Toner, and external additive for toner

Inventors: Sho Kimura (Kashiwa, JP); Shuhei Moribe (Mishima, JP); Takashi Matsui (Mishima, JP); Hiroyuki Tomono (Numazu, JP); Shotaro Nomura (Suntou-gun, JP); Atsuhiko Ohmori (Yokohama, JP); Takuya Mizuguchi (Suntou-gun, JP); Tatsuya Saeki (Suntou-gun, JP); Katsuhisa Yamazaki (Numazu, JP)
Assignee: Canon Kabushiki Kaisha
G03G9/0825G03G9/0833G03G9/08755
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,241,430
App. No.
15/969,192
Granted
Mar 26, 2019
Kind
B2
Abstract

A toner comprising: a toner particle containing a binder resin and a colorant; and an external additive, wherein the external additive is a composite particle having an organic substance and an organosilicon polymer coating layer on the surface of the organic substance, and when a curve for the variation (dE′/dT) in the storage elastic modulus E′ of the toner with respect to temperature T [° C.] is obtained on the basis of a curve of the temperature T—the storage elastic modulus E′ [Pa] of the toner, as determined by powder dynamic viscoelasticity measurements of the toner, the relative minimum value on the lowest temperature side between the onset temperature and 90° C. is −1.35×10 8 or less.

Claims (11)

1. A toner comprising:

a toner particle containing a binder resin and a colorant; and

an external additive, wherein

the external additive is a core-shell type composite particle having:

a core containing a crystalline polyester resin; and

an organosilicon polymer-containing coating layer on the surface of the core,

a softening point of the toner particle is from 90° C. to 180° C., and

a softening point (Tm) of the crystalline polyester resin is from 50° C. to 105° C.

2. The toner according to claim 1 , wherein an acid value of the crystalline polyester resin is from 4 mg KOH/g to 20 mg KOH/g.

3. The toner according to claim 1 , wherein the crystalline polyester resin has a urethane bond.

4. The toner according to claim 1 , wherein a weight average molecular weight Mw of the crystalline polyester resin is 18,000 or more.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 26, 2018
From: KIMURA, SHO; MORIBE, SHUHEI; MATSUI, TAKASHI; TOMONO, HIROYUKI; NOMURA, SHOTARO; OHMORI, ATSUHIKO; MIZUGUCHI, TAKUYA; SAEKI, TATSUYA; YAMAZAKI, KATSUHISA
To: CANON KABUSHIKI KAISHA
Reel/Frame 047850/0872 →
Priority Claims (2)
JP 2017-094209 · May 10, 2017 · national
JP 2018-082313 · Apr 23, 2018 · national
Continuity (1)
Related Publication 20180329323A1 · Nov 15, 2018
Cited By (17)
US 12,197,170 US 12,228,882 US 12,242,226 US 12,259,682 US 12,271,150 US 12,306,581 US 12,405,545 US 12,429,789 US 12,429,790 US 12,474,649 US 12,504,700 US 12,529,971 US 12,535,748 US 12,535,750 US 12,578,664 US 12,645,162 US 12,681,399