IP Library Granted Patent US 11,890,780
Granted Patent B2
US 11,890,780 · App. 16/909,847 · Granted Feb 6, 2024

Additive manufacturing method and device for ceramic and composite thereof

Inventors: Hai'ou Zhang (Wuhan, CN); Xiaoqi Hu (Wuhan, CN); Guilan Wang (Wuhan, CN); Cheng Yang (Wuhan, CN)
Assignee: Huazhong University of Science & Technology
B28B11/089B22F10/25B22F10/50B22F10/66B22F12/17B22F12/53B22F12/90B28B1/001B28B11/0872B33Y10/00B33Y30/00C22F1/04B22F10/36
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,890,780
App. No.
16/909,847
Granted
Feb 6, 2024
Kind
B2
Abstract

Additive manufacturing (AM) methods and devices for high-melting-point materials are disclosed. In an embodiment, an additive manufacturing method includes the following steps. (S1) Slicing a three-dimensional computer-aided design model of a workpiece into multiple layers according to shape, thickness, and size accuracy requirements, and obtaining data of the multiple layers. (S2) Planning a forming path according to the data of the multiple layers and generating computer numerical control (CNC) codes for forming the multiple layers. (S3) Obtaining a formed part by preheating a substrate, performing a layer-by-layer spraying deposition by a cold spraying method, and heating a spray area to a temperature until the spraying deposition of all sliced layers is completed. (S4) Subjecting the formed part to a surface modification treatment by a laser shock peening method.

Claims (39)

1. An additive manufacturing method implemented by a gantry machine tool, comprising the steps of:

(S1) slicing a three-dimensional computer-aided design model of a workpiece into multiple layers according to a shape requirement, a thickness requirement, and a surface accuracy requirement, and obtaining data of the multiple layers, wherein the obtained data comprise thickness data, shape data, and surface accuracy data of each slice layer and a melting point of a material;

(S2) planning a forming path according to the data of the multiple layers, and generating computer numerical control codes for forming the multiple layers;

(S3) obtaining a formed part by:

preheating a substrate;

performing, by a spraying deposition module comprising a cold spraying gun, a layer-by-layer spraying deposition of the material as a sprayed powder by cold spray according to the computer numerical control codes in step (S2); and

heating a spray area to a temperature until the spraying deposition of all slice layers is completed, wherein the temperature is in a range of the melting point of the sprayed powder minus 200° C. to the melting point of the sprayed powder; and

(S4) subjecting the formed part to a surface modification treatment by a laser shock peening method so that the formed part has a predetermined residual compressive stress;

wherein heating the spray area of step (S3) comprises:

heating, by a first heating unit, the substrate while performing the spraying deposition in forming a first slice layer until the spraying deposition of the first slice layer is completed; and

heating, by a second heating unit, a surface of an uppermost formed slice layer while performing the spraying deposition on the surface of the uppermost formed slice layer, and repeating until the spraying deposition of all slice layers is completed; and

wherein:

the surfaces of the formed slice layers are heated by a ring-shaped laser beam;

the ring-shaped laser beam and the sprayed powder are coaxially output by a nozzle;

a composite nozzle inner wall separates the sprayed powder from the coaxial ring-shaped laser beam, the coaxial ring-shaped laser beam being outside the sprayed powder;

the gantry machine tool comprises the spraying deposition module, the first heating unit, and the second heating unit; the first heating unit is provided above the substrate,

the second heating unit and the cold spraying gun are provided at a bottom of a first spindle provided on the gantry machine tool to move synchronously;

a temperature sensor is configured to monitor a temperature of the heated spray area in real-time; and

a power, a pulse width, and a frequency of the ring-shaped laser beam are adjusted via a real-time closed-loop feedback mechanism according to the monitored temperature of the uppermost formed slice layer.

2. The method according to claim 1 , wherein the substrate is heated by at least one item selected from the group consisting of a heating furnace provided outside a spray chamber, a plasma device provided inside the spray chamber, and an electromagnetic heating coil.

3. The method according to claim 1 , wherein in step (S3), the substrate is preheated to 600° C. to 1,100° C., and the spray area is heated to 800° C. to 1,400° C.

4. An additive manufacturing method implemented by a gantry machine tool, comprising the steps of:

(S1) slicing a three-dimensional computer-aided design model of a workpiece into multiple layers according to a shape requirement, a thickness requirement, and a surface accuracy requirement, and obtaining data of the multiple layers, wherein the obtained data comprise thickness data, shape data, and surface accuracy data of each slice layer and a melting point of a material;

(S2) planning a forming path according to the data of the multiple layers, and generating computer numerical control codes for forming the multiple layers;

(S3) obtaining a formed part by:

preheating a substrate;

performing, by a spraying deposition module comprising a cold spraying gun, a layer-by-layer spraying deposition of the material as a sprayed powder by cold spray according to the computer numerical control codes in step (S2); and

heating a spray area to a temperature until the spraying deposition of all slice layers is completed, wherein the temperature is in a range of the melting point of the sprayed powder minus 200° C. to the melting point of the sprayed powder; and

(S4) subjecting the formed part to a surface modification treatment by a laser shock peening method so that the formed part has a predetermined residual compressive stress;

wherein heating the spray area of step (S3) comprises:

heating, by a first heating unit, the substrate while performing the spraying deposition in forming a first slice layer until the spraying deposition of the first slice layer is completed; and

heating, by a second heating unit, a surface of an uppermost formed slice layer while performing the spraying deposition on the surface of the uppermost formed slice layer, and repeating until the spraying deposition of all slice layers is completed; and

wherein:

the surfaces of the formed slice layers are heated by a ring-shaped laser beam;

the ring-shaped laser beam and the sprayed powder are coaxially output by a nozzle;

the gantry machine tool comprises the spraying deposition module, the first heating unit, and the second heating unit; the first heating unit is provided above the substrate,

the second heating unit and the cold spraying gun are provided at a bottom of a first spindle provided on the gantry machine tool to move synchronously;

a temperature sensor is configured to monitor a temperature of the heated spray area in real-time; and

a power, a pulse width, and a frequency of the ring-shaped laser beam are adjusted via a real-time closed-loop feedback mechanism according to the monitored temperature of the uppermost formed slice layer.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 24, 2020
From: ZHANG, HAI'OU; HU, XIAOQI; WANG, GUILAN; YANG, CHENG
To: HUAZHONG UNIVERSITY OF SCIENCE & TECHNOLOGY
Reel/Frame 053029/0174 →
Priority Claims (1)
CN 201910546152.4 · Jun 24, 2019 · national
Continuity (1)
Related Publication 20200398457A1 · Dec 24, 2020