IP Library Granted Patent US 9,808,971
Granted Patent B2
US 9,808,971 · App. 14/960,115 · Granted Nov 7, 2017

Nozzle shut off for injection molding system

Inventor: Richard Ernest Fitzpatrick (Loveland, CO)
Assignee: EXTRUDE TO FILL, LLC
B29C45/13B29C45/03B29C45/18B29C45/23B29C45/40B29C45/47B29C45/60B29C45/73B29C45/74B29C45/76B29C45/77B29C45/78G05B19/042H02K7/14B29C45/5092B29C2045/1792B29C2045/1875B29C2945/76006B29C2945/76257B29C2945/76381B29C2945/76498B29C2945/76665B29C2945/76859B29K2005/00B29K2105/26B29K2995/0008G05B2219/2624
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,808,971
App. No.
14/960,115
Granted
Nov 7, 2017
Kind
B2
Abstract

An injection molding apparatus and method of fabricating a molded part are provided. The apparatus may include a barrel, a nozzle enclosing an end of the barrel and defining an opening in fluid communication with an inside of the barrel, and an extrusion screw positioned at least partially inside the barrel and rotatable relative to the barrel. The extrusion screw may include a screw tip. Relative axial movement between the barrel and the extrusion screw may open or close the opening of the nozzle to permit or prevent, respectively, material flow through the opening of the nozzle. The method may include clamping a mold, opening a nozzle, rotating the extrusion screw to pump a molten material into the mold until the mold is filled, closing the nozzle, and unclamping the mold to release a molded part.

Claims (81)

1. A method of fabricating a molded part, the method comprising:

clamping a mold;

opening a nozzle by separating a tip of an extrusion screw from an opening formed in the nozzle;

rotating the extrusion screw to pump a molten material into the mold until the mold is filled;

closing the nozzle by positioning the tip of the extrusion screw in sealed engagement with the nozzle; and

unclamping the mold to release the molded part;

wherein:

opening the nozzle comprises rotating the extrusion screw to move the screw tip away from the nozzle; and

closing the nozzle comprises reversing rotation of the extrusion screw to move the screw tip into contact with the nozzle.

2. The method of claim 1 , further comprising heating a material in a barrel to form the molten material prior to opening the nozzle.

3. The method of claim 2 , further comprising:

filling a hopper with the material in a form of pellets or flakes; and

cooling the hopper prior to heating the material in the barrel.

4. The method of claim 1 , further comprising cooling the mold to solidify the molten material in the mold.

5. The method of claim 1 , wherein an injection pressure in a barrel filled with the molten material is substantially the same as or up to 10% higher than the pressure in a mold cavity defined by the mold.

6. The method of claim 1 , wherein the material is selected from a group consisting of amorphous thermoplastics, crystalline and semi-crystalline thermoplastics, virgin resins, fiber reinforced plastics, recycled thermoplastics, post-industrial recycled resins, post-consumer recycled resins, mixed and comingled thermoplastic resins, organic resins, organic food compounds, carbohydrate based resins, sugar-based compounds, gelatin, propylene glycol compounds, starch based compounds, and metal injection molding (MIM) feedstocks.

7. A method of fabricating a molded part, the method comprising:

clamping a mold;

opening a nozzle by separating a tip of an extrusion screw from an opening formed in the nozzle;

rotating the extrusion screw to pump a molten material into the mold until the mold is filled;

closing the nozzle by positioning the tip of the extrusion screw in sealed engagement with the nozzle; and

unclamping the mold to release the molded part;

wherein:

opening the nozzle comprises moving a barrel in a first direction relative to an extrusion screw to move a nozzle attached to the barrel away from a tip of the extrusion screw; and

closing the nozzle comprises moving the barrel in a second direction opposite the first direction relative to the extrusion screw to move the nozzle into engagement with the screw tip.

8. A method of fabricating a plastic component by an apparatus comprising a hopper, an extrusion screw with a screw tip, a nozzle, one or more heaters, and a motor, the method comprising:

clamping a mold;

activating the motor to rotate the extrusion screw to move the screw tip away from the nozzle to open the nozzle;

rotating the extrusion screw to pump a molten material into the mold until the mold is filled;

reversing rotation of the extrusion screw to move the screw tip to close the nozzle;

cooling the mold to solidify the molten material in the mold; and

unclamping the mold to release a molded part.

9. The method of claim 8 , further comprising:

moving the extrusion screw to place the nozzle against a gate of the mold; and

turning on the one or more heaters to melt material filled in a barrel from the hopper prior to clamping.

10. The method of claim 8 , further comprising:

filling a hopper with a material in a form of pellets or flakes; and

cooling the hopper prior to turning on the one or more heaters.

11. The method of claim 8 , wherein clamping the mold comprises applying an air pressure ranging from 90 psi to 110 psi.

12. The method of claim 11 , wherein unclamping the mold comprises releasing the air pressure.

13. The method of claim 8 , wherein the screw tip is spaced away from the nozzle when the nozzle is open.

14. The method of claim 8 , wherein the molten material is under a pressure that is the same as or up to 10% higher than a pressure in the mold.

15. The method of claim 8 , wherein the material is selected from a group consisting of amorphous thermoplastics, crystalline and semi-crystalline thermoplastics, virgin resins, fiber reinforced plastics, recycled thermoplastics, post-industrial recycled resins, post-consumer recycled resins, mixed and comingled thermoplastic resins, organic resins, organic food compounds, carbohydrate based resins, sugar-based compounds, gelatin, propylene glycol compounds, starch based compounds, and metal injection molding (MIM) feedstocks.

16. An injection molding apparatus comprising:

a barrel;

a nozzle enclosing an end of the barrel and defining an opening in fluid communication with an inside of the barrel; and

an extrusion screw positioned at least partially inside the barrel and rotatable relative to the barrel, the extrusion screw including a screw tip configured to prevent formation of a cold slug in the opening of the nozzle;

wherein relative axial movement between the barrel and the extrusion screw opens or closes the opening of the nozzle to permit or prevent, respectively, material flow through the opening of the nozzle; and

wherein the screw tip comprises:

a cylindrical tip portion configured to extend to an exterior surface of the nozzle and seal the opening of the nozzle; and

an angled portion extending rearwardly and outwardly from the cylindrical tip portion, the angled portion configured to form a seal with a portion of the nozzle surrounding the opening.

17. The apparatus of claim 16 , wherein the screw tip and the extrusion screw are formed as a single part.

18. The apparatus of claim 16 , wherein the screw tip is formed separately from the extrusion screw and is attached to an end of the extrusion screw.

19. The apparatus of claim 16 , wherein the nozzle is attached to the barrel.

20. The apparatus of claim 16 , wherein the barrel is moveable along an axial direction between a first position in which the screw tip closes the opening of the nozzle and a second position in which the screw tip is spaced apart from the opening of the nozzle.

21. The apparatus of claim 16 , wherein the nozzle abuts against the end of the barrel.

22. The apparatus of claim 16 , wherein the extrusion screw is moveable along an axial direction between a first position in which the screw tip closes the opening of the nozzle and a second position in which the screw tip is spaced apart from the opening of the nozzle.

23. The apparatus of claim 16 , wherein:

the cylindrical tip portion is shaped to match the geometry of the opening of the nozzle; and

the angled portion is shaped to match the geometry of the portion of the nozzle surrounding the opening.

24. The apparatus of claim 16 , wherein a leading surface of the cylindrical tip portion is configured to be flush with the exterior surface of the nozzle when the opening of the nozzle is closed.

25. The apparatus of claim 16 , wherein the cylindrical tip portion has a smaller axial length than the angled portion.

26. An apparatus comprising:

an extrusion screw inside a barrel;

a hopper coupled to the barrel and configured to fill a material into the barrel;

one or more heaters configured to heat the material inside the barrel;

a nozzle having a tip portion configured to enclose the screw tip, a barrel connection configured to connect to the barrel, and a middle portion between the tip portion and the barrel connection, the tip portion of the nozzle having an opening for injecting the material; and

a screw tip coupled to the extrusion screw, the screw tip configured to fit inside the tip portion of the nozzle and displace the material from the opening in the tip portion of the nozzle to prevent formation of a cold slug in the opening, the screw tip configured to move along an axial direction to open and close the opening;

wherein the screw tip comprises:

a cylindrical tip portion configured to extend to an exterior surface of the tip portion of the nozzle and seal the opening in the tip portion of the nozzle; and

an angled portion extending rearwardly and outwardly from the cylindrical tip portion, the angled portion configured to form a seal with the middle portion of the nozzle.

27. The apparatus of claim 26 , wherein the angled portion transitions from a larger diameter of the extrusion screw to the opening in the tip portion of the nozzle.

28. The apparatus claim 27 , wherein the angled portion has an angle from the axial direction between 15° and 45°.

29. The apparatus of claim 26 , wherein the opening in the tip portion of the nozzle is proportional to the diameter of the extrusion screw to allow easy flow of the material into a mold cavity.

30. The apparatus of claim 26 , wherein the barrel connection of the nozzle comprises threads configured to attach to threads of the barrel near an end of the barrel.

31. The apparatus of claim 26 , wherein the screw tip comprises threads configured to attach to threads of the extrusion screw near an end of the screw.

32. The apparatus of claim 26 , wherein:

the cylindrical tip portion is shaped to match the geometry of the tip portion of the nozzle; and

the angled portion is shaped to match the geometry of the middle portion of the nozzle.

33. The apparatus of claim 26 , wherein a leading surface of the cylindrical tip portion is configured to be flush with the exterior surface of the nozzle when the opening in the tip portion of the nozzle is closed.

34. The apparatus of claim 26 , wherein the cylindrical tip portion has a smaller axial length than the angled portion.

Assignments (2)
CHANGE OF NAME Recorded Aug 25, 2020
From: EXTRUDE TO FILL, LLC
To: EXTRUDE TO FILL, INC.
Reel/Frame 053599/0045 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 17, 2017
From: FITZPATRICK, RICHARD ERNEST
To: EXTRUDE TO FILL, LLC
Reel/Frame 042415/0372 →
Continuity (4)
Provisional Application 62087414 · Dec 4, 2014
Provisional Application 62087449 · Dec 4, 2014
Provisional Application 62087480 · Dec 4, 2014
Related Publication 20160158981A1 · Jun 9, 2016