IP Library Granted Patent US 9,498,927
Granted Patent B2
US 9,498,927 · App. 13/842,462 · Granted Nov 22, 2016

Decorative foam and method

Inventors: Richard L. Watkins (Portland, OR); Hossein Baghdadi (Portland, OR); Charles Edwards (Portland, OR); Yihua Chang (Portland, OR)
Assignee: NIKE, Inc.
B29D35/122A43B1/0027A43B13/16B29C44/0461B29C44/445C08J9/0004C08J9/122C08J9/18C08J9/232B29C43/003C08J2203/06C08J2203/08C08J2300/22C08J2300/26C08J2375/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,498,927
App. No.
13/842,462
Granted
Nov 22, 2016
Kind
B2
Abstract

Decorative foamed articles are prepared from foamed pellets, beads, particles, or other articles of a thermoplastic elastomer infused with a supercritical fluid in a pressurized container, then rapidly depressurized and heated either by immersion in a heated fluid that can rapidly heat the article or with infrared or microwave radiation to heat and foam the pellets, beads, particles, or other articles that are then molded into the articles. The pellets are dyed with a nonionic or anionic dye one of: (1) before being infused with the supercritical fluid, (2) during being infused with the supercritical fluid by a nonionic or anionic dye dissolved or dispersed in the supercritical fluid, which optionally comprises a polar liquid, (3) during immersion in the heated fluid, where the heated fluid contains the dye, or (4) after being foamed.

Claims (35)

1. A method of foaming an article, comprising

infusing the article with a supercritical fluid, wherein the article is a pellet, bead, or particle comprising a thermoplastic elastomer;

removing the article from the supercritical fluid, and either

(i) immersing the article in a heated fluid or

(ii) irradiating the article with infrared or microwave radiation to foam the article, wherein the article is dyed during at least one of the infusing step and the immersing step, wherein dyeing the article during the infusing step comprises infusing the article with a supercritical fluid that has a dye dispersed or dissolved in the supercritical fluid and wherein dyeing the article during the immersing step comprises providing a heated fluid that contains a dye in solution and immersing the article in the heated fluid such that a dyed, foamed article is made.

2. A method according to claim 1 , wherein the thermoplastic elastomer comprises at least one of a thermoplastic polyurethane elastomer, a thermoplastic polyurea elastomer, a thermoplastic polyamide elastomer, and a thermoplastic polyester elastomer.

3. A method according to claim 2 , wherein, after removing the article from the supercritical fluid, the article is immersed in the heated fluid and the heated fluid comprises water, an anionic dye, and a quaternary (tetraalkyl) ammonium salt selected from soluble tetrabutylammonium compounds and tetrahexylammonium compounds.

4. A method of foaming an article, comprising

infusing the article with a supercritical fluid;

removing the article from the supercritical fluid, and either

(i) immersing the article in a heated fluid or

(ii) irradiating the article with infrared or microwave radiation to foam the article,

wherein the article is dyed during at least one of the infusing step and the immersing step, wherein dyeing the article during the infusing step comprises infusing the article with a supercritical fluid that has a dye dispersed or dissolved in the supercritical fluid and wherein dyeing the article during the immersing step comprises providing a heated fluid that contains a dye in solution and immersing the article in the heated fluid such that a dyed, foamed article is made,

wherein the supercritical fluid comprises an anionic dye or nonionic dye.

5. A method according to claim 4 , wherein the supercritical fluid further comprises a polar liquid.

6. A method according to claim 1 , further comprising molding the dyed, foamed article after it is made.

7. A method of foaming an article, comprising

infusing the article with a supercritical fluid;

removing the article from the supercritical fluid, and either

(i) immersing the article in a heated fluid or

(ii) irradiating the article with infrared or microwave radiation to foam the article,

wherein the article is dyed during at least one of the infusing step and the immersing step, wherein dyeing the article during the infusing step comprises infusing the article with a supercritical fluid that has a dye dispersed or dissolved in the supercritical fluid and wherein dyeing the article during the immersing step comprises providing a heated fluid that contains a dye in solution and immersing the article in the heated fluid such that a dyed, foamed article is made and

molding the dyed, foamed article after it is made

wherein the foamed article is a pellet, bead, or particle and further comprising a step of molding a plurality of the foamed articles together.

8. A method according to claim 7 , wherein the plurality of the foamed articles includes articles of at least two different colors.

9. A method according to claim 8 , wherein the plurality of the foamed articles are coated with an adhesive before being molded together.

10. A method according to claim 8 , wherein the plurality of the foamed articles are molded together in a matrix of unfoamed thermoplastic elastomer.

11. A method according to claim 8 , wherein the plurality of the foamed articles are molded together in a matrix of foamed thermoplastic elastomer.

12. A method according to claim 1 , wherein the supercritical fluid comprises an anionic dye or nonionic dye and further comprises a polar liquid.

13. A method according to claim 4 , wherein the thermoplastic elastomer comprises at least one of a thermoplastic polyurethane elastomer, a thermoplastic polyurea elastomer, a thermoplastic polyamide elastomer, and a thermoplastic polyester elastomer.

14. A method according to claim 4 , wherein, after removing the article from the supercritical fluid, the article is immersed in the heated fluid and the heated fluid comprises water, an anionic dye, and a quaternary (tetraalkyl) ammonium salt selected from soluble tetrabutylammonium compounds and tetrahexylammonium compounds.

15. A method according to claim 4 , further comprising molding the dyed, foamed article after it is made.

16. A method according to claim 7 , wherein the thermoplastic elastomer comprises at least one of a thermoplastic polyurethane elastomer, a thermoplastic polyurea elastomer, a thermoplastic polyamide elastomer, and a thermoplastic polyester elastomer.

17. A method according to claim 7 , wherein, after removing the article from the supercritical fluid, the article is immersed in the heated fluid and the heated fluid comprises water, an anionic dye, and a quaternary (tetraalkyl) ammonium salt selected from soluble tetrabutylammonium compounds and tetrahexylammonium compounds.

18. A method according to claim 7 , wherein the supercritical fluid comprises an anionic dye or nonionic dye and further comprises a polar liquid.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 24, 2013
From: WATKINS, RICHARD L.; BAGHDADI, HOSSEIN; EDWARDS, CHARLES; CHANG, YIHUA
To: NIKE, INC.
Reel/Frame 030869/0152 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 24, 2013
From: NIKE, INC.
To: NIKE INTERNATIONAL LTD.
Reel/Frame 030869/0229 →
Continuity (1)
Related Publication 20140259329A1 · Sep 18, 2014