IP Library Granted Patent US 9,718,229
Granted Patent B2
US 9,718,229 · App. 14/861,257 · Granted Aug 1, 2017

Methods of using retrofitted injection molding machines with reduced temperatures

Inventors: Gene Michael Altonen (West Chester, OH); Michael Thomas Dodd (Walton, KY)
Assignee: IMFLUX INC.
B29C45/77B29C33/3842B29C45/74B29C45/76B29C45/762B29C45/78B29C2045/776B29C2945/76498B29C2945/76501B29C2945/76535B29C2945/76545B29C2945/76561B29C2945/76688B29C2945/76859B29C2945/76936B29C2945/76939B29K2101/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,718,229
App. No.
14/861,257
Granted
Aug 1, 2017
Kind
B2
Abstract

An injection molding machine that uses a mold and a native controller to operate according to an original mold cycle to mold plastic objects is retrofitted with a retrofit controller; the retrofitted machine uses the mold and the retrofit controller to operate according to a retrofit mold cycle to mold plastic objects. When molding according to the retrofit mold cycle, the injection molding machine uses lower temperatures, when compared to molding according to the original mold cycle.

Claims (34)

1. A method of using an injection molding machine, the method comprising:

first, injection molding using a first injection molding machine, a first mold, and a native controller to injection mold production versions of a plastic object according to an original mold cycle for the first mold, the first injection molding machine including an injection unit, a nozzle in fluid communication with the injection unit, and the first mold, which is in fluid communication with the nozzle, wherein the native controller is programmed with at least a portion of the original mold cycle, wherein during the original mold cycle, the first injection molding machine has an average original mold cycle machine temperature profile; and

second, injection molding using a second injection molding machine, a second mold, the native controller, and a retrofit controller to injection mold production versions of the plastic object according to a retrofit mold cycle for the second mold, the second injection molding machine including an injection unit, a nozzle in fluid communication with the injection unit, and the second mold, which is in fluid communication with the nozzle, wherein the retrofit controller is programmed with at least a portion of the retrofit mold cycle, wherein during the retrofit mold cycle the second injection molding machine has an average retrofit mold cycle machine temperature profile, wherein the native controller controls at least one of cooling the plastic object, opening the mold, ejecting the molded object, closing the mold, and recovering the second injection molding machine for a new cycle;

wherein the average retrofit mold cycle machine temperature profile is 5-50° C. less than the average original mold cycle machine temperature profile.

2. The method of claim 1 , wherein:

the first step includes the injection molding of the production versions of the plastic object, which is made from a first plastic material; and

the second step includes the injection molding of the production versions of the plastic object, which is made from a second plastic material that is essentially the same as the first plastic material.

3. The method of claim 2 , wherein the second plastic material is the same as the first plastic material.

4. The method of claim 2 , wherein the second mold has the same configuration as the first mold.

5. The method of claim 2 , wherein the second mold is the first mold.

6. The method of claim 4 , wherein the second injection molding machine has the same configuration as the first injection molding machine.

7. The method of claim 4 , wherein the second injection molding machine is the first injection molding machine.

8. The method of claim 7 , wherein during the retrofit mold cycle the injection molding machine has an average retrofit mold cycle machine temperature profile that is 10-50° C. less than the average original mold cycle machine temperature profile.

9. The method of claim 7 , wherein during the retrofit mold cycle the injection molding machine has an average retrofit mold cycle machine temperature profile that is 20-50° C. less than the average original mold cycle machine temperature profile.

10. The method of claim 7 , wherein during the retrofit mold cycle the injection molding machine has an average retrofit mold cycle machine temperature profile that is 30-50° C. less than the average original mold cycle machine temperature profile.

11. The method of claim 7 , wherein:

during a filling portion of the original mold cycle the injection molding machine has an average original filling portion machine temperature profile; and

during a filling portion of the retrofit mold cycle the injection molding machine has an average retrofit filling portion machine temperature profile that is 5-50° C. less than the average original filling portion machine temperature profile.

12. The method of claim 7 , wherein:

at a beginning of a filling portion of the original mold cycle the injection molding machine has an original beginning filling portion machine temperature profile; and

at a beginning of a filling portion of the retrofit mold cycle the injection molding machine has a retrofit beginning filling portion machine temperature profile that is 5-50° C. less than the original beginning filling portion machine temperature profile.

13. A method of using an injection molding machine, the method comprising:

first, injection molding using an injection molding machine, a mold, and a native controller to injection mold production versions of a plastic object made from a plastic material according to an original mold cycle, the injection molding machine including an injection unit, a nozzle in fluid communication with the injection unit, and the mold, which is in fluid communication with the nozzle, wherein the native controller is programmed with at least a portion of an original mold cycle for the mold, wherein during the original mold cycle the plastic material has an average original mold cycle melt temperature, measured at the nozzle of the first injection molding machine; and

second, injection molding using the injection molding machine, the mold, the native controller, and a retrofit controller to injection mold production versions of the plastic object made from the plastic material according to a retrofit mold cycle, wherein the retrofit controller is programmed with at least a portion of a retrofit mold cycle for the mold, wherein during the retrofit mold cycle the plastic material has an average retrofit mold cycle melt temperature, measured at the nozzle of the second injection molding machine, wherein the native controller controls at least one of cooling the plastic object, opening the mold, ejecting the molded object, closing the mold, and recovering the second injection molding machine for a new cycle;

wherein the average retrofit mold cycle melt temperature is 5-50° C. less than the average original mold cycle melt temperature.

14. The method of claim 13 , wherein the average retrofit mold cycle melt temperature is 10-50° C. less than the average original mold cycle melt temperature.

15. The method of claim 13 , wherein the average retrofit mold cycle melt temperature is 20-50° C. less than the average original mold cycle melt temperature.

16. The method of claim 13 , wherein the average retrofit mold cycle melt temperature is 30-50° C. less than the average original mold cycle melt temperature.

17. The method of claim 13 , wherein:

during a filling portion of the original mold cycle the injection molding machine has an average original filling portion melt temperature; and

during a filling portion of the retrofit mold cycle the injection molding machine has an average retrofit filling portion melt temperature that is 5-50° C. less than the average original filling portion melt temperature.

18. The method of claim 13 , wherein:

at a beginning of a filling portion of the original mold cycle the injection molding machine has an original beginning filling portion melt temperature; and

at a beginning of a filling portion of the retrofit mold cycle the injection molding machine has a retrofit beginning filling portion melt temperature profile that is 5-50° C. less than the original beginning filling portion melt temperature.

Assignments (2)
NUNC PRO TUNC ASSIGNMENT Recorded Jul 29, 2024
From: IMFLUX, INC.
To: THE PROCTER & GAMBLE COMPANY
Reel/Frame 068178/0055 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 24, 2016
From: ALTONEN, GENE MICHAEL; DODD, MICHAEL THOMAS
To: IMFLUX INC
Reel/Frame 039520/0834 →
Continuity (2)
Provisional Application 62053499 · Sep 22, 2014
Related Publication 20160082639A1 · Mar 24, 2016