IP Library Granted Patent US 10,138,787
Granted Patent B2
US 10,138,787 · App. 14/652,875 · Granted Nov 27, 2018

Treatment device equipped with catalyst-supporting honeycomb structure, and method for producing same

Inventors: Seigo Yamamoto (Osaka, JP); Susumu Hikazudani (Osaka, JP); Naoe Hino (Osaka, JP); Fumiya Tubo (Osaka, JP); Tetsuo Kodama (Osaka, JP); Shunsuke Hiraiwa (Osaka, JP); Ryoichi Koumaru (Osaka, JP)
Assignee: Hitachi Zosen Corporation
F01N3/28B01D46/2418B01D53/885B01J23/22B01J35/04B01J37/0234C04B38/0006F01N3/2066C04B2111/0081F01N2310/02F01N2330/101Y02T10/24Y10T29/49346
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,138,787
App. No.
14/652,875
Granted
Nov 27, 2018
Kind
B2
Abstract

To provide a treatment device equipped with a catalyst-supporting honeycomb structure, the device being for use in, for example, an exhaust gas purification treatment, hydrogen production by ammonia decomposition or the like, and a method for producing the same. The catalyst-supporting honeycomb structure is produced by forming the inorganic binder-containing functional catalyst-supporting corrugated glass paper without removing an organic binder originally contained in the glass paper and by using the corrugated glass paper in combination with the inorganic binder-containing functional catalyst-supporting flat glass paper. In the treatment device equipped with a catalyst-supporting honeycomb structure, a corrugated glass paper having an inorganic binder-containing functional catalyst supported thereon and a flat glass paper having the same inorganic binder-containing functional catalyst supported thereon are alternately stacked to form the catalyst-supporting honeycomb structure, and this catalyst-supporting honeycomb structure is packed in a casing.

Claims (15)

1. A method for producing a treatment device equipped with a catalyst-supporting honeycomb structure, which is characterized in that the method comprises the steps of:

applying a functional catalyst-containing slurry having an inorganic binder mixed therein on a flat glass paper;

placing and heating the slurry-applied flat glass paper on a corrugation mold of a high temperature, while shaping the glass paper with a presser jig and removing moisture in the slurry on the surface of the glass paper to dry the glass paper, thereby forming an inorganic binder-containing functional catalyst-supporting corrugated glass paper;

releasing the inorganic binder-containing functional catalyst-supporting corrugated glass paper from the corrugation mold while holding the shape;

meanwhile, placing and heating the slurry-applied flat glass paper on a flat mold of a high temperature to remove moisture in the slurry on the surface of the glass paper and dry the glass paper, thereby forming an inorganic binder-containing functional catalyst-supporting flat glass paper;

releasing the inorganic binder-containing functional catalyst-supporting flat glass paper from the flat mold while holding the shape; and

alternately stacking the inorganic binder-containing functional catalyst-supporting corrugated glass paper and the inorganic binder-containing functional catalyst-supporting flat glass paper and packing the stack in a casing.

2. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 1 , which is characterized in that the surface temperatures of the corrugation mold and the flat mold are within the range of from 200 to 500° C.

3. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 2 , which is characterized in that the inorganic binder contains at least one inorganic oxide selected from the group consisting of a silica sol, an alumina sol, a γ-alumina, a titanium oxide sol, and a zirconia sol.

4. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 2 , which is characterized in that the method comprises the step of: further baking the inorganic binder-containing functional catalyst-supporting corrugated glass paper and the inorganic binder-containing functional catalyst-supporting flat glass paper released from the respective molds to thermally decompose and remove an organic binder originally contained in the glass papers, while holding the shapes of the glass papers by the inorganic binder, to thereby form an inorganic binder-containing functional catalyst-supporting corrugated glass paper and an inorganic binder-containing functional catalyst-supporting flat glass paper.

5. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 2 , which is characterized in that, in the step of packing in the casing, the inorganic binder-containing functional catalyst-supporting corrugated glass paper and the inorganic binder-containing functional catalyst-supporting flat glass paper are alternately stacked without being bonded to each other.

6. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 1 , which is characterized in that the inorganic binder contains at least one inorganic oxide selected from the group consisting of a silica sol, an alumina sol, a γ-alumina, a titanium oxide sol, and a zirconia sol.

7. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 6 , which is characterized in that the method comprises the step of: further baking the inorganic binder-containing functional catalyst-supporting corrugated glass paper and the inorganic binder-containing functional catalyst-supporting flat glass paper released from the respective molds to thermally decompose and remove an organic binder originally contained in the glass papers, while holding the shapes of the glass papers by the inorganic binder, to thereby form an inorganic binder-containing functional catalyst-supporting corrugated glass paper and an inorganic binder-containing functional catalyst-supporting flat glass paper.

8. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 1 , which is characterized in that the method comprises the step of: further baking the inorganic binder-containing functional catalyst-supporting corrugated glass paper and the inorganic binder-containing functional catalyst-supporting flat glass paper released from the respective molds to thermally decompose and remove an organic binder originally contained in the glass papers, while holding the shapes of the glass papers by the inorganic binder, to thereby form an inorganic binder-containing functional catalyst-supporting corrugated glass paper and an inorganic binder-containing functional catalyst-supporting flat glass paper.

9. The method for producing a treatment device equipped with a catalyst-supporting honeycomb structure according to claim 1 , which is characterized in that, in the step of packing in the casing, the inorganic binder-containing functional catalyst-supporting corrugated glass paper and the inorganic binder-containing functional catalyst-supporting flat glass paper are alternately stacked without being bonded to each other.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 6, 2016
From: YAMAMOTO, SEIGO; HIKAZUDANI, SUSUMU; HINO, NAOE; TUBO, FUMIYA; KODAMA, TETSUO; HIRAIWA, SHUNSUKE; KOUMARU, RYOICHI
To: HITACHI ZOSEN CORPORATION
Reel/Frame 039642/0352 →
Priority Claims (1)
JP 2012-274299 · Dec 17, 2012 · national
Continuity (1)
Related Publication 20150330280A1 · Nov 19, 2015