IP Library Granted Patent US 9,745,510
Granted Patent B2
US 9,745,510 · App. 14/683,046 · Granted Aug 29, 2017

Fluoride fluorescent material and method for producing the same

Inventors: Sadakazu Wakui (Tokushima, JP); Shoji Hosokawa (Tokushima, JP)
Assignee: NICHIA CORPORATION
C09K11/617C09K11/616H01L33/502H01L2224/48247H01L2224/48257H01L2224/73265
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,745,510
App. No.
14/683,046
Granted
Aug 29, 2017
Kind
B2
Abstract

A method for producing a fluoride fluorescent material includes: subjecting a mixture that contains a fluoride compound in a liquid medium to a pressurization treatment and a heating treatment, the fluoride compound having a chemical composition represented by the following formula: A 2 [M 1−a Mn 4+ a F 6 ]. A is at least one cation selected from the group consisting of K + , Li + , Na + , Rb + , Cs + and NH 4 + , M is at least one element selected from the group consisting of Group 4 elements and Group 14 elements, and a is a number that satisfies 0 <a <0.2. The pressurization treatment is performed at a pressure of 1.5 MPa or higher.

Claims (10)

1. A method for producing a fluoride fluorescent material, comprising:

subjecting a mixture that contains a fluoride compound in a liquid medium to a pressurization treatment and a heating treatment, the fluoride compound having a chemical composition represented by the following formula (I):

A 2 [M 1−a Mn 4+ a F 6 ]  (I)

wherein A is at least one cation selected from the group consisting of K + , Li + , Na + , Rb + , Cs + and NH 4 + , M is at least one element selected from the group consisting of Group 4 elements and Group 14 elements, and a is a number that satisfies 0<a<0.2, and

wherein the pressurization treatment is performed at a pressure of 1.5 MPa or higher.

2. The method according to claim 1 , wherein the heating treatment is performed at a temperature of 100° C. or higher.

3. The method according to claim 1 , wherein the liquid medium is an aqueous medium.

4. The method according to claim 1 , wherein the liquid medium contains potassium.

5. The method according to claim 1 , wherein an amount of a liquid medium used in the pressurization treatment is in a range of 100 to 160 parts by mass based on 100 parts by mass of the fluoride compound.

6. The method according to claim 1 , wherein an amount of a liquid medium used in the pressurization treatment is in a range of 130 to 160 parts by mass based on 100 parts by mass of the fluoride compound.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 9, 2015
From: WAKUI, SADAKAZU; HOSOKAWA, SHOJI
To: NICHIA CORPORATION
Reel/Frame 035374/0684 →
Priority Claims (1)
JP 2014-080656 · Apr 10, 2014 · national
Continuity (1)
Related Publication 20150291878A1 · Oct 15, 2015