Processing post-industrial and post-consumer waste streams and preparation of post-industrial and post-consumer products therefrom
A system for and method of, processing post-consumer and post-industrial waste streams, producing active ingredients for waste stream processing, processing aqueous waste streams, preparing and collecting a multi-purpose chemical precursor, removing phosphates, nitrates, heavy metals, and other contaminants from aqueous waste streams, collecting and processing a post-consumer and post-industrial product from aqueous waste streams, administering and positioning assets and processes associated with waste stream processing, and scheduling operations for sub-systems of the system.
1. A method of producing a composite ash from paper and/or carpet exothermic processing waste, the composite ash reactive with a pH greater than about 7.0, the method comprising the steps of:
a) receiving a paper or carpet exothermic processing waste stream;
b) adding a mineral product to the exothermic processing waste stream as a catalyst and thermally processing the paper or carpet exothermic processing waste stream, for a period of about 30.0 minutes to about 12.0 hours, at an average process bed temperature of about 600 to about 1000 degrees C., to remove organics, for yielding the composite ash, of common crystalline and amorphous non-crystalline composition, the composite ash comprising metakaolin and at least one of a group consisting of mineral oxide and mineral carbonate, wherein the mineral product is yielded from a previously-run thermal processing of a paper or carpet exothermic processing waste stream and the mineral product is essentially the same as the composite ash; and
c) recovering and collecting the composite ash.
2. The method of producing the composite ash of claim 1 , wherein receiving the paper or carpet exothermic processing waste stream comprises at least one of a group of steps consisting of dewatering the paper or carpet exothermic processing waste stream, de-lumping the paper or carpet exothermic processing waste stream, and comminuting the paper or carpet exothermic processing waste stream.
3. The method of producing the composite ash of claim 1 , wherein thermally processing the paper or carpet exothermic processing waste stream comprises removing organics without essentially decomposing calcium carbonate present in the composite ash.
4. The method of producing the composite ash of claim 1 , wherein thermally processing the paper or carpet exothermic processing waste stream comprises allowing combustion gases to flow in co-current direction with any of the composite ash produced.
5. The method of producing the composite ash of claim 1 , wherein thermally processing the paper or carpet exothermic processing waste stream comprises recovering energy to recycle for use anywhere in the method of producing the composite ash.
6. The method of producing the composite ash of claim 1 , wherein thermally processing the paper or carpet exothermic processing waste stream comprises thermally processing, for a period of about 30.0 minutes to about 2.0 hours, at an average process bed temperature in the range of about 600 to about to 825 degrees C.
7. The method of producing the composite ash of claim 1 , wherein thermally processing the paper or carpet exothermic processing waste stream comprises thermally processing, for a period of about 30.0 minutes to about 1.0 hours, at an average process bed temperature in the range of about 600 to about to 800 degrees C.