Method to manufacture potted electronic assemblies for extreme mechanical and thermal environments

Inventors: Walter J. Whatley (San Diego, CA); Noel Martinez (Vista, CA); Clay S. Staley (Murphy, TX)
Assignee: General Atomics
H05K3/285H05K3/24H05K3/284H05K3/325
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,418,991
App. No.
17/847,173
Granted
Sep 16, 2025
Kind
B1
Abstract

A method for manufacturing potted electronic assemblies are described. Embodiments of the method and system may provide a potting compound having a first coefficient of thermal expansion different from a second coefficient of thermal expansion for a circuit board, provide a fiber reinforcement having a third coefficient of thermal expansion selected so that when the potting compound is combined with the fiber reinforcement the combined coefficient of thermal expansion is closer to the second coefficient of thermal expansion than the first coefficient of thermal expansion is to the second coefficient of thermal expansion, and apply the fiber reinforcement and the potting compound to the circuit board.

Claims (69)

1. A method for manufacturing potted electronic assemblies, comprising:

providing a low-viscosity resin potting compound having a first coefficient of thermal expansion different from a second coefficient of thermal expansion for a circuit board;

providing a fiber reinforcement having a third coefficient of thermal expansion selected so that when the potting compound is combined with the fiber reinforcement the combined coefficient of thermal expansion is closer to the second coefficient of thermal expansion than the first coefficient of thermal expansion is to the second coefficient of thermal expansion; and

applying the fiber reinforcement and the potting compound to the circuit board.

2. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement into a mold; and

dispersing said fiber reinforcement in the mold.

3. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement into a mold; and

ultrasonically dispersing said fiber reinforcement in the mold.

4. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement into a mold; and

dispersing said fiber reinforcement with a sonicator probe.

5. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement into a mold; and

dispersing said fiber reinforcement with a rotor-stator disperser.

6. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement into a mold; and

mechanically dispersing said fiber reinforcement in the mold.

7. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement into a mold; and

said applying the fiber reinforcement and the potting compound to the circuit board comprising:

curing said potting compound.

8. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement into a mold; and

said applying the fiber reinforcement and the potting compound to the circuit board comprising:

curing said potting compound by heating said potting compound.

9. The method of claim 1 comprising:

said providing said fiber reinforcement comprising:

placing said fiber reinforcement and alcohol or other suitable solvent in a mold; and

dispersing said fiber reinforcement in the alcohol or other suitable solvent, wherein the fiber reinforcement dispersed in the alcohol or other suitable solvent comprises a fiber slug having a molded geometry.

10. The method of claim 9 comprising:

said providing said fiber reinforcement comprising:

after dispersing the fiber reinforcement, removing the fiber slug from the mold.

11. The method of claim 10 comprising:

said applying said fiber reinforcement and said potting compound to the circuit board comprising:

interposing the fiber slug between the circuit board and another circuit board.

12. The method of claim 11 comprising:

said applying said fiber reinforcement and said potting compound to the circuit board comprising:

installing the fiber slug interposed between the circuit board and the another circuit board in a structural housing.

13. The method of claim 11 comprising:

said applying said fiber reinforcement and said potting compound to the circuit board comprising:

after interposing the fiber slug, drying the fiber reinforcement by evaporating the alcohol or other suitable solvent from the fiber slug.

14. The method of claim 13 comprising:

said applying said fiber reinforcement and said potting compound to the circuit board comprising:

impregnating said potting compound into said fiber reinforcement.

15. The method of claim 1 comprising:

said applying said fiber reinforcement and said potting compound to the circuit board comprising:

interposing a fiber slug between the circuit board and another circuit board, wherein the fiber slug comprises a molded geometry of said fiber reinforcement dispersed in alcohol or other suitable solvent.

16. The method of claim 15 comprising:

said applying said fiber reinforcement and said potting compound to the circuit board comprising:

after interposing the fiber slug, drying the fiber reinforcement by evaporating the alcohol or other suitable solvent from the fiber slug; and

impregnating said potting compound into said fiber reinforcement.

17. The method of claim 16 comprising:

said impregnating said potting compound into said fiber reinforcement comprising:

applying a vacuum to the fiber reinforcement in a vacuum chamber.

18. The method of claim 17 comprising:

said impregnating said potting compound into said fiber reinforcement comprising:

after applying the vacuum, applying additional hydrostatic pressure over atmospheric pressure to the vacuum chamber.

19. The method of claim 18 comprising:

said impregnating said potting compound into said fiber reinforcement comprising:

after applying the additional hydrostatic pressure, again applying the vacuum to the vacuum chamber.

Continuity (1)
Continuation 16844659 · Apr 9, 2020
References Cited (23)
US H1245H · Griswold · 1993 [cited by applicant]
US 5317914A · Franco, Jr. · 1994 [cited by applicant]
US 5381304A · Theroux · 1995 [cited by applicant]
US 6664318B1 · Bymark · 2003 [cited by applicant]
US 6744637B2 · Blazic · 2004 [cited by applicant]
US 7475637B2 · Rastegar · 2009 [cited by applicant]
US 8458899B2 · Mitchell · 2013 [cited by applicant]
US 8640619B1 · Dimke · 2014 [cited by applicant]
US 9860992B1 · Chao · 2018 [cited by applicant]
US 10188001B2 · Thomas · 2019 [cited by examiner]
US 10362692B2 · Lv · 2019 [cited by applicant]
US 11395414B1 · Whatley · 2022 [cited by applicant]
US 20070139044A1 · Lamb · 2007 [cited by applicant]
US 20080036075A1 · Taylor · 2008 [cited by applicant]
US 20090004557A1 · Lasarov · 2009 [cited by applicant]
US 20110229702A1 · Aizpuru · 2011 [cited by applicant]
US 20180352666A1 · Liskow · 2018 [cited by applicant]
DE 102006019250A1 · 2007 [cited by examiner]
WO 2005064262 · 2005 [cited by applicant]
USPTO; Non-Final Office Action issued in U.S. Appl. No. 16/844,659 mailed Dec. 15, 2021. [cited by applicant]
USPTO; Notice of Allowance issued in U.S. Appl. No. 16/844,659 mailed Mar. 29, 2022. [cited by applicant]
USPTO; Restriction Requirement issued in U.S. Appl. No. 16/844,659 mailed Aug. 2, 2021. [cited by applicant]
Whatley, et al.; U.S. Appl. No. 16/844,659, filed Apr. 9, 2020. [cited by applicant]