Reconfigurable devices with multi-layer composite phase change materials

Inventors: Jeong-Sun Moon (Moorpark, CA); Hwa Chang Seo (Malibu, CA); Kyung-Ah Son (Moorpark, CA)
Assignee: HRL LABORATORIES, LLC
H10N70/231G11C13/0004H10N70/026H10N70/041H10N70/8613H10N70/8828
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,446,477
App. No.
17/858,948
Granted
Oct 14, 2025
Kind
B1
Abstract

A device having: a multilayer composite phase change material structure with: a bottom PCM layer of a first SbTe PCM material having a first metallic doping; a first composite PCM layer on the bottom PCM layer, wherein the first composite PCM layer comprises at least: a first composite layer, comprising said first PCM material having a second metallic doping; and a second composite layer, comprising said first SbTe PCM material undoped, on the first composite layer; and a top PCM layer, comprising first SbTe PCM material having said first metallic doping, on the composite PCM layer. The first metallic doping can be identical to the second metallic doping. The first PCM material can comprise SbTe and the first and second metallic dopings can comprise one of Ge, In and GeIn.

Claims (47)

1. A device having:

a multilayer composite phase change material structure comprising:

a bottom SbTe PCM layer of a first PCM material having a first metallic doping;

a first composite PCM layer on the bottom PCM layer, wherein the first composite PCM layer comprises at least:

a first composite layer, comprising said first PCM material having a second metallic doping; and

a second composite layer, comprising said first SbTe PCM material undoped, on the first composite layer; and

a top PCM layer, comprising first SbTe PCM material having said first metallic doping, on the composite PCM layer.

2. The device of claim 1 , wherein said first PCM material comprises SbTe and wherein said first and second metallic dopings comprise each one of Ge, In, and GeIn.

3. The device of claim 2 wherein:

the bottom PCM layer is a GeInSbTe layer that is 5-15 nm thick;

the top PCM layer is a GeInSbTe layer that is 5-15 nm thick;

the second composite layer is a SbTe layer that is 5-15 nm thick; and

the first composite layer is a GeInSbTe layer that is 5-15 nm thick.

4. The device of claim 1 wherein the first composite PCM layer comprises a superposition of n pairs comprising each said second composite layer on top of said first composite layer with metal-doped SbTe PCM and undoped SbTe PCM, wherein n is greater than one.

5. The device of claim 1 further comprising:

a first ohmic contact on a first end of the multilayer composite phase change material structure;

a second ohmic contact on a second end of the multilayer composite phase change material structure;

a substrate; and

a heater on the substrate and coupled to the multilayer composite phase change material structure.

6. The device of claim 5 wherein the heater comprises TiW.

7. The device of claim 5 further comprising:

a thermal dielectric layer between the heater and the multilayer composite phase change material (PCM);

wherein the thermal dielectric layer comprises SiNx, AlN, diamond, or SiC.

8. The device of claim 5 further comprising:

a thermal barrier coupled between the heater and the substrate;

wherein the thermal barrier comprises SiO 2 .

9. The device of claim 5 :

having a dielectric on the substrate and surrounding the heater; and

wherein the dielectric is configured so that the multilayer composite phase change material structure is planar.

10. The device of claim 5 wherein the substrate comprises:

high-resistance Si, sapphire, borofloat, quartz, or fused silica.

11. The device of claim 5 further comprising:

an encapsulating layer partially covering the first ohmic contact and the second ohmic contact, and covering a top of the top PCM layer between the first ohmic contact and the second ohmic contact;

wherein the encapsulating layer comprises SiNx.

12. A method of providing a phase change material structure, the method comprising:

forming a bottom PCM layer by sputtering a first SbTe PCM material having a first metallic doping in an amorphous phase;

forming a composite phase change material layer on the bottom PCM layer, wherein the first composite phase change material layer comprises at least:

a first composite layer, formed by sputtering said first PCM material having a second metallic doping in an amorphous phase; and

a second composite layer, formed by sputtering said first SbTe PCM material, undoped, in an amorphous phase on the first composite layer; and

forming a top SbTe PCM layer layer on the composite PCM layer by sputtering said first PCM material having said first metallic dopingin an amorphous phase.

13. The method of claim 12 , wherein said first PCM material comprises SbTe and wherein said first and second metallic dopings comprise each one of Ge, In, and GeIn.

14. The method of claim 13 , further comprising:

forming a first ohmic contact on a first end of the multilayer composite phase change material structure; and

forming a second ohmic contact on a second end of the multilayer composite phase change material structure

providing a substrate; and

providing a heater on the substrate, wherein the heater is coupled to the multilayer composite phase change material sructure.

15. The method of claim 12 , wherein the first composite PCM layer comprises a superposition of n pairs of SbTe-based doped and undoped PCM comprising each said second composite layer on top of said first composite layer, wherein n is greater than one.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 3, 2022
From: MOON, JEONG-SUN; SEO, HWA CHANG; SON, KYUNG-AH
To: HRL LABORATORIES, LLC
Reel/Frame 061642/0622 →
Continuity (1)
Provisional Application 63241465 · Sep 7, 2021
References Cited (46)
US 7728319B2 · Goux · 2010 [cited by applicant]
US 8900930B2 · Moon · 2014 [cited by applicant]
US 9293699B1 · Moon · 2016 [cited by applicant]
US 9362379B2 · Moon · 2016 [cited by applicant]
US 9368720B1 · Moon et al. · 2016 [cited by applicant]
US 9972905B2 · Schaffner et al. · 2018 [cited by applicant]
US 10937960B2 · Slovin · 2021 [cited by examiner]
US 11187891B1 · Moon et al. · 2021 [cited by applicant]
US 11314109B1 · Moon et al. · 2022 [cited by applicant]
US 20060082427A1 · Joung · 2006 [cited by applicant]
US 20100096255A1 · Ye · 2010 [cited by applicant]
US 20130181182A1 · Perniola · 2013 [cited by applicant]
US 20140264230A1 · Borodulin · 2014 [cited by applicant]
Botula, A., et al., “A Thin-film SOI 180 nm CMOS RF Switch Technology”, Silicon Monolithic Integrated Circuits in RF Systems (SIRF), pp. 1-4, Jan. 2009. [cited by applicant]
Chua et al., “Low resistance, high dynamic range reconfigurable phase change switch for RF applications”, Applied Physics Letters, vol. 97, 183506-1 to 83506-3, 2010. [cited by applicant]
EE Times, Nov. 2011, “Samsung preps 8-Gbit phase-change memory”, pp. 1-6. [cited by applicant]
Kelly, D. et al., “The State-of-the-art of Silicon-on-Sapphire CMOS RF switches”, CSICS Digest, pp. 200-203, 2005. [cited by applicant]
Lankhorst, et al., “Low-cost and nanoscale non-volatile memory concept for future silicon chips,” Nature Materials, vol. 4, Apr. 2005, pp. 347-352. [cited by applicant]
Lo, et al., “Three-terminal probe reconfigurable phase-change material switches”, IEEE Transactions on Electron Devices., vol. 57, No. 1, pp. 312-320, Jan. 2010. [cited by applicant]
Makioka, S. et al., “Super self-aligned GaAs RF switch IC with 0.25 dB extremely low insertion loss for mobile communications”, IEEE Transactions Electron Devices, vol. 48, No. 8, pp. 1510-1514, Aug. 2001. [cited by applicant]
Moon, J. S. et al., “11 THz figure-of-merit phase-change RF switches for reconfigurable wireless front-ends”, IEEE MTT-S International Microwave Symposium, pp. 1-4, 2015. [cited by applicant]
Moon, J.S et al., “High-linearity 1 ohm RF switches with phase-change materials”, SIRF, pp. 7-9, Jan. 2014. [cited by applicant]
Oomachi, et al. “Recording Characteristics of Ge Doped Eutectic SbTe Phase Change Discs with Various Compositions and Its Potential for High Density Recording,” Japanese Journal of Applied Physics, vol. 41, No. 3, Mar. … [cited by applicant]
Perniola et al, “Electrical behavior of phase change memory cells based on GeTe”, IEEE EDL., vol. 31, No. 5, pp. 488-490, May 2010. [cited by applicant]
Rebeiz, G. et al., “Tuning in to RF MEMS” IEEE Microwave Magazine, pp. 55-72, Oct. 2009. [cited by applicant]
Tomback, A. et al., “Cellular Antenna Switches for Multimode Applications based on a Silicon-on-Insulator Technology”, Radio Frequency Integrated Circuits Symposium (RFIC), pp. 271-274, May 2010. [cited by applicant]
Wen et al., “A phase-change via-reconfigurable on-chip inductor”, IEDM Tech digest, pp. 10.3.1-10.3.4, Dec. 2010. [cited by applicant]
Zhu, M., et al. “One order of magnitude faster phase change at reduced power in Ti—Sb—Te”, Nature Communications, Published online Jul. 8, 2014. doi:10.1038/ncomms5086; PMCID: PMC4102114 (6 pages). [cited by applicant]
From U.S. Appl. No. 14/528,945 (now U.S. Pat. No. 9,368,720), Notice of Allowance dated Feb. 16, 2016. [cited by applicant]
From U.S. Appl. No. 14/528,945 (now U.S. Pat. No. 9,368,720), Office Action dated Oct. 16, 2015. [cited by applicant]
From U.S. Appl. No. 15/444,101 (unpublished, non-publication request filed), Decision dated Oct. 24, 2021. [cited by applicant]
From U.S. Appl. No. 15/444,101 (unpublished, non-publication request filed), Office action dated Mar. 11, 2019. [cited by applicant]
From U.S. Appl. No. 15/444,101 (unpublished, non-publication request filed), Office action dated Jan. 3, 2019. [cited by applicant]
From U.S. Appl. No. 15/444,101 (unpublished, non-publication request filed), Office action dated Aug. 9, 2018. [cited by applicant]
From U.S. Appl. No. 15/444,101 (unpublished, non-publication request filed), Office action dated Jun. 7, 2018. [cited by applicant]
From U.S. Appl. No. 15/444,101 (unpublished, non-publication request filed), Office action dated Mar. 27, 2019. [cited by applicant]
From U.S. Appl. No. 15/444,101 (unpublished, non-publication request filed), Office action dated Oct. 6, 2017. [cited by applicant]
J. S. Moon, H. Seo, K. Son, K. Lee, D. Zehnder, H. Tai, and D. Le, “5 THz Figure-of-Merit Reliable Phase-change RF Switches for Millimeter-wave Applications”, [cited by applicant]
P. Borodulin et al., “Recent Advances in Fabrication and Characterization of GeTe-based phase-change RF switches and MMICs”, IEEE MTT-S 2017 International Microwave Symposium Digest, 2017, entire document. [cited by applicant]
El-Hinnawy et al., “Four-terminal inline Chalcogenide phase-change RF switch using an independent resistive heater for thermal actuation”, IEEE EDL, vol. 34, (2013), entire document. [cited by applicant]
Y-H Shim and M. Rais-Zadel, “Non-linear analysis of RF ohmic switches based on phase—change materials”, IEEE EDL, vol. 35, (2014) , entire document. [cited by applicant]
J. S. Moon, H. C. Seo, and D. Le, “Development toward high-power sub-1 ohm DC-67 GHz RF switches using phase change materials for reconfigurable RF front-end”, [cited by applicant]
J. S. Moon et al., “Reconfigurable Infrared spectral imaging with robust phase change materials”, SPIE Proceedings, 2019, entire document. [cited by applicant]
J. S. Moon et al., “Electrically-programmable optical devices with phase change materials”, SPIE Proceedings, 2020, entire document. [cited by applicant]
U.S. Appl. No. 15/444,101, filed Feb. 27, 2017. [cited by applicant]
El-Hinnawy et al., “A 25 THz F [cited by applicant]