IP Library Granted Patent US 11,145,867
Granted Patent B2
US 11,145,867 · App. 16/654,723 · Granted Oct 12, 2021

Surface treated copper foil

Inventors: Chien-Ming Lai (Taipei, TW); Yao-Sheng Lai (Taipei, TW); Jui-Chang Chou (Taipei, TW)
Assignee: CHANG CHUN PETROCHEMICAL CO., LTD.
H01M4/661B32B15/01B32B15/08B32B15/20C25D1/04C25D3/04C25D3/12C25D3/22C25D3/38C25D5/10C25D5/14C25D5/16C25D5/48H01M4/0469H01M4/70H01M10/0525H05K1/0242H05K1/09H05K1/18H05K1/181H05K3/384H05K3/389B32B2255/06B32B2255/205B32B2255/28B32B2307/202B32B2457/08H01M2004/027H05K2201/0338H05K2201/0355H05K2201/0373H05K2201/10522H05K2201/2054H05K2203/0307Y10T428/12431
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,145,867
App. No.
16/654,723
Granted
Oct 12, 2021
Kind
B2
Abstract

Surface-treated copper foils exhibiting a void volume (Vv) in a range of 0.4 to 2.2 μm 3 /μm 2 and an arithmetic mean waviness (Wa) lower than or equal to 0.4 μm are reported. Where the surface-treated copper foil is treated on the drum side and includes a treatment layer comprising a nodule layer. Such surface-treated copper foils can be used as a conductive material having low transmission loss, for example in circuit boards.

Claims (28)

1. A surface-treated copper foil comprising:

an electrodeposited copper foil including a drum side and a deposited side, and

a treatment layer disposed on the drum side providing a surface-treated side,

wherein the treatment layer comprises a nodule layer and wherein the surface-treated side exhibits a void volume (Vv) in a range of 0.4 to 2.2 μm 3 /μm 2 and an arithmetic mean waviness (Wa) lower than or equal to 0.4 μm.

2. The surface-treated copper foil of claim 1 , wherein the surface-treated side exhibits an arithmetic mean waviness (Wa) in a range of 0.1 to 0.4 μm.

3. The surface-treated copper foil of claim 1 , wherein the surface-treated side exhibits a core void volume (Vvc) in a range of 0.4 to 2 μm 3 /μm 2 .

4. The surface-treated copper foil of claim 1 , wherein the surface-treated side exhibits a dale void volume (Vvv) in a range of 0.01 to 0.1 μm 3 /μm 2 .

5. The surface-treated copper foil of claim 1 , wherein the surface-treated side exhibits a reflectance at 700 nm in a range of 28% to 76%.

6. The surface-treated copper foil of claim 1 , wherein the surface-treated side exhibits a reflectance at 700 nm greater than 40%.

7. The surface-treated copper foil of claim 6 , wherein the surface-treated side exhibits a reflectance at 700 nm in a range of 40% to 70%.

8. The surface-treated copper foil of claim 1 , wherein the treatment layer further comprises at least one of a barrier layer, an anti-tarnish layer, and a coupling layer.

9. The surface-treated copper foil of claim 8 , wherein the barrier layer is made of metal or an alloy containing the metal, and the metal is selected from at least one of Ni, Zn, Cr, Co, Mo, Fe, Sn, and V.

10. The surface-treated copper foil of claim 8 , wherein the coupling layer includes silicon.

11. The surface-treated copper foil of claim 1 , wherein the nodule layer comprises copper nodules.

12. A device comprising,

a circuit board including the surface-treated copper foil of claim 1 and a plurality of components mounted on the circuit board,

wherein at least a first component and a second component of the plurality of components are electrically connected to each other through the surface-treated copper foil of the circuit board.

13. A laminate comprising,

a resin layer, and

a surface-treated copper foil comprising,

an electrodeposited copper foil including a drum side and a deposited side,

a treatment layer disposed on the drum side providing a surface-treated side in contact with the resin layer, and wherein the treatment layer comprises a nodule layer,

wherein the surface-treated side exhibits a void volume (Vv) in a range of 0.4 to 2.2 μm 3 /μm 2 , an arithmetic mean waviness (Wa) in a range of 0.1 to 0.4 μm, a core void volume (Vvc) in a range of 0.4 to 2 μm 3 /μm 2 , and a dale void volume (Vvv) in a range of 0.01 to 0.1 μm 3 /μm 2 , and a surface reflectance at 700 nm in a range of 40% to 70%.

14. A surface-treated copper foil comprising:

an electrodeposited copper foil including a drum side and a deposited side, and

a treatment layer disposed on the drum side providing a surface-treated side,

wherein the treatment layer comprises a nodule layer and wherein the surface-treated side exhibits a void volume (Vv) in a range of 0.4 to 2.2 μm 3 /μm 2 and an arithmetic mean waviness (Wa) lower than or equal to 0.4 μm,

wherein the nodule layer comprises copper nodules, and the treatment layer further comprises at least one of a barrier layer, an anti-tarnish layer, and a coupling layer.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 16, 2019
From: LAI, CHIEN-MING; LAI, YAO-SHENG; CHOU, JUI-CHANG
To: CHANG CHUN PETROCHEMICAL CO., LTD.
Reel/Frame 050736/0893 →
Continuity (2)
Provisional Application 62800263 · Feb 1, 2019
Related Publication 20200248330A1 · Aug 6, 2020