of 3<m<5, 0<x<1, 0<y<9 and 0<n<10;

sintering the mixture to a sintered product; and

pulverizing the sintered product,

wherein the ratio of the intensity of a peak existing at a position of the diffraction angle of 36.0° to 36.6° to that at a position of the diffraction angle of 35.0° to 36.0° in an X-ray diffraction pattern is 0.58 or higher.

2. The method for producing a red phosphor according to claim 1 , wherein the alkali earth metal element A includes at least calcium (Ca) and strontium (Sr) and wherein, with a ratio α of the number of atoms of Ca, a ratio β of the number of atoms of Sr and with a ratio γ of another element of the group II, the relationships (m=α+β+γ) and 0≦α/(α+β)≦0.3 are met.

3. A white light source comprising:

a blue light emitting diode provided on a device substrate; and

a kneaded mass arranged on the blue light emitting diode,

wherein the kneaded mass is a mass of a transparent resin obtained on kneading a red phosphor and a green phosphor together,

wherein the red phosphor containing an element A, europium (Eu), silicon (Si), carbon (C), oxygen (O) and nitrogen (N) in ratios of the numbers of atoms of the following compositional formula (1):

[Chemical Formula 1]

[A (m-x) Eu x ][Si (9-y) C y ]O n N [12-2(n-m)/3]    compositional formula (1)

 where the element A is at least one of magnesium (Mg), calcium (Ca), strontium (Sr) and barium (Ba), and where m, x, y and n in the compositional formula (1) satisfy the relationships of 3<m<5, 0<x<1, 0<y<9 and 0<n<10, and

wherein the ratio of the intensity of a peak existing at a position of the diffraction angle of 36.0° to 36.6° to that at a position of the diffraction angle of 35.0° to 36.0° in an X-ray diffraction pattern is 0.58 or higher.

4. The white light source according to claim 3 , wherein the alkali earth metal element A includes at least calcium (Ca) and strontium (Sr) and wherein, with a ratio α of the number of atoms of Ca, a ratio β of the number of atoms of Sr and with a ratio γ of another element of the group II, the relationships (m=α+β+γ) and 0≦α/(α+β)≦0.3 are met.

5. An illumination device comprising:

a plurality of white light sources arranged on an illumination substrate, each white light source including a blue light emitting diode provided or a device substrate; and

a kneaded mass arranged cm the blue light emitting diode,

wherein the kneaded mass is a mass of to transparent resin obtained on kneading a red phosphor and a green phosphor together,

wherein the red phosphor containing an element A, europium (Eu), silicon (Si), carbon (C), oxygen (O) and nitrogen (N) in ratios of the numbers of atoms of the following compositional formula (1):

[Chemical Formula 4]

[A (m-x) Eu x ][Si (9-y) C y ]O n N [12-2(n-m)/3]    compositional formula (1)

 where the element A is at least one of magnesium (Mg), calcium (Ca), strontium (Sr) and barium (Ba), and where m, x, y and n in the compositional formula (1) satisfy the relationships of 3<m<5, 0<x<1, 0<y<9 and 0<n<10, and

wherein the ratio of the intensity of a peak existing at a position of the diffraction angle of 36.0° to 36.6° to that at a position of the diffraction angle of 35.0° to 36.0° in an X-ray diffraction pattern is 0.58 or higher.

6. The illumination device according to claim 5 , wherein the alkali earth metal element A includes at least calcium (Ca) and strontium (Sr) and wherein, with a ratio α of the number of atoms of Ca, a ratio β of the number of atoms of Sr and with a ratio γ of another element of the group II, the relationships (m=α+β+γ) and 0≦α/(α+β)≦0.3 are met.

7. A liquid crystal display comprising:

a liquid crystal display panel; and

a backlight obtained using a plurality of white light sources, the backlight illuminating the liquid crystal display panel;

each white light source including a blue light emitting diode provided on a device substrate; and

a kneaded mass arranged on the blue light emitting diode,

wherein the kneaded mass is a mass of a transparent resin obtained on kneading a red phosphor and a green phosphor together,

wherein the red phosphor containing an element A, europium (Eu), silicon (Si), carbon (C), oxygen (O) and nitrogen (N) in ratios of the numbers of atoms of the following compositional formula (1):

[Chemical Formula 5]

[A (m-x) Eu x ][Si (9-y) C y ]O n N [12-2(n-m)/3]    compositional formula (1)

 where the element A is at least one of magnesium (Mg), calcium (Ca), strontium (Sr) and barium (Ba), and where m, x, y and n in the compositional formula (1) satisfy the relationships of 3<m<5, 0<x<1, 0<y<9 and 0<n<10, and

wherein the ratio of the intensity of a peak existing at a position of the diffraction angle of 36.0° to 36.6° to that at a position of the diffraction angle of 35.0° to 36.0° in an X-ray diffraction pattern is 0.58 or higher.

8. The liquid crystal display according to claim 7 , wherein the alkali earth metal element A includes at least calcium (Ca) and strontium (Sr) and wherein, with a ratio α of the number of atoms of Ca, a ratio β of the number of atoms of Sr and with a ratio γ of another element of the group II, the relationships (m=α+β+γ) and 0≦α/(α+β)≦0.3 are met.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 7, 2014
From: IZAWA, TAKAMASA; AKIHO, HIRAKU; KUSUNOKI, TSUNEO; IGARASHI, TAKAHIRO; KANNO, MASAKI
To: DEXERIALS CORPORATION
Reel/Frame 034125/0919 →
Priority Claims (5)
JP 2010-293419 · Dec 28, 2010 · national
JP 2011-000264 · Jan 4, 2011 · national
JP 2011-108873 · May 14, 2011 · national
JP 2011-108874 · May 14, 2011 · national
JP 2011-108876 · May 14, 2011 · national
Continuity (2)
Continuation 13338592 · Dec 28, 2011
Related Publication 20140320787A1 · Oct 30, 2014