Warp stretch fabric and method
A warp-directional stretch fabric that defines two right faces and is formed from warp yarns defined by a nylon and fill yarns defined by an aramid. The fabric can be incorporated into a toothed belt, for example a transmission belt, to produce a belt that has enhanced structural and resistance capabilities while capable of being produced at a lower cost than prior art belts. A method of producing an improved toothed belt including the fabric is also provided.
1. A method of producing a toothed belt comprising the steps of: providing a rubber core material, warp yams defined by a nylon material, and fill yams defined by a aramid material,
molding the rubber core material into a circular belt with at least one exterior surface,
weaving the warp yams and the fill yams into a double-faced fabric, whereby the double-faced fabric exhibits more than forty-five percent (45%) elongation in the warp direction and less than twenty-five percent (25%) elongation in the fill direction, attaching the double-faced fabric to the circular belt exterior surface, and molding the circular belt to define a plurality of teeth;
whereby weaving the warp and fill yarns further comprises weaving the double-faced fabric via a four harness satin weave in a broken twill pattern.
2. The method of claim 1 whereby the nylon material is nylon 6, 6.
3. The method of claim 1 whereby the aramid material is meta-aramid.
4. The method of claim 1 whereby the aramid material is para-aramid.