IP Library Granted Patent US 9,741,933
Granted Patent B2
US 9,741,933 · App. 14/666,642 · Granted Aug 22, 2017

Method for repairing organic EL element, method for manufacturing organic EL panel, and light-emitting device

Inventor: Yoshikazu Sakaguchi (Tokyo, JP)
Assignee: NEC LIGHTING, LTD.
H01L51/0031H01L51/5221H01L2251/564H01L2251/568
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,741,933
App. No.
14/666,642
Granted
Aug 22, 2017
Kind
B2
Abstract

The present invention provides a method for repairing an organic EL element and a method for manufacturing an organic EL panel that can reduce a production cycle time. A method for repairing an organic EL element includes an application step of repeatedly applying a pulse voltage having ON-period and OFF-period to an organic EL element. In the application step, the pulse voltage is a forward voltage or a reverse voltage, and the ON-period is equal to or longer than a time constant that is the product of an element capacity of the organic EL element and a wiring resistance including the element.

Claims (34)

1. A method for repairing an organic electroluminescence (EL) element, comprising:

an application step of repeatedly applying a pulse voltage having an ON-period and an OFF-period to an organic EL element to repair the organic EL element,

wherein in the application step, the pulse voltage is a forward voltage during the ON-period, and a reverse direction bias lower than an absolute value of a breakdown voltage is applied during the OFF-period,

the ON-period is equal to or longer than a time constant that is the product of an element capacity of the organic EL element and a wiring resistance including the element, and

wherein repairing the organic EL element comprises repairing a short circuit between an anode and a cathode of the EL element.

2. The method according to claim 1 , wherein the waveform of the pulse wave is at least one selected from the group consisting of square waves (rectangular waves), reverse sawtooth waves, sawtooth waves (ramp waves), triangle waves, Sine waves (sinusoidal waves), trapezoidal waves, Gaussian pulse waves, and stepped sinusoidal waves.

3. The method according to claim 2 , wherein in the application step, at least one of increase or reduction of the forward voltage to be applied is performed every repetition of voltage application.

4. The method according to claim 2 , wherein in the application step, the forward voltage is repeatedly applied while sweeping from the high-voltage side to the low-voltage side after sweeping from the low-voltage side to the high-voltage side.

5. The method according to claim 1 , wherein in the application step, at least one of increase or reduction of the forward voltage to be applied is performed every repetition of voltage application.

6. A method for manufacturing an organic electroluminescence (EL) panel, comprising:

a formation step of forming an organic EL panel by laminating a first electrode layer, an organic light-emitting layer, and a second electrode layer in this order on a base material; and

a repair step of repairing the organic EL element laminated, wherein the repair step is performed by the method according to claim 1 .

7. The method according to claim 1 , wherein in the application step, the forward voltage is repeatedly applied while sweeping from the high-voltage side to the low-voltage side after sweeping from the low-voltage side to the high-voltage side.

8. A method for repairing an organic electroluminescence (EL) element, comprising:

an application step of repeatedly applying a forward pulse voltage and not applying a reverse direction bias to an organic EL element to repair the organic EL element,

wherein the pulse voltage is within a range of ±1.5V at most from ½ potential of a threshold voltage, while sweeping from a low-voltage side to a high-voltage side, and

wherein repairing the organic EL element comprises repairing a short circuit between an anode and a cathode of the EL element.

9. The method according to claim 8 , wherein in the application step, the forward voltage is repeatedly applied while sweeping from the high-voltage side to the low-voltage side after sweeping from the low-voltage side to the high-voltage side.

10. The method according to claim 9 , wherein in the application step, each repetition cycle includes an OFF-period.

11. A method for manufacturing an organic electroluminescence (EL) panel, comprising:

a formation step of forming an organic EL panel by laminating a first electrode layer, an organic light-emitting layer, and a second electrode layer in this order on a base material; and

a repair step of repairing the organic EL element laminated, wherein the repair step is performed by the method according to claim 9 .

12. The method according to claim 8 , wherein in the application step, each repetition cycle includes an OFF-period.

13. A method for manufacturing an organic electroluminescence (EL) panel, comprising:

a formation step of forming an organic EL panel by laminating a first electrode layer, an organic light-emitting layer, and a second electrode layer in this order on a base material, and

a repair step of repairing the organic EL element laminated, wherein the repair step is performed by the method according to claim 8 .

14. A method for repairing an organic electroluminescence (EL) element, comprising:

an application step of repeatedly applying a pulse voltage having an ON-period and an OFF-period to an organic EL element to repair the organic EL element,

wherein in the application step, the pulse voltage is a forward voltage, and a reverse direction bias is not applied,

the ON-period is equal to or longer than a time constant that is the product of an element capacity of the organic EL element and a wiring resistance including the element, and

wherein repairing the organic EL element comprises repairing a short circuit between an anode and a cathode of the EL element.

15. The method according to claim 14 , wherein the waveform of the pulse wave is at least one selected from the group consisting of square waves (rectangular waves), reverse sawtooth waves, sawtooth waves (ramp waves), triangle waves, Sine waves (sinusoidal waves), trapezoidal waves, Gaussian pulse waves, and stepped sinusoidal waves.

16. The method according to claim 14 , wherein in the application step, the forward voltage is repeatedly applied within a range of ±1.5V at most from ½ potential of a threshold voltage, while sweeping from a low-voltage side to a high-voltage side.

17. The method according to claim 15 , wherein in the application step, the forward voltage is repeatedly applied within a range of ±1.5V at most from ½ potential of a threshold voltage, while sweeping from a low-voltage side to a high-voltage side.

Assignments (4)
CHANGE OF ADDRESS Recorded Jan 23, 2024
From: HOTALUX, LTD.
To: HOTALUX, LTD.
Reel/Frame 066365/0200 →
CORRECTIVE ASSIGNMENT TO CORRECT THE ASSIGNEE ADDRESS PREVIOUSLY RECORDED AT REEL: 050850 FRAME: 0287. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT. Recorded Nov 6, 2019
From: HOTALUX, LTD.
To: HOTALUX, LTD.
Reel/Frame 050942/0429 →
CHANGE OF NAME Recorded Oct 29, 2019
From: NEC LIGHTING, LTD.
To: HOTALUX, LTD.
Reel/Frame 050850/0287 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 24, 2015
From: SAKAGUCHI, YOSHIKAZU
To: NEC LIGHTING, LTD.
Reel/Frame 035239/0597 →
Priority Claims (1)
JP 2014-070206 · Mar 28, 2014 · national
Continuity (1)
Related Publication 20150280174A1 · Oct 1, 2015